Stress-enhanced performance of a FinFet using surface/channel orientations and strained capping layers

Assignee: Synopsys, Inc.
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,939,862
App. No.
11/755,715
Granted
May 10, 2011
Kind
B2
Abstract

Different approaches for FinFET performance enhancement based on surface/channel direction and type of strained capping layer are provided. In one relatively simple and inexpensive approach providing a performance boost, a single surface/channel direction orientation and a single strained capping layer can be used for both n-channel FinFETs (nFinFETs) and p-channel FinFETs (pFinFETs). In another approach including more process steps (thereby increasing manufacturing cost) but providing a significantly higher performance boost, different surface/channel direction orientations and different strained capping layers can be used for nFinFETs and pFinFETs.

Claims (11)

1. An integrated circuit (IC) including a plurality of pFinFETs and nFinFETs, each FinFET comprising:

a source;

a drain;

a vertical channel connecting the source and the drain, the vertical channel forming a fin, the fin having a (100) surface orientation and a <110> channel direction orientation, the fin being formed above a substrate of FinFET;

a gate straddling the fin; and

a compressive capping layer covering at least the fin and the gate to increase carrier mobility in the FinFET,

wherein the surface orientation, the channel direction orientation, and the compressive capping layer increase electron mobility for the nFinFETs and increase hole mobility for the pFinFETs, thereby improving both the nFinFETs and the pFinFETs.

2. The IC of claim 1 , wherein the compressive capping layer is silicon nitride.

3. The IC of claim 2 , wherein the silicon nitride is between 40 nm and 100 nm thick.

4. The IC of claim 2 , wherein the silicon nitride is approximately 50 nm thick.

5. The IC of claim 2 , wherein the compressive capping layer of silicon nitride has approximately 2.5 GPa compressive stress.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 30, 2007
From: MOROZ, VICTOR; KING LIU, TSU-JAE
To: SYNOPSYS, INC.
Reel/Frame 019359/0076 →
Continuity (1)
Related Publication 20080296632A1 · Dec 4, 2008