Method of using landplaster as a wallboard filler
A gypsum slurry includes calcium sulfate hemihydrate, water and calcium sulfate dihydrate, where the calcium sulfate dihydrate is added downstream of the mixer. In an optional embodiment, the a gypsum slurry includes calcium sulfate hemihydrate, a polycarboxylate dispersant, water and coated calcium sulfate dihydrate. In this case, the hydrophilic, dispersible coating is selected to serve as a modifier to enhance the ability of the dispersant to fluidize the gypsum slurry.
1. A method of making a gypsum slurry comprising:
combining calcium sulfate hemihydrate, a set retarder and water in a mixer to make a gypsum slurry;
introducing foam into the gypsum slurry; and
adding calcium sulfate dihydrate to the gypsum slurry downstream of the mixer.
2. The method of claim 1 wherein said combining step comprises mixing.
3. The method of claim 1 wherein said introducing step comprises making a second slurry of landplaster, water and a foaming agent prior to said adding step and wherein said adding step comprises adding said landplaster in said second slurry downstream of the mixer.
4. The method of claim 1 further comprising measuring an amount of calcium sulfate dihydrate to be from about 3% to about 10% of the total amount of calcium sulfate materials.
5. The method of claim 1 , wherein said combining step further comprises adding a polycarboxylate dispersant and a modifier for enhancing performance of said dispersant, wherein said modifier is selected from the group consisting of cement, lime, slaked lime, soda ash, potash, carbonates, silicates, hydroxides, phosphonates and phosphates.
6. The method of claim 1 , further comprising adding at least one of the group consisting of a modifier, a fluidity enhancing component, a trimetaphosphate compound, a set accelerator and a thickener to the slurry prior to said dividing step.
7. The method of claim 1 further comprising treating the landplaster with a coating solution prior to said adding step.
8. The method of claim 7 wherein said adding step further comprises adding the coated landplaster in the coating solution to the slurry.