IP Library Granted Patent US 7,159,805
Granted Patent B2
US 7,159,805 · App. 10/105,205 · Granted Jan 9, 2007

Methods of modifying fibers

Assignee: Evanite Fiber Corporation
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,159,805
App. No.
10/105,205
Granted
Jan 9, 2007
Kind
B2
Abstract

Methods of modifying fibers, such as glass fibers, are disclosed. The modified fibers can be used, for example, in a lead acid battery.

Claims (37)

1. A method of modifying a plurality of fibers, comprising:

applying pressure at more than one angle to the plurality of fibers,

wherein the plurality of fibers has an average length of greater than 1.5 millimeters before applying pressure and an average length of less than 1.5 millimeters after applying pressure, the pressure is sequentially applied at more than one angle, and the plurality of fibers is rotated between sequential steps of applying pressure.

2. The method of claim 1 , wherein the pressure is at least 50 pounds per square inch.

3. The method of claim 1 , wherein the plurality of fibers comprise a plurality of glass fibers.

4. The method of claim 1 , wherein the first average length is at least five millimeters.

5. The method of claim 1 , wherein pressure is applied for at least one second.

6. The method of claim 1 , wherein the second average length is less than 0.5 millimeter.

7. The method of claim 1 , wherein after applying pressure the plurality of fibers has an acid absorption of less than 1350%.

8. The method of claim 1 , wherein the plurality of fibers comprise a plurality of C glass fibers.

9. A method of modifying a plurality of fibers, comprising:

applying pressure to the plurality of fibers,

wherein the plurality of fibers has a first average length before applying pressure and a second average length after applying pressure, the first average length being at least 15 times greater than the second average length, and

wherein pressure is sequentially applied at more than one angle.

10. The method of claim 9 , wherein the first average length is at least 20 times the second average length.

11. The method of claim 9 , wherein the first average length is at least 25 times the second average length.

12. The method of claim 9 , wherein the plurality of fibers is rotated between sequential steps of applying pressure.

13. The method of claim 9 , wherein the pressure is at least 50 pounds per square inch.

14. The method of claim 9 , wherein the plurality of fibers comprise a plurality of glass fibers.

15. The method of claim 9 , wherein the first average length is at least five millimeters.

16. The method of claim 9 , wherein pressure is applied for at least one second.

17. The method of claim 9 , wherein the second average length is less than 1.5 millimeter.

18. The method of claim 9 , wherein after applying pressure the plurality of fibers has an acid absorption of less than 1350%.

19. The method of claim 9 , wherein the plurality of fibers comprise a plurality of C glass fibers.

20. A method of modifying a plurality of fibers, comprising:

applying a first pressure to the plurality of fibers;

removing the first pressure from the plurality of fibers;

rotating the plurality of fibers; and

applying a second pressure to the plurality of fibers,

wherein the plurality of fibers has a first average length before applying the first pressure and a second average length after applying the second pressure, the first average length being greater than the second average length.

21. The method of claim 20 , wherein a pressure selected from the group consisting of the first pressure and the second pressure is at least 50 pounds per square inch.

22. The method of claim 20 , wherein the plurality of fibers comprise a plurality of glass fibers.

23. The method of claim 20 , wherein the first average length is at least five millimeters.

24. The method of claim 20 , wherein a pressure selected from the group consisting of the first pressure and the second pressure is applied for at least one second.

25. The method of claim 20 , wherein the second average length is less than 1.5 millimeters.

26. The method of claim 20 , wherein after applying pressure the plurality of fibers has an acid absorption of less than 1350%.

27. The method of claim 20 , wherein the plurality of fibers comprise a plurality of C glass fibers.

Assignments (3)
NOTICE OF GRANT OF SECURITY INTEREST IN PATENTS Recorded Jan 4, 2022
From: HOLLINGSWORTH & VOSE FIBER COMPANY
To: BANK OF AMERICA, N.A., AS COLLATERAL AGENT
Reel/Frame 058570/0715 →
CHANGE OF NAME Recorded Jan 29, 2018
From: EVANITE FIBER CORPORATION
To: HOLLINGSWORTH & VOSE FIBER COMPANY
Reel/Frame 045183/0204 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 17, 2002
From: REHER, RONALD D.; WINDISCH, JOHN D.; RUSSELL, STEVEN J.
To: EVANITE FIBER CORPORATION
Reel/Frame 013006/0041 →
Continuity (1)
Related Publication 20030182972A1 · Oct 2, 2003