SAG-RESISTANT BUILDING PANEL
Described herein is a building panel comprising a body comprising a first fibrous material comprising inorganic fiber, a non-woven scrim coupled to the body; and wherein the non-woven scrim has a thickness ranging from about 8 mils to about 20 mils.
1 . A building panel comprising:
a body comprising a first fibrous material comprising inorganic fiber;
a non-woven scrim coupled to the body; and
wherein the non-woven scrim has a thickness ranging from about 8 mils to about 20 mils.
2 . The building panel according to claim 1 , wherein the first fibrous material is present in the body in amount ranging from about 15 wt. % to about 35 wt. % based on the total weight of the body.
3 .- 4 . (canceled)
5 . The building panel according to claim 1 , wherein the body comprises a second fibrous material that includes an organic fiber.
6 . The building panel according to claim 1 , wherein the body has a porosity ranging from about 60% to about 98%.
7 . The building panel according to claim 1 , wherein the body further comprises a filler present in the body in amount ranging from about 30 wt. % to about 70 wt. % based on the total weight of the body; and
wherein the filler is selected from calcium carbonate, limestone, titanium dioxide, sand, barium sulfate, clay, mica, dolomite, silica, talc, perlite, polymers, gypsum, wollastonite, expanded-perlite, calcite, aluminum trihydrate.
8 .- 9 . (canceled)
10 . The building panel according to claim 1 , wherein the non-woven scrim is coupled to the body by adhesive.
11 . The building panel according to claim 1 , wherein the thickness of the non-woven scrim ranges from about 12 mils to about 16 mils.
12 . The building panel according to claim 1 , wherein the non-woven scrim exhibits an airflow resistance less than about 500 mks rayls.
13 . The building panel according to claim 1 , wherein the body has a thickness ranging from about 0.4 inches to about 1.0 inch.
14 . A building panel comprising:
a body comprising a fibrous material that is present in an amounting ranging from about 15 wt. % to about 35 wt. % based on the total weight of the body;
a facing layer having a basis weight ranging from about 2.0 g/ft 2 to about 5.0 g/ft 2 ; and
wherein the facing layer is coupled to the body, and the facing layer comprises a non-woven scrim.
15 . The building panel according to claim 14 , wherein the fibrous material is present in the body in amount ranging from about 20 wt. % to about 30 wt. % based on the total weight of the body.
16 . The building panel according to claim 14 , wherein the fibrous material is an inorganic fiber, selected from the group consisting of mineral wool, rock wool, stone wool, and glass fibers.
17 . (canceled)
18 . The building panel according to claim 14 , wherein the body has a porosity ranging from about 60% to about 98%.
19 . The building panel according to claim 14 , wherein the body further comprises a filler present in the body in amount ranging from about 30 wt. % to about 70 wt. % based on the total weight of the body.
20 .- 25 . (canceled)
26 . The building panel according to claim 14 , wherein the facing layer is substantially free of impregnated film.
27 . A building panel comprising:
a body having a first major surface opposite a second major surface and a side surface extending between the first and second major surface, the body having a first thickness as measured between the first major surface and the second major surface of the body, and the body comprising a fibrous material;
a facing layer having a basis weight ranging from about 2.4 g/ft 2 to about 4.0 g/ft 2 , the facing layer having a first major surface opposite a second major surface and a side surface extending between the first and second major surface, the facing layer having a second thickness as measured between the first major surface and the second major surface of the facing layer, and the facing layer comprising a non-woven scrim; and
wherein the facing layer is coupled to the body, and wherein a ratio of the first thickness to the second thickness ranges from about 20:1 to about 125:1.
28 . The building panel according to claim 27 , wherein the fibrous material is present in the body in amount ranging from about 15 wt. % to about 35 wt. % based on the total weight of the body; and wherein the body has a porosity ranging from about 60% to about 98%.
29 .- 32 . (canceled)
33 . The building panel according to claim 27 , wherein the body further comprises a filler present in the body in amount ranging from about 30 wt. % to about 70 wt. % based on the total weight of the body; and
wherein the filler is selected from calcium carbonate, limestone, titanium dioxide, sand, barium sulfate, clay, mica, dolomite, silica, talc, perlite, polymers, gypsum, wollastonite, expanded-perlite, calcite, aluminum trihydrate.
34 .- 36 . (canceled)
37 . The building panel according to claim 27 , wherein the second thickness ranges from about 8 mils to about 20 mils, and wherein the first thickness ranges from about 0.4 inches to about 1.0 inches.
38 .- 39 . (canceled)
40 . The building panel according to claim 27 , wherein the facing layer is substantially free of impregnated film.
41 .- 51 . (canceled)