Method of protecting wood through enhanced penetration of wood preservatives and a related solution

Assignee: Kop-Coat, Inc.
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,896,960
App. No.
12/236,044
Granted
Mar 1, 2011
Kind
B2
Abstract

A method of protecting wood through enhanced penetration of wood preservatives includes providing a solution including (a) at least one amine oxide, (b) at least one organic wood preservative and (c) a buffering agent. The solution preferably has a pH of about 7 to 10. The solution is applied to the surface of the wood after which, with or without intervening storage, the materials are activated to effect enhanced penetration of the organic wood preservative into the wood. One may effect application at a solution temperature of about 30 to 75° C. and preferably about 50 to 60° C. to effect activation at a higher temperature and high relative humidity. In a preferred practice, the wood may be heated before and/or after application of the solution. The solution is also disclosed as a product.

Claims (45)

1. A wood preservative solution comprising

at least one amine oxide,

at least one wood preservative and a buffering agent with the balance being at least one suitable solvent,

said solution having a pH of about 7 to 10, and

said buffering agent being present in a sufficiently small amount that it does not provide a substantial wood preservation effect, whereby the interaction of the amine oxide with the buffering agent will have a synergistic effect to effect a greater depth of penetration of said wood preservative.

2. The solution of claim 1 including

employing water as said solvent.

3. The solution of claim 1 including

said amine oxide being selected from the group of alkyl dimethyl amine oxides, decyl dimethyl amine oxide, lauryl dimethyl amine oxide, isoalkyl dimethyl amine oxide, myristyl dimethyl amine oxide, cetyl dimethyl amine oxide, stearyl dimethyl amine oxide, octyl dimethyl amine oxide and N-alkyl(C12-C16)-N,N-dimethylamine oxide (ADO) and combinations thereof.

4. The solution of claim 1 including

employing said buffering agent in an amount of about 3 to 80 weight percent based on total solution weight.

5. The solution of claim 4 including

employing said amine oxide in an amount of about 0.11 to 70 weight percent based on total solution weight.

6. The solution of claim 5 including

employing said wood preservative in an amount of about 3 ppm to 50 percent based on total solution weight.

7. The solution of claim 5 including

employing said amine oxide in a weight percent of about 1 to 20 percent of said solution.

8. The solution of claim 1 including

employing said buffering agent in a weight percent of about 5 to 30 percent of said solution weight.

9. The solution of claim 1 including

employing as said solution a solution having a pH of about 7 to 8.5.

10. The solution of claim 1 including

employing at least one solvent additive in said solution.

11. The solution of claim 10 including

said solvent additive selected from the group consisting of glycols, alcohols and combinations thereof.

12. The solution of claim 10 including

a water repellent being present as a said additive.

13. The solution of claim 12 including

said water repellent including a wax-polymer emulsion.

14. The solution of claim 1 including

said wood preservative being present in amount of about 20 ppm to 5000 ppm.

15. The solution of claim 14 including

said wood preservative including at least one fungicide.

16. The solution of claim 15 including

said fungicide selected from the group consisting of 3-iodo-2-propynyl butyl carbamate, diiodomethyl-p-tolylsulfone, triazoles, isothiazalones, phenols, quaternary ammonium compounds and combinations thereof.

17. The solution of claim 14 including

said wood preservatives including at least one insecticide.

18. The solution of claim 17 including

said insecticide including at least one material selected from the group consisting of nicotinimides, pyrethroids and combinations thereof.

19. The solution of claim 1 including

said wood being a wood selected from the group consisting of engineered wood and laminated wood having a glued layer or substantial amount of glue therein.

20. A wood preservative solution comprising

at least one amine oxide,

at least one wood preservative and a buffering agent with the balance being at least one suitable solvent, and

said buffering agent about 50 to 60 weight percent borax and about 40 to 50 weight percent boric acid.

Assignments (2)
SECURITY INTEREST Recorded Jun 7, 2010
From: KOP-COAT, INC.; RPM WOOD FINISHES GROUP, INC.; CHEMICAL SPECIALTIES MANUFACTURING CORPORATION; DAY-GLO COLOR CORP; DRYVIT SYSTEMS, INC.
To: WACHOVIA CAPITAL FINANCE CORPORATION (NEW ENGLAND)
Reel/Frame 024492/0441 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 12, 2008
From: WARD, HANS A.; SCOTT, CAMERON
To: KOP-COAT, INC.
Reel/Frame 021820/0491 →
Continuity (2)
Division 11135770 · May 24, 2005
Related Publication 20090088481A1 · Apr 2, 2009