Method of producing an exfoliated polymer-clay nanocomposite through solid-state shear pulverization
A method of producing a polymer-clay nanocomposite comprises providing a supply of polymer-clay mixture, exfoliating the mixture through solid-state shear pulverization in the presence of cooling sufficient to maintain the extruded mixture in the solid state during the pulverization, and discharging the resulting exfoliated mixture. The invention is also directed to a method of producing a polymer hybrid nanocomposite, wherein a component is dispersed throughout a polymer matrix by solid-state shear pulverization of a polymer mixed with the second component.
1. A method of producing a polymer-clay nanocomposite, comprising the steps of:
providing a polymer-clay mixture comprising a polymer and clay;
exfoliating the clay through solid-state shear pulverization in a twin-screw pulverizer and in the presence of cooling sufficient to maintain the mixture in the solid state during the pulverization; and
discharging the mixture as a polymer-clay nanocomposite containing the exfoliated clay.
2. The method of claim 1 , wherein the mixture comprises at least about 3 wt % organoclay.
3. The method of claim 1 , wherein the mixture comprises about 10 wt % organoclay.
4. The method of claim 3 , wherein the organoclay contains between about 40–50 wt % clay and between about 50–60 wt % organic content.
5. The method of claim 4 , wherein the organoclay is a montmorillonite.
6. The method of claim 1 , wherein the polymer-clay mixture comprises a polymer selected from the group consisting of polypropylene, polyolefins, polystyrene, polymethacrylates, poly(ethylene-co-vinyl acetate), polyhydroxystyrene, poly (vinyl pyridine), polyvinylalcohol, polyacrylamide, polycaprolactone, copolymers of ethylene, copolymers of propylene, copolymers of acetate, poly (ethylene terephthalate), nylon, and blends thereof.
7. The method of claim 1 , further comprising a step of cooling a pulverizer barrel with a chilled fluid to about 10° Celsius during the pulverization.
8. The method of claim 1 , wherein the clay comprises an organoclay, and wherein the polymer comprises a nonpolar polymer.
9. A method of producing a polymer-clay nanocomposite, comprising the steps of:
melt extruding a polymer-clay mixture comprising a polymer and clay;
exfoliating the clay through solid-state shear pulverization in a twin-screw pulverizer and in the presence of cooling sufficient to maintain the mixture in the solid state during the pulverization; and
discharging the mixture as a polymer-clay nanocomposite containing the exfoliated clay.
10. The method of claim 9 , wherein the mixture comprises at least about 3 wt % organoclay.
11. The method of claim 10 , wherein the organoclay contains between about 40–50 wt % clay and between about 50–60 wt % organic content.
12. The method of claim 11 , wherein the organoclay is a montmorillonite.
13. The method of claim 9 , wherein the mixture comprises about 10 wt % organoclay.
14. The method of claim 9 , wherein the polymer-clay mixture comprises a polymer selected from the group consisting of polypropylene, polyolefins, polystyrene, polymethacrylates, poly(ethylene-co-vinyl acetate), polyhydroxystyrene, poly (vinyl pyridine), polyvinylalcohol, polyacrylamide, polycaprolactone, copolymers of ethylene, copolymers of propylene, copolymers of acetate, poly (ethylene terephthalate), nylon, and blends thereof.
15. The method of claim 9 , further comprising a step of cooling a pulverizer barrel with a chilled fluid to about 10° Celsius during the pulverization.
16. The method of claim 9 , wherein the clay comprises an organoclay, and wherein the polymer comprises a nonpolar polymer.