IP Library Granted Patent US 7,850,865
Granted Patent B1
US 7,850,865 · App. 12/127,252 · Granted Dec 14, 2010

Highly concentrated foam formulation for blast mitigation

Assignee: Sandia Corporation
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,850,865
App. No.
12/127,252
Granted
Dec 14, 2010
Kind
B1
Abstract

A highly concentrated foam formulation for blast suppression and dispersion mitigation for use in responding to a terrorism incident involving a radiological dispersion device. The foam formulation is more concentrated and more stable than the current blast suppression foam (AFC-380), which reduces the logistics burden on the user.

Claims (76)

1. A highly concentrated blast foam concentrate composition, comprising:

1-5 wt % nonionic polymer;

1-8 wt % anionic polymer viscosity enhancer/thickener;

5-18 wt % first anionic surfactant foaming agent;

1-4 wt % foam stabilizer;

5-25 wt % solvent;

5-15 wt % alcohol; and

25-75 wt % second anionic surfactant foaming agent;

wherein the nonionic polymer is selected from the group consisting of 2-hydroxyethylcellulose, carboxymethyl cellulose, polyanionic cellulose, hydroxymethylcellulose, hydroxypropylcellulose, and hydroxypropylmethyl cellulose.

2. The concentrate composition of claim 1 , wherein the anionic polymer viscosity enhancer/thickener is selected from the group consisting of Xantham gum, Guar gum, agar, carrageenan, sodium alginate, caseinate, and natural or synthetic polysaccharide polymers.

3. A highly concentrated blast foam concentrate composition, comprising:

1-5 wt % nonionic polymer;

1-8 wt % anionic polymer viscosity enhancer/thickener;

5-18 wt % first anionic surfactant foaming agent;

1-4 wt % foam stabilizer;

5-25 wt % solvent;

5-15 wt % alcohol; and

25-75 wt % second anionic surfactant foaming agent;

wherein the first anionic surfactant foaming agent is selected from the group consisting of sodium dodecyl sulfate, carboxylic acid salts, sulfonic acid salts, sulfuric acid ester salts, and phosphoric acid esters.

4. A highly concentrated blast foam concentrate composition, comprising:

1-5 wt % nonionic polymer;

1-8 wt % anionic polymer viscosity enhancer/thickener;

5-18 wt % first anionic surfactant foaming agent;

1-4 wt % foam stabilizer;

5-25 wt % solvent;

5-15 wt % alcohol; and

25-75 wt % second anionic surfactant foaming agent;

wherein the foam stabilizer is selected from the group consisting of n-dodecanol, n-tetradecanol, n-tridecanol, and n-hexadecanol.

5. A highly concentrated blast foam concentrate composition, comprising:

1-5 wt % nonionic polymer;

1-8 wt % anionic polymer viscosity enhancer/thickener;

5-18 wt % first anionic surfactant foaming agent;

1-4 wt % foam stabilizer;

5-25 wt % solvent;

5-15 wt % alcohol; and

25-75 wt % second anionic surfactant foaming agent;

wherein the solvent is selected from the group consisting of diethylene glycol monobutyl ether, tripropylene glycol methyl ether, propylene glycol, hexylene glycol, ethylene glycol, and ether solvents.

6. A highly concentrated blast foam concentrate composition, comprising:

1-5 wt % nonionic polymer;

1-8 wt % anionic polymer viscosity enhancer/thickener;

5-18 wt % first anionic surfactant foaming agent;

1-4 wt % foam stabilizer;

5-25 wt % solvent;

5-15 wt % alcohol; and

25-75 wt % second anionic surfactant foaming agent;

wherein the alcohol is selected from the group consisting of isobutanol (iBOH), tert-butanol, propanol, isopropyl alcohol, and low molecular weight alcohols.

7. A highly concentrated blast foam concentrate composition, comprising:

1-5 wt % nonionic polymer;

1-8 wt % anionic polymer viscosity enhancer/thickener;

5-18 wt % first anionic surfactant foaming agent;

1-4 wt % foam stabilizer;

5-25 wt % solvent;

5-15 wt % alcohol; and

25-75 wt % second anionic surfactant foaming agent;

wherein the second anionic surfactant foaming agent is selected from the group consisting of BioTerge AS-40, alpha-olefin sulfonate anionic surfactant, carboxylic acid salts, sulfonic acid salts, sulfuric acid ester salts, and phosphoric acid esters.

8. A highly concentrated blast foam concentrate composition, comprising:

3.0 wt % 2-hydroxyethylcellulose;

4.4 wt % xantham gum;

13.7 wt % sodium dodecyl sulfate;

2.4 wt % n-dodecanol;

15.7 wt % diethylene glycol monobutyl ether;

10.0 wt % isobutanol; and

50.8 wt % alpha-olefin sulfonate anionic surfactant.

9. A highly concentrated blast foam concentrate composition, consisting of:

3.0 wt % 2-hydroxyethylcellulose;

4.4 wt % xantham gum;

13.7 wt % sodium dodecyl sulfate;

2.4 wt % n-dodecanol;

15.7 wt % diethylene glycol monobutyl ether;

10.0 wt % isobutanol; and

50 . 8 wt % alpha-olefin sulfonate anionic surfactant.

10. The concentrate composition of claim 3 , wherein the anionic polymer viscosity enhancer/thickener is selected from the group consisting of Xantham gum, Guar gum, agar, carrageenan, sodium alginate, caseinate, and natural or synthetic polysaccharide polymers.

11. The concentrate composition of claim 4 , wherein the anionic polymer viscosity enhancer/thickener is selected from the group consisting of Xantham gum, Guar gum, agar, carrageenan, sodium alginate, caseinate, and natural or synthetic polysaccharide polymers.

12. The concentrate composition of claim 5 , wherein the anionic polymer viscosity enhancer/thickener is selected from the group consisting of Xantham gum, Guar gum, agar, carrageenan, sodium alginate, caseinate, and natural or synthetic polysaccharide polymers.

13. The concentrate composition of claim 6 , wherein the anionic polymer viscosity enhancer/thickener is selected from the group consisting of Xantham gum, Guar gum, agar, carrageenan, sodium alginate, caseinate, and natural or synthetic polysaccharide polymers.

14. The concentrate composition of claim 7 , wherein the anionic polymer viscosity enhancer/thickener is selected from the group consisting of Xantham gum, Guar gum, agar, carrageenan, sodium alginate, caseinate, and natural or synthetic polysaccharide polymers.

Assignments (4)
CHANGE OF NAME Recorded Sep 27, 2018
From: SANDIA CORPORATION
To: NATIONAL TECHNOLOGY & ENGINEERING SOLUTIONS OF SANDIA, LLC
Reel/Frame 047157/0622 →
CONFIRMATORY LICENSE Recorded Sep 26, 2008
From: SANDIA CORPORATION
To: ENERGY, U.S. DEPARTMENT OF
Reel/Frame 021597/0194 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 30, 2008
From: DUGGER, MICHAEL T.; OHLHAUSEN, JAMES A.
To: SANDIA CORPORATION, OPERATOR OF SANDIA NATIONAL LABORATORIES
Reel/Frame 021027/0517 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 29, 2008
From: TUCKER, MARK D.; GAO, HUIZHEN
To: SANDIA CORPORATION, OPERATOR OF SANDIA NATIONAL LABORATORIES
Reel/Frame 021024/0948 →