Accelerated test method for ferroelectric memory device
An accelerated test method evaluates, under accelerated conditions (a temperature T 2 and a voltage V 2 ), an endurance characteristic of a ferroelectric memory device having a capacitor element including a ferroelectric film under actual operating conditions (a temperature T 1 and a voltage V 1 ). An acceleration factor (K) required to evaluate the endurance characteristic is derived by using an expression: logK=A(1/V 1 −1/V 2 )+B(1/V 1 T 1 −1/V 2 T 2 ) (where each of A and B is a constant).
1. An accelerated test method for evaluating, under accelerated conditions (a temperature T 2 and a voltage V 2 ), an endurance characteristic of a ferroelectric memory device comprising a capacitor element having a ferroelectric film under actual operating conditions (a temperature T 1 and a voltage V 1 ), the method comprising the step of:
deriving an acceleration factor (K) required to evaluate the endurance characteristic by using a following expression (1):
log K=A (1/ V 1 −1 /V 2 )+ B (1/ V 1 T 1 −1 /V 2 T 2 )
(where each of A and B is a constant),
the method further comprising the sub-steps:
determining the number (Lc) of occurrences of polarization inversion when a remanence of the ferroelectric film reaches a specified decrease rate at each of a plurality of polarization inversion voltages (V) at a plurality of temperatures;
determining a constant (α) at a specified temperature (T) by using a following expression (2):
log Lc=C+α/V (where each of C and α is a constant) (2); and
determining the constants A and B by using a following expression (3):
α= A+B/T (3).