Abstract

According to a previously known method for producing an optical component from synthetic quartz glass, a coaxial arrangement comprising an outer jacket tube, an inner jacket tube that is provided with an internal bore, and a core rod whose bottom face rests on a thrust bearing within the internal bore, is fed into a heating zone in a vertical orientation, is softened therein zone by zone, and is elongated so as to obtain the quartz glass component. In order to create a simple and inexpensive method that is based on said method and makes it possible to reproducibly manufacture a high-quality optical component, the thrust bearing is embodied as a constriction of the internal bore of the inner jacket tube.

Claims (20)

1 . A method for producing an optical component from synthetic quartz glass, said method comprising: feeding a coaxial arrangement comprising an outer jacket tube, an inner jacket tube provided with an internal bore, and a core rod having a lower face end resting on an abutment within the internal bore in vertical orientation to a heating zone, softening said coaxial arrangement therein zonewise and elongating said coaxial arrangement to obtain the optical component, wherein the abutment is configured as a constriction of the internal bore of the inner jacket tube.

2 . The method according to claim 1 , wherein the constriction is provided with an axially continuous opening.

3 . The method according to claim 1 , wherein the core rod comprises a core region having an outer diameter surrounded by a cladding glass layer having an outer diameter wherein a ratio of the outer diameter of the cladding glass layer to the outer diameter of the core region ranges from 2to 4.

4 . The method according to claim 1 , wherein the core rod is formed from butt-jointed core rod pieces.

5 . The method according to claim 4 , wherein the core rod pieces are loosely stacked one upon the other.

6 . The method according to claim 1 , wherein a mechanical stop is provided which prevents an upward movement of the core rod in a direction opposite to a pulling direction.

7 . The method according to claim 1 , wherein the core rod and the inner jack tube define therebetween an inner annular gap with a mean gap width in a range between 0.5 mm and 1.5 mm.

8 . The method according to claim 1 , wherein the inner jack tube and the outer jacket tube define therebetween an outer annular gap with a mean gap width of not more than 2 mm.

9 . The method according claim 1 , wherein the inner jacket tube is movably held in a lateral direction.

10 . The method according to claim 1 , wherein a holding cylinder of quartz glass is fused onto an upper end of the outer jacket tube.

11 . The method according to claim 10 , wherein the holding cylinder has a circumferential groove in which a gripper engages the holding cylinder.

12 . The method according to claim 1 , wherein a first holding means engages an upper end of the outer jacket tube, and a second holding means engages an upper end of the inner jacket tube, the first holding means and the second holding means being mechanically independent of each other.

13 . The method according to any one of claim 1 , wherein a first holding means engages an upper end of the outer jacket tube, and that an upper end of the inner jacket tube is held on the outer jacket tube or on the first holding means.

14 . The method according to claim 13 , wherein the upper end of the inner jacket tube or a mechanical extension of the inner jacket tube is provided with an outer collar which rests on the outer jacket tube or on a mechanical extension thereof.

15 . The method according to claim 1 , wherein the inner jacket tube has a mean hydroxyl group content of less than 1 wt ppm.

16 . The method according to claim 1 , wherein the inner jacket tube is produced by elongating a hollow cylinder which has been mechanically treated to a final dimension.

17 . The method according to claim 1 , wherein the outer jacket tube comprises a hollow cylinder which has been mechanically treated to a final dimension.

18 . The method according to claim 1 , wherein the outer jacket tube is provided with a downwardly tapering lower end.

19 . The method according to claim 1 , wherein the core rod comprises a core region having an outer diameter surrounded by a cladding glass layer having an outer diameter, wherein a ratio of the outer diameter of the cladding glass layer to the outer diameter of the core region ranges from 2.5 to 3.5.

20 . The method according to claim 1 , wherein the inner jacket tube and the outer jacket tube define therebetween an outer annular gap having a mean gap width of not more than 1 mm.

Assignments (3)
CORRECTIVE ASSIGNMENT TO CORRECT REEL/FRAME NO. 020532/0533, PREVIOUSLY RECORDED ON 2/11/08. Recorded Apr 22, 2008
From: HERAEUS TENEVO GMBH
To: HERAEUS QUARZGLAS GMBH & CO. KG
Reel/Frame 021018/0043 →
MERGER Recorded Feb 11, 2008
From: HERAUS TENEVO GMBH
To: HERAEUS QUARZGLAS GMBH & CO. KG
Reel/Frame 020532/0533 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 30, 2006
From: HOFMANN, ACHIM; SCHMITT, CLEMENS; VYDRA, JAN
To: HERAEUS TENEVO GMBH
Reel/Frame 018346/0770 →