IP Library › Granted Patent US 8,003,255
Granted Patent B2
US 8,003,255 · App. 11/937,042 · Granted Aug 23, 2011

Nonaqueous electrolyte battery, lithium titanium composite oxide and battery pack

Assignee: Kabushiki Kaisha Toshiba
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,003,255
App. No.
11/937,042
Granted
Aug 23, 2011
Kind
B2
Abstract

A nonaqueous electrolyte battery is provided and includes: a negative electrode including a lithium titanium composite oxide showing an X-ray diffraction pattern in which each of main peak intensities of rutile TiO 2 , anatase TiO 2 and Li 2 TiO 3 is 5 or less with respect to a main peak intensity of ramsdellite lithium titanate of 100; a positive electrode; and a nonaqueous electrolyte.

Claims (27)

1. A nonaqueous electrolyte battery comprising:

a negative electrode including a lithium titanium composite oxide showing an X-ray diffraction pattern in which each of main peak intensities of rutile TiO 2 , anatase TiO 2 and Li 2 TiO 3 is 5 or less with respect to a main peak intensity of ramsdellite lithium titanate of 100;a positive electrode; and

a nonaqueous electrolyte,

wherein the lithium titanium composite oxide includes at least one element selected from the group consisting of B, Na, and K.

2. The nonaqueous electrolyte battery according to claim 1 , wherein the lithium titanium composite oxide shows an X-ray diffraction pattern in which each of main peak intensities of rutile TiO 2 , anatase TiO 2 and Li 2 TiO 3 is 3 or less with respect to a main peak intensity of ramsdellite lithium titanate of 100.

3. The nonaqueous electrolyte battery according to claim 1 , wherein the lithium titanium composite oxide includes the at least one element in an amount of 0.01 to 5 wt %.

4. The nonaqueous electrolyte battery according to claim 1 , wherein the at least element is segregated on an interface of a crystallite of the lithium titanium composite oxide.

5. The nonaqueous electrolyte battery according to claim 1 , wherein the lithium titanium composite oxide has a crystallite diameter of 80.1 nm or less.

6. The nonaqueous electrolyte battery according to claim 1 , wherein the nonaqueous electrolyte includes a mixture solvent of two or more selected from the group consisting of propylene carbonate, ethylene carbonate, and y-butyrolactone.

7. The nonaqueous electrolyte battery according to claim 1 , wherein the nonaqueous electrolyte includes y-butyrolactone.

8. A nonaqueous electrolyte battery comprising:

a negative electrode including a lithium titanium composite oxide showing an X-ray diffraction pattern in which each of main peak intensities of rutile TiO 2 , anatase TiO 2 and Li 2 TiO 3 is 5 or less with respect to a total of main peak intensities of ramsdellite lithium titanate and spinel lithium titanate of 100;

a positive electrode; and

a nonaqueous electrolyte,

wherein the lithium titanium composite oxide includes at least one element selected from the group consisting of B, Na, and K.

9. The nonaqueous electrolyte battery according to claim 8 , wherein a ratio of the main peak intensity of ramsdellite lithium titanate to the main peak intensity of spinel lithium titanate falls within a range from 1:9 to 5:5.

10. A lithium titanium composite oxide showing an X-ray diffraction pattern in which each of main peak intensities of rutile TiO 2 , anatase TiO 2 and Li 2 TiO 3 is 5 or less with respect to a main peak intensity of ramsdellite lithium titanate of 100,

wherein the lithium titanium composite oxide includes at least one element selected from the group consisting of B, Na, and K.

11. A battery pack comprising a plurality of nonaqueous electrolytic batteries, each of the nonaqueous electrolyte batteries includes:

a negative electrode including a lithium titanium composite oxide showing an X-ray diffraction pattern in which each of main peak intensities of rutile TiO 2 , anatase TiO 2 and Li 2 TiO 3 is 5 or less with respect to a main peak intensity of ramsdellite lithium titanate of 100; a positive electrode; and

a nonaqueous electrolyte,

wherein the lithium titanium composite oxide includes at least one element selected from the group consisting of B, Na, and K.

12. A battery pack comprising a plurality of nonaqueous electrolytic batteries, wherein each of the nonaqueous electrolyte batteries includes:

a negative electrode including a lithium titanium composite oxide showing an X-ray diffraction pattern in which each of main peak intensities of rutile TiO 2 , anatase TiO 2 and Li 2 TiO 3 is 5 or less with respect to a total of main peak intensities of ramsdellite lithium titanate and spinel lithium titanate of 100;

a positive electrode; and

a nonaqueous electrolyte,

wherein the lithium titanium composite oxide includes at least one element selected from the group consisting of B, Na, and K.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 13, 2007
From: INAGAKI, HIROKI; HARADA, YASUHIRO; TAKAMI, NORIO
To: KABUSHIKI KAISHA TOSHIBA
Reel/Frame 020104/0727 →
Priority Claims (1)
JP 2006-305285 · Nov 10, 2006 · national
Continuity (1)
Related Publication 20080113264A1 · May 15, 2008