IP Library Granted Patent US 6,866,796
Granted Patent B2
US 6,866,796 · App. 10/329,271 · Granted Mar 15, 2005

Blue phosphor for fluorescent display and method for synthesizing the same

Assignee: Electronics and Telecommunications Research Institute
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 6,866,796
App. No.
10/329,271
Granted
Mar 15, 2005
Kind
B2
Abstract

Provided are a blue phosphor for a fluorescent display having a high luminous efficiency, and a method for synthesizing the same. The blue phosphor is obtained from a host composed of strontium carbonate (SrCO 3 ) and an activator composed of a cerium compound. The method for synthesizing the blue phosphor includes preparing a mixture having strontium carbonate (SrCO 3 ) and a cerium oxide (CeO 2 ) homogenously mixed according to the composition having the following general formula: SrCO 3 +xCeO 2 wherein 0.01≦x≦0.5, and annealing the mixture at 800 to 900° C.

Claims (13)

1. A blue phosphor for a fluorescent display obtained from a host composed of strontium carbonate (SrCO 3 ) and an activator composed of a cerium compound.

2. The blue phosphor of claim 1 , wherein the cerium compound is a cerium oxide (CeO 2 ).

3. The blue phosphor of claim 1 , wherein the host and the activator are mixed in a molar ratio of 1:0.01˜1:0.5.

4. The blue phosphor of claim 2 , wherein the host and the activator are mixed in a molar ratio of 1:0.01˜1:0.5.

5. A method for synthesizing a blue phosphor for a fluorescent display, comprising:

(a) preparing a mixture having strontium carbonate (SrCO 3 ) and a cerium oxide (CeO 2 ) homogenously mixed therein; and

(b) heating the mixture.

6. The method of claim 5 , wherein in step (a), the strontium carbonate (SrCO 3 ) and the cerium oxide (CeO 2 ) are mixed according to the composition having the following general formula:

SrCO 3 +xCeO 2

wherein 0.01≦x≦0.5.

7. The method of claim 6 , wherein the strontium carbonate (SrCO 3 ) and the cerium oxide (CeO 2 ) are mixed in a molar ratio of 1:0.05.

8. The method of claim 5 , wherein in step (b), heating is performed at 800° C. to 900° C.

9. The method of claim 5 , wherein in step (b), heating is performed for 12 to 36 hours.

Assignments (3)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 23, 2012
From: IPG ELECTRONICS 502 LIMITED; ELECTRONICS AND TELECOMMUNICATIONS RESEARCH INSTITUTE
To: PENDRAGON ELECTRONICS AND TELECOMMUNICATIONS RESEARCH LLC
Reel/Frame 028611/0643 →
ASSIGNMENT OF ONE HALF (1/2) OF ALL OF ASSIGNORS' RIGHT, TITLE AND INTEREST Recorded Nov 3, 2009
From: ELECTRONICS AND TELECOMMUNICATIONS RESEARCH INSTITUTE
To: IPG ELECTRONICS 502 LIMITED
Reel/Frame 023456/0363 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 24, 2002
From: KANG, SEUNG-YOUL; SUH, KYUNG-SOO
To: ELECTRONICS AND TELECOMMUNICATIONS RESEARCH INSTITUTE
Reel/Frame 013627/0314 →
Priority Claims (1)
KR 2001-85039 · Dec 26, 2001 · national
Continuity (1)
Related Publication 20030122109A1 · Jul 3, 2003