Method for determining degree of aging of a polymer resin material

Assignee: The Boeing Company
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,956,327
App. No.
12/235,399
Granted
Jun 7, 2011
Kind
B2
Abstract

A method of determining degree of aging of an incompletely cured polymer resin material collecting IR spectra on a series of standards with carefully controlled aging time and data collected at appropriate time intervals with the standard LC method for determining cure condition of the material, using said spectra and LC data to make a multivariate calibration model and using said model to predict the cure condition of uncured samples of interest.

Claims (39)

1. A method of determining degree of aging of an incompletely cured polymer resin material comprising the steps of:

irradiating said polymer resin material with infrared energy over a spectrum of wavelengths;

detecting said infrared energy reflected from said polymer resin over said spectrum of wavelengths;

performing multivariate analysis on the spectrum of said reflected infrared energy;

comparing results of said multivariate analysis with a predetermined correlation between model infrared energy spectra comprising said spectrum of wavelengths collected from a plurality of model polymer resin samples, said model polymer resin samples each comprising a different degree of aging; and,

determining a degree of aging of said polymer resin material level based on said predetermined correlation.

2. The method of claim 1 , wherein said multivariate analysis comprises multivariate statistical approaches to determine changes in absorbance and/or reflectance values at selected groups of wavelengths comprising said spectrum of wavelengths, said changes with respect to a reference spectrum.

3. The method of claim 1 , wherein said incompletely cured polymer resin material comprises a material selected from the group consisting of an adhesive, a surface treating material, and a fiber resin composite material impregnated with said incompletely cured polymer resin material.

4. The method of claim 1 , wherein said incompletely cured polymer resin material comprises carbon fiber reinforced composite sheet material impregnated with said incompletely cured polymer resin material.

5. The method of claim 1 , wherein said different level of aging in said model polymer resin material is determined by an independent chemical analysis.

6. The method of claim 5 , wherein said independent chemical analysis comprises high pressure liquid chromatography (HPLC).

7. The method of claim 1 , wherein said step of irradiating said polymer resin material is preceded by collecting a reference spectrum over said spectrum of wavelengths from a reference sample wherein said polymer resin material is present at a predetermined degree of aging.

8. The method of claim 1 , wherein said step of irradiating said polymer resin material is preceded by a calibration process comprising collecting reference spectra over said spectrum of wavelengths from a reference sample comprising a predetermined IR spectroscopy measurement spectrum.

9. The method of claim 1 , wherein said steps comprise a near-IR measurement and said spectrum of wavelengths comprises a range of wavelengths from about 2.5 to 25 microns.

10. The method of claim 1 , wherein said steps comprise a Fourier Transform (FT)-IR measurement and said spectrum of wavelengths comprises a range of wavelengths from about 2.5 to 25 microns.

11. The method of claim 1 , wherein said steps are performed by a hand-held portable IR spectrometer.

12. The method of claim 1 , wherein said steps comprise a process selected from the group consisting of aircraft manufacturing, aircraft assembly, aircraft maintenance, and aircraft repair.

13. A method of determining degree of aging of an incompletely cured polymer resin material comprising the steps of:

collecting a reference spectrum over a spectrum of infrared wavelengths from a reference sample wherein said polymer resin material is present at a predetermined level of aging;

irradiating said polymer resin material with infrared energy over a spectrum of wavelengths;

detecting said infrared energy reflected from said ed polymer resin over said spectrum of wavelengths;

performing multivariate analysis on the spectrum of said reflected infrared energy;

comparing results of said multivariate analysis with a predetermined correlation between model infrared energy spectra comprising said spectrum of wavelengths collected from a plurality of model polymer resin samples, said model polymer resin samples each comprising a different level of aging; and,

determining a level of aging of said polymer resin material based on said predetermined correlation.

14. The method of claim 13 , wherein said multivariate analysis comprises multivariate statistical approaches to determine changes in absorbance and/or reflectance values at selected groups of wavelengths comprising said spectrum of wavelengths, said changes with respect to a reference spectrum.

15. The method of claim 13 , wherein said incompletely cured polymer resin material comprises a material selected from the group consisting of an adhesive, a surface treating material, and a fiber resin composite material impregnated with said incompletely cured polymer resin material.

16. The method of claim 13 , wherein said incompletely cured polymer resin material comprises carbon fiber reinforced composite sheet material impregnated with said incompletely cured polymer resin material.

17. The method of claim 13 , wherein said different level of aging in said model polymer resin material is determined by an independent chemical analysis.

18. The method of claim 17 , wherein said independent chemical analysis comprises high pressure liquid chromatography (HPLC).

19. The method of claim 13 , wherein said steps comprise a near-IR measurement and said spectrum of wavelengths comprises a range of wavelengths from about 2.5 to 25 microns.

20. The method of claim 13 , wherein said steps comprise a Fourier Transform (FT)-IR measurement and said spectrum of wavelengths comprises a range of wavelengths from about 2.5 to 25 microns.

21. The method of claim 13 , wherein said steps are performed by a hand-held portable IR spectrometer.

22. The method of claim 13 , wherein said steps comprise a process selected from the group consisting of aircraft manufacturing, aircraft assembly, aircraft maintenance, and aircraft repair.

23. A method of determining degree of aging of an incompletely cured polymer resin material impregnated into a carbon fiber reinforced composite sheet material comprising:

irradiating said sheet material with infrared energy over a spectrum of wavelengths;

detecting said infrared energy reflected from said sheet material over said spectrum of wavelengths;

performing multivariate analysis on the spectrum of said reflected infrared energy;

comparing results of said multivariate analysis with a predetermined correlation between model infrared energy spectra comprising said spectrum of wavelengths collected from a plurality of model sheet material samples, said model sheet material samples each comprising a different degree of aging of said polymer resin material; and,

determining a degree of aging of said polymer resin material in said sheet material based on said predetermined correlation.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 22, 2008
From: SHELLEY, PAUL H.; WERNER, GREGORY J.; BARATTO, JOE
To: THE BOEING COMPANY
Reel/Frame 021566/0787 →
Continuity (1)
Related Publication 20100276578A1 · Nov 4, 2010