Thermoresponsive polymer and production method thereof
A material which expresses its critical solution temperature even in an aqueous solution containing a buffer or salt, and at the same time, shows small variation width of the critical solution temperature even when concentration of salt or the like contained in water, a buffer liquid or the like is different, interacts with a substance such as a component in the living body and can therefore be used efficiently in the isolation of substances, is provided. A monomer represented by a formula (1) and a thermoresponsive polymer which contains said monomer as a polymerization component.
1. A thermoresponsive polymer obtained by polymerizing the monomer represented by a formula (1)
wherein R 1 is hydrogen or methyl,
wherein when R 1 is hydrogen, R 2 is carbamoyl, or at least one group selected from the class consisting of methyl, ethyl, propyl, butyl, pentyl, hexyl, cyclopentyl, cyclohexyl, cycloheptyl, methoxy, ethoxy, propoxy, butoxy, pentyloxy and hexyloxy, wherein one or more hydrogen atoms are substituted by carbamoyl; or
wherein when R 1 is methyl, R 2 is carbamoyl, or at least one group selected from the class consisting of methyl, propyl, butyl, pentyl, hexyl, cyclopentyl, cyclohexyl, cycloheptyl, methoxy, ethoxy, propoxy, butoxy, pentyloxy and hexyloxy, wherein one or more hydrogen atoms are substituted by carbamoyl.
2. A thermoresponsive polymer obtained by polymerizing only the monomer represented by a formula (1)
wherein R 1 is hydrogen or methyl, and R 2 is carbamoyl, or at least one group selected from the class consisting of methyl, ethyl, propyl, butyl, pentyl, hexyl, cyclopentyl, cyclohexyl, cycloheptyl, methoxy, ethoxy, propoxy, butoxy, pentyloxy and hexyloxy, wherein one or more hydrogen atoms are substituted by carbamoyl.
3. The thermoresponsive polymer described in claim 1 , which has a number average molecular weight of from 10 3 to 10 6 .
4. The thermoresponsive polymer described in claim 2 , which has a number average molecular weight of from 10 3 to 10 6 .
5. A method for producing the thermoresponsive polymer described in claim 1 , which comprises treating a polymerization solvent containing a monomer represented by the formula (1) and an initiator with a temperature or light capable of generating a radical from the initiator to perform a polymerization.
6. A method for producing the thermoresponsive polymer described in claim 2 , which comprises treating a polymerization solvent containing a monomer represented by the formula (1) and an initiator with a temperature or light capable of generating a radical from the initiator to perform a polymerization.