Method for the production of an elastic laminate material web

Inventor: Marcus Schoenbeck (Gronau, DE)
Assignee: Mondi Gronau GmbH
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,562,783
App. No.
11/152,425
Granted
Oct 22, 2013
Kind
B2
Abstract

A method for the production of an elastic laminate material web comprises laminating a cover material onto a carrier film consisting of a thermoplastic elastomer, using a hot-melt glue. The carrier film is rolled off a film roll and has a polymer powder on at least one side, to prevent interlocking of the layers of the carrier film in the film roll. The melt temperature of the powder is less than or equal to the gluing temperature of the hot-melt glue, so that the powder melts during lamination.

Claims (33)

1. In a process for the production of an elastic laminate material web, comprising the following steps:

processing a carrier film made of a thermoplastic elastomer from a film roll;

laminating a cover material on at least one side of the carrier film using a hot melt glue which is applied to the carrier film at a glue temperature;

wherein the carrier film is a mono-film produced by extrusion from a polymer selected from the group consisting of styrene-isoprene-styrene block copolymer, styrene-butadiene-styrene block copolymer, styrene ethylene/butylene block copolymer, polyurethanes and ethylene copolymers,

wherein the improvement comprises:

applying a polymer powder directly to a surface of the carrier film on at least one side of the carrier film prior to the carrier film being rolled to prevent the carrier film from sticking to itself in the film roll,

wherein the material in said film roll consists of said carrier film provided as a mono-film and said polymer powder, which acts as a spacer in the storaae of said film roll, and

wherein the powder is present on the carrier film at a weight per area of less than or equal to 1 g/m 2 ,

wherein the powder consists of a polyethylene or ethylene vinyl acetate having a melt temperature which is less than the glue temperature of the hot melt glue applied to the carrier film, so that the powder melts and mixes into the hot melt glue during the step of laminating.

2. A method according to claim 1 , wherein the cover material is laminated onto the carrier film on both sides of the carrier film.

3. A method according to claim 1 , wherein the cover material is a textile material.

4. A method according to claim 1 , wherein the hot-melt glue is selected from the group of SIS-based and SBS-based polymers.

5. A method according to claim 1 , wherein the hot-melt glue is applied to each side of the carrier film to which the cover material is laminated at a weight per area unit between 7 and 20 g/m 2 .

6. A method according to claim 1 , wherein a ratio of weight per area unit of the hot melt glue and the powder is at least 7:1.

7. In a process for the production of an elastic laminate material web, comprising the following steps:

processing a carrier film made of a thermoplastic elastomer from a film roll;

laminating a cover material on at least one side of the carrier film using a hot melt glue which is applied to the carrier film at a glue temperature;

wherein the carrier film is a mono-film produced by extrusion from a polymer selected from the group consisting of styrene-isoprene-styrene block copolymer, styrene-butadiene-styrene block copolymer, styrene ethylene/butylene-styrene block copolymer, polyurethanes and ethylene copolymers,

wherein the improvement comprises:

applying a polymer powder directly to a surface of the carrier film on at least one side of the carrier film prior the carrier film being rolled to prevent the carrier film from sticking to itself in the film roll, and

blowing or brushing off the surface of the carrier film after the film is unrolled and prior to laminating so that residual powder is present on the carrier film at a weight per area of less than or equal to 1 g/m 2 during the step of laminating,

wherein the material in said film roll consists of said carrier film provided as a mono-film and said polymer powder, which acts as a spacer in the storage of said film roll, and

wherein the powder consists of a polyethylene or ethylene vinyl acetate having a melt temperature which is less than the glue temperature of the hot melt glue applied to the carrier film, so that the powder melts and mixes into the hot melt glue during the step of laminating.

8. A method according to claim 7 , wherein a ratio of weight per area unit of the hot melt glue and the powder is at least 7:1.

9. In a process for the production of an elastic laminate material web, comprising the following steps:

processing a carrier film made of a thermoplastic elastomer from a film roll;

laminating a cover material on at least one side of the carrier film using a hot melt glue which is applied to the carrier film at a glue temperature;

wherein the carrier film is a mono-film produced by extrusion from a polymer selected from the group consisting of styrene-isoprene-styrene block copolymer, styrene-butadiene-styrene block copolymer, styrene ethylene/butylene block copolymer, polyurethanes and ethylene copolymers,

wherein the improvement comprises:

applying a polymer powder directly to a surface of the carrier film on at least one side of the carrier film prior to the carrier film being rolled to prevent the carrier film from sticking to itself in the film roll,

wherein the material in said film roll consists of said carrier film provided as a mono-film and said polymer powder, which acts as a spacer in the storage of said film roll, and

wherein the powder consists of a polyethylene or ethylene vinyl acetate having a melt temperature which is less than the glue temperature of the hot melt glue applied to the carrier film, so that the powder melts and mixes into the hot melt glue during the step of laminating.

10. A method according to claim 9 , wherein a ratio of weight per area unit of the hot melt glue and the powder is at least 7:1.

Assignments (2)
CHANGE OF NAME Recorded Aug 7, 2013
From: NORDENIA DEUTSCHLAND GRONAU GMBH
To: MONDI GRONAU GMBH
Reel/Frame 031077/0901 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 8, 2005
From: SCHONBECK, MARCUS
To: NORDENIA DEUTSCHLAND GRONAU GMBH
Reel/Frame 016864/0667 →
Priority Claims (1)
EP 05007885 · Apr 11, 2005 · regional
Continuity (1)
Related Publication 20060225835A1 · Oct 12, 2006