Preparation method of 1,5-dimethyltetralin using dealuminated zeolite beta catalyst
The present invention relates to a method for preparing 1,5-dimethyltetralin using a dealuminated zeolite beta catalyst. The preparation method of 1,5-dimethyltetralin according to the present invention has the effects of not only showing high conversion and high selectivity of 1,5-dimethyltetralin but also of suppressing deactivation of a zeolite beta catalyst so as to enhance the catalyst life, by using the dealuminated zeolite beta catalyst.
1. A method for preparing 1,5-dimethyltetralin comprising:
adding 5-ortho-tolylpentene to a vessel;
adding a dealuminated zeolite beta catalyst to the vessel, wherein the dealuminated zeolite beta catalyst has a SiO2/Al2O3 molar ratio of 14 and an average particle size of 1.5 mm; and
heating the vessel to a temperature of 120° C. at normal pressure to recover 1,5-dimethyltetralin, wherein 1,5-dimethyltetralin is recovered at a conversion % value of 100%.