Method for measuring the degree of crosslinking of pressure sensitive adhesive

Assignee: Daxon Technology Inc.
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,405,828
App. No.
11/453,805
Granted
Jul 29, 2008
Kind
B2
Abstract

A method for measuring the degree of crosslinking of pressure sensitive adhesive. The method, having the advantages of simple steps and short measuring time, comprises immersing a transparent substrate coated with a pressure sensitive adhesive in a solvent. After a specific period, the haze of the transparent substrate is measured. The obtained haze is compared with a predetermined reference, thereby determining the degree of crosslinking of the pressure sensitive adhesive.

Claims (14)

1. A method for measuring the degree of crosslinking of pressure sensitive adhesive, comprising:

providing a transparent substrate coated with a pressure sensitive adhesive;

immersing the transparent substrate in a solvent;

measuring the haze of the transparent substrate; and

comparing the obtained haze with a predetermined reference, thereby concluding the degree of crosslinking of the pressure sensitive adhesive.

2. The method as claimed in claim 1 , wherein the transparent substrate comprises substrate employed in LCD or transparent optical film.

3. The method as claimed in claim 1 , wherein the transparent substrate is glass.

4. The method as claimed in claim 1 , wherein the transparent substrate comprises triacetate cellulose film, release film, antireflection film, or polarizing film.

5. The method as claimed in claim 1 , wherein the pressure sensitive adhesive comprises natural rubber pressure sensitive adhesive, synthetic rubber pressure sensitive adhesive, or alkene polymer pressure sensitive adhesive.

6. The method as claimed in claim 1 , wherein the pressure sensitive adhesive is polyacrylate.

7. The method as claimed in claim 1 , wherein the transparent substrate is immersed in the solvent for 2˜4 min.

8. The method as claimed in claim 1 , wherein the solvent comprises alcohol, alkane, ether, or ester.

9. The method as claimed in claim 1 , wherein the solvent comprises methanol, ethanol, n-propanol, i-propanol, n-butanol, n-hexane, ethyl ether, tetrahydrofuran, or ethyl acetate.

10. The method as claimed in claim 1 , wherein the predetermined reference indicates the relationship between haze and gel fraction.

Assignments (2)
CHANGE OF NAME Recorded Jan 19, 2015
From: DAXON TECHNOLOGY INC.
To: BENQ MATERIALS CORPORATION
Reel/Frame 034741/0434 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 16, 2006
From: TAN, YI-HUI; KUO, HAO-FEI; LO, JEN-YEN
To: DAXON TECHNOLOGY INC.
Reel/Frame 017981/0831 →
Priority Claims (1)
TW 94144442 A · Dec 15, 2005 · national
Continuity (1)
Related Publication 20070139650A1 · Jun 21, 2007