Thermoplastic elastomer compositions

Assignee: Dow Global Technologies Inc.
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,459,500
App. No.
10/429,651
Granted
Dec 2, 2008
Kind
B2
Abstract

A unique thermoplastic olefin composition having: (a) at least 40 percent by weight of a propylene-alpha olefin copolymer based on the total weight of polymers in the composition, the propylene-alpha olefin copolymer having at least 60 percent by weight units derived from propylene, at least 6 percent by weight units derived from an alpha olefin, a molecular weight distribution less than 3.5, and a broad composition distribution; and (b) at least 20 percent by weight of a polypropylene based on the total weight of polymers in the composition, the polypropylene having at least 93 percent by weight units derived from propylene, a molecular weight distribution of greater than 3.5, a heat of fusion greater than the heat of fusion exhibited by the propylene-alpha olefin copolymer, and a melting point T max of at least 120° C.

Claims (14)

1. A thermoplastic olefin composition, comprising:

(a) at least about 40 percent by weight of a propylene-alpha olefin copolymer based on the total weight of polymers in the composition, the propylene-alpha olefin copolymer forming a continuous phase of the composition and the propylene-alpha olefin copolymer having:

(1) at least about 60 percent by weight units derived from propylene;

(2) at least about 5 percent by weight units derived from an alpha olefin;

(3) a molecular weight distribution less than about 3.5;

(4) a broad composition distribution;

(5) a heat of fusion of less than about 40 Joules/gram; and

(6) optionally, a glass transition temperature (Tgp) less than about −10° C.;

(b) at least about 20 percent by weight of a polypropylene based on the total weight of polymers in the composition, the polypropylene having:

(1) at least about 93 percent by weight units derived from propylene;

(2) a heat of fusion greater than the heat of fusion exhibited by the propylene-alpha olefin copolymer; and

(3) a melting point T max of at least about 120° C.; and

(c) at least about 10 percent by weight of an ethylene-alpha olefin elastomer based on the total weight of polymers in the composition.

2. The thermoplastic olefin composition of claim 1 , wherein the ethylene-alpha olefin elastomer is selected from the group consisting of: ethylene-propylene copolymer, ethylene-propylene-diene terpolymer, ethylene-butene copolymer, ethylene-4-methyl-1-pentene copolymer, ethylene-hexene copolymer, ethylene-octene copolymer, ethylene-heptene copolymer and mixtures thereof.

Assignments (2)
CHANGE OF NAME Recorded Jul 28, 2017
From: DOW GLOBAL TECHNOLOGIES INC.
To: DOW GLOBAL TECHNOLOGIES LLC
Reel/Frame 043367/0608 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 8, 2005
From: TAU, LI-MIN; CHEUNG, YUNWA WILSON; DIEHL, CHARLES F.; HAZLITT, LONNIE G.
To: DOW GLOBAL TECHNOLOGIES INC.
Reel/Frame 015876/0292 →
Continuity (1)
Related Publication 20040087751A1 · May 6, 2004