Method for controlling average pore diameter of porous body comprising apatite/collagen composite fibers

Assignees: Hoya Corporation; National Institute for Materials Science
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,008,357
App. No.
10/599,435
Granted
Aug 30, 2011
Kind
B2
Abstract

In the process of producing a porous body containing a fibrous apatite/collagen composite by gelating a dispersion comprising the fibrous apatite/collagen composite, collagen and water, freeze-drying the resultant gel to form a porous body, and cross-linking collagen in the porous body, a method for controlling the average pore diameter of the porous body by the solidification time of the gel in the freezing step.

Claims (10)

1. A method for controlling an average pore diameter of a porous body comprising a fibrous apatite/collagen composite, said porous body being produced by:

gelating a dispersion comprising said fibrous apatite/collagen composite, collagen and water;

freeze-drying the resultant gel to form a porous body; and

cross-linking the collagen in said porous body,

wherein the average pore diameter of the porous body is controlled by the following in the following order:

a) freezing pluralities of gels at various freezing-environment temperatures and measuring the solidification time of each gel to prepare a graph showing the relation between the freezing-environment temperature and the solidification time;

b) measuring the average pore diameter of the porous body obtained at various lengths of solidification time to prepare a graph showing the relation between solidification time and average pore diameter;

c) determining the solidification time for providing a desired average pore diameter of said porous body from the graph of the solidification time and the average pore diameter; and

d) determining the freezing-environment temperature for achieving the determined solidification time from the graph of the freezing-environment temperature and the solidification time.

2. The method for controlling the average pore diameter according to claim 1 , wherein the temperature for keeping said gel for freezing is −100° C. to 0° C.

Assignments (2)
MERGER Recorded Jul 26, 2011
From: PENTAX CORPORATION
To: HOYA CORPORATION
Reel/Frame 026652/0086 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 12, 2006
From: SHOJI, DAISUKE; KAWAMURA, KATSUMI; NAKAJIMA, TAKEHIKO; TANAKA, JUNZO; KIKUCHI, MASANORI; IKOMA, TOSHIYUKI; MOCHIZUKI, NAOMI
To: PENTAX CORPORATION; NATIONAL INSTITUTE FOR MATERIALS SCIENCE
Reel/Frame 018618/0255 →
Priority Claims (1)
JP 2004-100765 · Mar 30, 2004 · national
Continuity (1)
Related Publication 20080234396A1 · Sep 25, 2008