IP Library Granted Patent US 12,552,096
Granted Patent B2
US 12,552,096 · App. 18/290,081 · Granted Feb 17, 2026

Three-dimensional printing with coalescing agent

Inventors: Karsten N. Wilson (Corvallis, OR); Emre Hiro Discekici (San Diego, CA); Vladek Kasperchik (Corvallis, OR); Timothy L. Weber (Corvallis, OR); Mark Kowalski (Corvallis, OR); Sterling Chaffins (Corvallis, OR); Devin Alexander Mourey (Corvallis, OR)
Assignee: Peridot Print LLC
B29C64/165B33Y10/00B33Y30/00B33Y70/00
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,552,096
App. No.
18/290,081
Granted
Feb 17, 2026
Kind
B2
Abstract

A method of three-dimensional printing can include iteratively applying a polymer build material as individual layers to a powder bed, where the polymer build material includes from about 80 wt % to 100 wt % polymeric particles, and based on a three-dimensional object model, selectively applying a coalescing agent onto individual layers of the polymer build material. The coalescing agent can include an aqueous liquid vehicle and a coalescing solvent that depresses a melting point of the polymeric particles. The method can include exposing the powder bed to heat to selectively coalesce portions of individual layers of the polymer build material in contact with the coalescing solvent. The heat may not be sufficient to coalesce the polymer build material that is not in contact with the coalescing solvent and may be sufficient to fuse the polymeric particles in contact with the coalescing solvent together to form a three-dimensional object.

Claims (27)

1 . A method of three-dimensional printing, the method comprising:

iteratively applying a polymer build material as individual layers to a powder bed, wherein the polymer build material includes from about 80 wt % to 100 wt % of polymeric particles;

based on a three-dimensional object model, selectively applying a coalescing agent onto individual layers of the polymer build material, the coalescing agent including an aqueous liquid vehicle and a coalescing solvent to depress a melting point of the polymeric particles, wherein the coalescing agent is free of a radiation absorber; and

exposing the powder bed to heat to selectively coalesce portions of individual layers of the polymer build material in contact with the coalescing solvent, wherein the heat is not sufficient to coalesce the polymer build material not in contact with the coalescing solvent, and wherein the polymeric particles in contact with the coalescing solvent fuse together to form a three-dimensional object.

2 . The method of three-dimensional printing of claim 1 , wherein the coalescing solvent depresses a melting point of the polymeric particles by about 1° C. to about 20° C. resulting in a modified melting point from about 90° C. to about 200° C.

3 . The method of three-dimensional printing of claim 1 , wherein the coalescing agent is applied to the polymer build material at a weight ratio of coalescing solvent to polymer particles of about 1:3 to about 20:1.

4 . The method of three-dimensional printing of claim 1 , wherein the heat is radiant heat applied for a heating time period that ranges from about 5 minutes to about 45 minutes and brings the powder bed to a temperature ranging from about 80° C. to about 160° C.

5 . The method of three-dimensional printing of claim 1 , wherein the three-dimensional object is a porous filter having a porosity ranging from about 20% to about 90% by volume.

6 . The method of three-dimensional printing of claim 1 , wherein the polymer build material includes polyamide-6, polyamide-8, polyamide-9, polyamide-11, polyamide-12, polyamide-6,6, polyamide-6, 12, polyamide-8,12, polyamide, thermoplastic polyamide, polymer blends thereof, amorphous polymers thereof, core-shell polymers thereof, or copolymers thereof, and wherein the polymeric particles have an average particle size of from about 50 μm to about 1 mm.

7 . The method of three-dimensional printing of claim 1 , wherein the coalescing solvent is selected from the group consisting of 1-(2-hydroxyethyl)-2-pyrrolidone, 1,5-pentanediol, benzyl alcohol, ester alcohols, glycol ethers, esters, dimethylsulfoxide, hexafluoroisopropanol, cresols, diols, 1,2-butanediol, 1-methyl-2,3-propanediol, 2-pyrrolidone, glycerol, 2-phyenoxyethanol, 2-phenylethanol, 3-phenylpropanol, and a combination thereof.

8 . A three-dimensional printing kit, comprising:

a polymer build material including from about 80 wt % to 100 wt % of polymeric particles; and

a coalescing agent including an aqueous liquid vehicle and a coalescing solvent that depresses a melting point of the polymeric particles when contacted therewith, wherein the coalescing agent is free of a radiation absorber,

wherein the three-dimensional printing kit excludes a fusing agent containing a radiation absorber.

9 . The three-dimensional printing kit of claim 8 , wherein the polymer build material includes polyamide-6, polyamide-8, polyamide-9, polyamide-11, polyamide-12, polyamide-6,6, polyamide-6,12, polyamide-8,12, polyamide, thermoplastic polyamide, polymer blends thereof, amorphous polymers thereof, core-shell polymers thereof, or copolymers thereof, and wherein the polymeric particles have an average particle size of from about 50 μm to about 1 mm.

10 . The three-dimensional printing kit of claim 8 , wherein the coalescing solvent is selected from the group consisting of 1-(2-hydroxyethyl)-2-pyrrolidone, 1,5-pentanediol, benzyl alcohol, ester alcohols, glycol ethers, esters, dimethylsulfoxide, hexafluoroisopropanol, cresols, diols, 1,2-butanediol, 1-methyl-2,3-propanediol, 2-pyrrolidone, glycerol, 2-phyenoxyethanol, 2-phenylethanol, 3-phenylpropanol, and a combination thereof.

11 . The three-dimensional printing kit of claim 8 , wherein the coalescing solvent is present in the coalescing agent in an amount of from about 30 wt % to about 70 wt %.

12 . The three-dimensional printing kit of claim 8 , wherein the coalescing solvent depresses a melting point of the polymeric particles by about 1° C. to about 20° C. resulting in a modified melting point from about 90° C. to about 200° C.

13 . A system for three-dimensional printing, the system comprising:

a polymer build material including from about 80 wt % to 100 wt % of polymeric particles;

a coalescing agent including an aqueous liquid vehicle and a coalescing solvent operable to depress a melting point of the polymeric particles, wherein the coalescing agent is free of a radiation absorber;

a printhead fluidly coupled to or fluidly coupleable to the coalescing agent to selectively and iteratively eject the coalescing agent onto successive placed individual layers of the polymer build material, wherein the coalescing agent depresses a melting point of the polymeric particles; and

a radiant heat source positioned or positionable to expose the individual layers of the polymer build material to radiation energy to selectively fuse the polymeric particles in contact with the coalescing solvent to iteratively form a three-dimensional object,

wherein the system excludes a fusing agent containing a radiation absorber.

14 . The system for three-dimensional printing of claim 13 , wherein the polymeric particles include polyamide-6, polyamide-8, polyamide-9, polyamide-11, polyamide-12, polyamide-6,6, polyamide-6,12, polyamide-8,12, polyamide, thermoplastic polyamide, polymer blends thereof, amorphous polymers thereof, core-shell polymers thereof, or a copolymer thereof.

15 . The system for three-dimensional printing of claim 13 , wherein the system is operable to form a three-dimensional porous object having a porosity ranging from about 20% to about 90% by volume.

16 . The system for three-dimensional printing of claim 13 , wherein the coalescing solvent is selected from the group consisting of 1-(2-hydroxyethyl)-2-pyrrolidone, 1,5-pentanediol, benzyl alcohol, ester alcohol, glycol ether, an ester, dimethylsulfoxide, hexafluoroisopropanol, cresols, diols, 1,2-butanediol, 1-methyl-2,3-propanediol, 2-pyrrolidone, glycerol, 2-phyenoxyethanol, 2-phenylethanol, 3-phenylpropanol, and a combination thereof.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 11, 2025
From: HEWLETT-PACKARD DEVELOPMENT COMPANY, L.P.
To: PERIDOT PRINT LLC
Reel/Frame 070187/0001 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 10, 2023
From: DISCEKICI, EMRE HIRO; WILSON, KARSTEN N.; KASPERCHIK, VLADEK; WEBER, TIMOTHY L.; KOWALSKI, MARK; CHAFFINS, STERLING; MOUREY, DEVIN ALEXANDER
To: HEWLETT-PACKARD DEVELOPMENT COMPANY, L.P.
Reel/Frame 066433/0057 →
Continuity (1)
Related Publication 20240253303A1 · Aug 1, 2024
References Cited (7)
US 12377604B2 · Ionescu · 2025 [cited by examiner]
US 20190111479A1 · Kasperchik et al. · 2019 [cited by applicant]
US 20200101531A1 · Prakash · 2020 [cited by examiner]
US 20230264414A1 · Erickson · 2023 [cited by examiner]
WO 2020246991A1 · 2020 [cited by applicant]
WO 2020251520A1 · 2020 [cited by applicant]
WO 2021080565A1 · 2021 [cited by applicant]
Cited By (1)
US 12,643,289