Method for preventing or inhibiting fouling in a gas-phase polyolefin polymerization process

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,253,239
App. No.
11/249,573
Granted
Aug 7, 2007
Kind
B2
Abstract

A method for preventing or inhibiting fouling in a gas-phase polyolefin polymerization process. The method includes maintaining the inside surface temperature of the process equipment below the dew point temperature of the gas mixture passing through the equipment.

Claims (16)

1. A method for preventing or inhibiting fouling in a gas-phase polyolefin polymerization process, comprising:

passing a gas mixture having an average temperature above its dew point temperature through process equipment; and

maintaining the inside surface temperature of the equipment below the dew point temperature of the gas mixture.

2. The method according to claim 1 , wherein the maintaining step comprises adding an inert condensable compound to the gas mixture.

3. The method according to claim 2 , wherein the inert condensable compound is a saturated hydrocarbon.

4. The method according to claim 3 , wherein the saturated hydrocarbon comprises butane, pentane, hexane, or mixtures thereof.

5. The method according to claim 1 , wherein the maintaining step comprises decreasing the velocity of the gas mixture flowing through the equipment.

6. The method according to claim 1 , wherein the process equipment comprises piping, heat exchangers, cyclone separators, gas ejectors, compressors, reactors, or combinations thereof.

7. A method for preventing or inhibiting fouling in a gas-phase polyolefin polymerization process, comprising:

diverting at least a portion of a gas mixture flowing through equipment in the polymerization process through a by-pass around the equipment;

maintaining the inside surface temperature of the equipment below the dew point temperature of the gas mixture; and

combining the portion of the gas mixture flowing through the by-pass with the portion of the gas mixture flowing through the equipment to form a combined gas mixture having an average temperature above the combined gas mixture's dew point temperature.

8. The method according to claim 7 , wherein the maintaining step comprises adding an inert condensable compound to the gas mixture.

9. The method according to claim 8 , wherein the inert condensable compound is a saturated hydrocarbon.

10. The method according to claim 9 , wherein the saturated hydrocarbon comprises butane, pentane, hexane, or mixtures thereof.

11. The method according to claim 7 , wherein the process equipment comprises heat exchangers.

Assignments (1)
RELEASE OF SECURITY INTEREST Recorded Aug 24, 2016
From: BANK OF AMERICA, N.A.
To: WESTLAKE LONGVIEW CORPORATION