Abstract

A solid oxide fuel cell (SOFC) includes a cathode electrode, a solid oxide electrolyte, and an anode electrode. The electrolyte includes yttria stabilized zirconia and scandia stabilized zirconia, such as scandia ceria stabilized zirconia.

Claims (26)

1 . A solid oxide fuel cell (SOFC), comprising:

a cathode electrode;

a solid oxide electrolyte; and

an anode electrode;

wherein the electrolyte comprises a yttria stabilized zirconia and a scandia stabilized zirconia.

2 . The electrolyte of claim 1 , wherein the electrolyte comprises a mixture of the yttria stabilized zirconia and the scandia stabilized zirconia.

3 . The SOFC of claim 2 , wherein the scandia stabilized zirconia comprises up to 1 molar percent ceria, alumina or yttria, about 6 to about 11 molar percent scandia and a balance comprising zirconia.

4 . The SOFC of claim 3 , wherein the electrolyte comprises a mixture of the yttria stabilized zirconia and scandia ceria stabilized zirconia.

5 . The SOFC of claim 1 , wherein the electrolyte comprises a mixture of yttria stabilized zirconia and [(ZrO 2 ) 1-y (CeO 2 ) y ] 1-x (Sc 2 O 3 ) x , where 0.06≦x≦0.11 and 0≦y≦0.01.

6 . The SOFC of claim 5 , wherein the yttria stabilized zirconia comprises 3 to 10 molar percent yttria.

7 . The SOFC of claim 1 , wherein a weight ratio of the yttria stabilized zirconia to the scandia stabilized zirconia in the electrolyte ranges from 1:4 to 1:1.

8 . The SOFC of claim 7 , wherein the weight ratio of the yttria stabilized zirconia to the scandia stabilized zirconia in the electrolyte ranges from 1:2 to 1:3.

9 . The SOFC of claim 1 , wherein the electrolyte is about 150 to about 300 microns thick.

10 . A solid oxide fuel cell (SOFC), comprising:

a cathode electrode;

a solid oxide electrolyte comprising a mixture of about 25 weight percent yttria stabilized zirconia which comprises 3 molar percent yttria, and about 75 weight percent scandia ceria stabilized zirconia which comprises 1 molar percent ceria and 10 molar percent scandia; and

an anode electrode.

11 . The SOFC of claim 10 , wherein the anode electrode comprises:

a first sublayer comprising samaria doped ceria; and

a second sublayer comprising a scandia ceria stabilized zirconia and gadolinia doped ceria ceramic phase and a nickel containing phase.

12 . A method of making a solid oxide fuel cell, comprising:

mixing yttria stabilized zirconia powder with scandia stabilized zirconia powder to form a powder mixture;

shaping the powder mixture;

sintering the shaped powder mixture to form an electrolyte;

forming an anode electrode on a first side of the electrolyte; and

forming a cathode electrode on a second side of the electrolyte.

Assignments (3)
RELEASE OF SECURITY INTEREST Recorded Nov 29, 2018
From: U.S. BANK NATIONAL ASSOCIATION, AS COLLATERAL AGENT
To: BLOOM ENERGY CORPORATION
Reel/Frame 047686/0121 →
SECURITY INTEREST Recorded Dec 15, 2015
From: BLOOM ENERGY CORPORATION
To: U.S. BANK NATIONAL ASSOCIATION, AS COLLATERAL AGENT
Reel/Frame 037301/0093 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 2, 2008
From: NGUYEN, DIEN; OSWAL, RAVI; ARMSTRONG, TAD; EI BATAWI, EMAD
To: BLOOM ENERGY CORPORATION
Reel/Frame 021190/0959 →