Environmentally safe electrochromic devices and assemblies

Inventors: Anoop Agrawal (Tucson, AZ); John P. Cronin (Tucson, AZ); Juan Carlos L. Tonazzi (Tucson, AZ)
Assignee: AJJER, LLC
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,599,467
App. No.
12/865,688
Granted
Dec 3, 2013
Kind
B2
Abstract

This invention recognizes the hazards of materials used to make electrochromic devices and the resulting mirror assemblies for automotive use. The invention provides novel ways to reduce these hazards and to manufacture these mirrors using renewable resources and smaller environmental footprint.

Claims (9)

1. An electrochromic mirror or a window comprising a rear element and a transparent front element being sealably bonded together along the perimeter with a sealant in a spaced apart relationship to define a chamber; wherein the said sealant system further comprises of a gap for the electrolyte to be introduced into the said chamber and a dam close to the said gap.

2. An electrochromic mirror or a window as in claim 1 where the said sealant and the dam are made out of the same material.

3. An electrochromic mirror or a window comprising a rear element and a transparent front element being sealably bonded together along the perimeter with a perimeter sealant in a spaced apart relationship to define a chamber; wherein the said perimeter sealant system further comprises of a main perimeter seal and a dam, wherein the dam is associated with the gap in the main seal, and the said gap is associated with the electrolyte to be introduced into the said chamber, wherein the said dam resists the penetration of the plug sealant into the chamber during the operation of plugging of the said gap.

4. An electrochromic mirror as in claim 3 , wherein in the perimeter sealant system and the dam and the perimeter sealant are made out of the same material or different materials.

5. An electrochromic mirror as in claim 4 , wherein the dam may or may not contact with the main sealant.

6. An electrochromic mirror or a window comprising a rear element and a transparent front element being sealably bonded together along the perimeter with a perimeter sealant in a spaced apart relationship to define a chamber; wherein the said perimeter sealant system further comprises of a main perimeter seal, a gap in the said seal and a dam near the said gap, and both the dam and the main sealant are formed so that they are cured or solidified after the assembly of the two substrates.

7. An electrochromic mirror or a window as in claim 6 , wherein both the dam and the main perimeter seal are formed in one operation.

8. An electrochromic mirror or a window as in claim 6 , wherein both the dam and the main perimeter seal are of the same height.

9. An electrochromic mirror or a window as in claim 6 , wherein the width of the main seal is different from the width of the dam.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 2, 2013
From: ELECTROCHOMIX, INC.
To: AJJER, LLC
Reel/Frame 030336/0314 →
Continuity (4)
Provisional Application 61063160 · Jan 31, 2008
Provisional Application 61068042 · Mar 4, 2008
Provisional Application 61056311 · May 27, 2008
Related Publication 20110051219A1 · Mar 3, 2011