IP Library Granted Patent US 9,827,467
Granted Patent B2
US 9,827,467 · App. 14/814,578 · Granted Nov 28, 2017

Golf ball cores made from plasticized thermoplastic compositions containing non-acid polymers

Inventors: Michael J. Sullivan (Old Lyme, CT); Robert Blink (Newport, RI); David A. Bulpett (Boston, MA); Mark L. Binette (Mattapoisett, MA); Brian Comeau (Berkley, MA)
Assignee: Acushnet Company
A63B37/0092A63B37/0044A63B37/0051A63B37/0063A63B37/0064A63B37/0075A63B37/0087A63B2037/0079
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,827,467
App. No.
14/814,578
Granted
Nov 28, 2017
Kind
B2
Abstract

Multi-layered golf balls containing a two-layered core assembly are provided. Preferably, at least one of the core layers is formed from a thermoplastic composition that comprises: a) thermoplastic non-acid polymer, and b) plasticizer. In one preferred embodiment, the inner core is made of a first thermoplastic composition comprising the non-acid polymer and plasticizer; and the outer core layer is made of a second thermoplastic composition. For example, an ethylene acid copolymer may be used to form the outer core layer. A fatty acid ester such as ethyl oleate is preferably used as the plasticizer. Suitable non-acid polymers include, for example, polyesters, polyamides, polyolefins, and polyurethanes. The core assembly has a relatively high resiliency at given compressions.

Claims (21)

1. A golf ball, comprising:

i) an inner core comprising a first thermoplastic material, the first thermoplastic material comprising: a) a thermoplastic non-acid polymer, wherein the non-acid polymer is selected from the group consisting of a polyether-amide block copolymer and a polyester-polyether block copolymer, and mixtures thereof; and b) a plasticizer; the inner core having an outer surface hardness (H inner core surface ) and a center hardness (H inner core center ), the H inner core surface being greater than the H inner core center to provide a positive hardness gradient; and

ii) an outer core layer comprising a second thermoplastic material, the outer core layer being disposed about the inner core and having an outer surface hardness (H outer surface of OC ) and a midpoint hardness (H midpoint of OC ), the H outer surface of OC being greater than the H midpoint of OC to provide a positive hardness gradient;

the inner core and outer core forming a core assembly, wherein the center hardness of the in core (H inner core center ) is in the range of about 10 Shore C to about 70 Shore C and the outer surface hardness of the outer core layer (H outer surface of OC ) is in the range of about 20 Shore C to about 95 Shore C to provide a positive hardness gradient across the core assembly; and

iii) a cover having at least one layer.

2. The golf ball of claim 1 , wherein the second thermoplastic material comprises: a) an acid copolymer of ethylene and an α,β-unsaturated carboxylic acid, optionally including a softening monomer selected from the group consisting of alkyl acrylates and methacrylates; b) plasticizer; and c) cation source present in an amount sufficient to neutralize from about 0 to about 100% of all acid groups present in the material.

3. The golf ball of claim 2 , wherein the second thermoplastic material comprises an ethylene acid copolymer containing acid groups such that greater than 70% of the acid groups arc neutralized.

4. The golf ball of claim 3 wherein 90% or greater of the acid groups are neutralized.

5. The golf ball of claim 4 , wherein the ethylene acid copolymer is selected from the group consisting of ethylene/(meth)acrylic acid/n-butyl acrylate; ethylene/(meth)acrylic acid/ethyl acrylate; ethylene/(meth)acrylic acid/methyl acrylate; ethylene/(meth)acrylic acid/n-butyl acrylate; and ethylene/(meth)acrylic acid/isobutyl acrylate copolymers.

6. The golf ball of claim 1 , wherein the second thermoplastic material is selected from the group consisting of polyesters; polyamides; polyamide-ethers, polyamide-esters; polyurethanes, polyureas; fluoropolymers; polystyrenes; polypropylenes; polyethylenes; polyvinyl chlorides; polyvinyl acetates; polycarbonates; polyvinyl alcohols; polyester-ethers; polyethers; polyimides, polyetherketones, polyamideimides; and mixtures therof.

7. The golf ball of claim 1 , wherein the inner core has a diameter in the range of about 0.100 to about 0.800 inches; and wherein the H inner core center is in the range of about 10 Shore C to about 70 Shore C and the H inner core surface is in the range of about 15 Shore C to about 90 Shore C.

8. The golf ball of claim 1 , wherein the H midpoint of OC is in the range of about 20 Shore C to about 85 Shore C and the H outer surface of OC is in the range of about 30 Shore C to about95 Shore C.

9. The golf ball of claim 1 , wherein the center hardness of the inner core (H inner core center ) is in the range of about 30 Shore C to about 65 Shore C and the outer surface hardness of the outer core layer (H outer surface of OC ) is in the range of about 40 Shore C to about 90 Shore C to provide a positive hardness gradient across the core assembly,

10. The golf ball of claim 1 , wherein the ball has a compression in the range of about 25 to about 55.

11. A golf ball, comprising:

i) an inner core comprising a first thermoplastic material, the first thermoplastic material comprising: a) a thermoplastic non-acid polymer; and b) a plasticizer, wherein the plasticizer is an alkyl oleate selected from the group consisting of methyl oleate, ethyl oleate, propyl oleate, butyl oleate, and octyl oleate, and mixtures thereof and the concentration of plasticizer in the first themolastic material is in the range of about 3% to about 50%; the inner core having an outer surface hardness (H inner core surface ) and a center hardness (H inner core center ), the H inner core surface being greater than the H inner core center to provide a positive hardness gradient; and

ii) an outer core layer comprising a second thermoplastic material, the outer core layer being disposed about the inner core and having an outer surface hardness (H outer surface of OC ) and a midpoint hardness (H midpoint of OC ), the H outer surface of OC being greater than the H midpoint of OC to provide a positive hardness gradient;

the inner core and outer core forming a core assembly, wherein the center hardness of the inner core (H inner core center ) is in the range of about 10 Shore C to about 70 Shore C and the outer surface hardness of the outer core layer (H outer surface of OC ) is in the range of about 20 Shore C to about 95 Shore C to provide a positive hardness gradient across the core assembly; and

iii) a cover having at least one layer.

12. The golf ball of claim 11 , wherein the non-acid polymer is selected from the group consisting of fluoropolymers, polystyrenes, polyolefins, polyamides, polyesters, polyethers, polyvinyl chlorides, polyvinyl acetates, polyimides, ethylene propylene rubber, ethylene propylene diene rubber, styrenic block copolymer rubbers, alkyl acrylate rubbers, and mixtures thereof.

13. The golf ball of claim 11 , wherein the non-acid polymer is a polyamide selected from the group consisting of polyamide 6; polyamide 6,6; polyamide 6,10; polyamide 6,12; polyamide 11; polyamide 12; polyamide 6,9; and polyamide 4,6, and copolymers and blends thereof.

Assignments (5)
ASSIGNMENT OF SECURITY INTEREST IN PATENTS (ASSIGNS 039506-0030) Recorded Aug 3, 2022
From: WELLS FARGO BANK, NATIONAL ASSOCIATION, AS RESIGNING ADMINISTRATIVE AGENT
To: JPMORGAN CHASE BANK, N.A., AS SUCCESSOR ADMINISTRATIVE AGENT
Reel/Frame 061521/0414 →
SECURITY INTEREST Recorded Aug 3, 2022
From: ACUSHNET COMPANY
To: JPMORGAN CHASE BANK, N.A., AS ADMINISTRATIVE AGENT
Reel/Frame 061099/0236 →
SECURITY INTEREST Recorded Jul 28, 2016
From: ACUSHNET COMPANY
To: WELLS FARGO BANK, NATIONAL ASSOCIATION, AS ADMINISTRATIVE AGENT
Reel/Frame 039506/0030 →
SECURITY INTEREST Recorded Dec 17, 2015
From: ACUSHNET COMPANY
To: KOREA DEVELOPMENT BANK, NEW YORK BANK
Reel/Frame 037310/0866 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 31, 2015
From: SULLIVAN, MICHAEL J.; BLINK, ROBERT; BULPETT, DAVID A.; BINETTE, MARK L.; COMEAU, BRIAN
To: ACUSHNET COMPANY
Reel/Frame 036223/0648 →
Continuity (1)
Related Publication 20170028264A1 · Feb 2, 2017