IP Library › Granted Patent US 7,879,421
Granted Patent B2
US 7,879,421 · App. 12/340,139 · Granted Feb 1, 2011

Friction stir welding of fiber reinforced thermoplastics

Assignee: General Electric Company
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,879,421
App. No.
12/340,139
Granted
Feb 1, 2011
Kind
B2
Abstract

A fiber-reinforced component is formed of a first composite member including a thermoplastic matrix with reinforcing fibers having a diameter and a length distributed therein in a selected orientation and a second composite member including a thermoplastic matrix with reinforcing fibers having a diameter and a length distributed therein in a selected orientation. The first composite member is bonded to the second composite member by a solid state bond along a predetermined joint path, such that an average volume fraction of the reinforcing fibers of the first composite member and the second composite member within the joint path is substantially the same as an average volume fraction of the reinforcing fibers of the first composite member and the second composite member within the remainder of the fiber-reinforced component.

Claims (8)

1. A fiber-reinforced component, comprising;

a first composite member comprising a thermoplastic matrix with reinforcing fibers disposed therein in a random three-dimensional orientation thereby imparting isotropic structural properties to the first composite member, each of the reinforcing fibers having a diameter of about 1 micrometer (40 microinches) to about 25 micrometers (980 microinches) and a length of about 1 mm (0.004 in.) to about 38 cm (14.7 in.);

a second composite member comprising a thermoplastic matrix with reinforcing fibers disposed therein in a random three-dimensional orientation thereby imparting isotropic structural properties to the second composite member, each of the reinforcing fibers having a diameter of about 1 micrometer (40 microinches) to about 25 micrometers (980 microinches) and a length of about 1 mm (0.004 in.) to about 38 cm (14.7 in.);

wherein the first composite member is bonded to the second composite member by a solid state bond along a predetermined joint path, such that an average volume fraction of the reinforcing fibers of the first composite member and the second composite member within the joint path is substantially the same as an average volume fraction of the reinforcing fibers of the first composite member and the second composite member within the remainder of the fiber-reinforced component; and

wherein a plurality of the reinforcing fibers of the first composite member and the second composite member are distributed within and across the joint path.

2. The fiber-reinforced component of claim 1 wherein the reinforcing fibers of the first composite member and the second composite member are uniformly distributed throughout the volume of each of the first composite member and the second composite member.

3. The fiber-reinforced component of claim 1 wherein the reinforcing fibers of the first composite member and the second composite member are disposed in a random orientation.

4. The fiber-reinforced component of claim 3 wherein the reinforcing fibers of the first composite member and the second composite member are disposed in a random orientation within the predetermined joint path.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 19, 2008
From: MANICKE, PAUL STEPHEN; HELDER, EARL CLAUDE
To: GENERAL ELECTRIC COMPANY
Reel/Frame 022009/0915 →
Continuity (2)
Division 11618307 · Dec 29, 2006
Related Publication 20090098369A1 · Apr 16, 2009