IP Library Granted Patent US 8,853,651
Granted Patent B2
US 8,853,651 · App. 12/943,708 · Granted Oct 7, 2014

Doped luminescent materials and particle discrimination using same

Inventors: F. Patrick Doty (Livermore, CA); Mark D. Allendorf (Pleasanton, CA); Patrick L. Feng (Livermore, CA)
Assignee: Sandia Corporation
C09K11/06G21K4/00C09K2211/1029C09K2211/185C09K2211/1092C09K2211/1074
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,853,651
App. No.
12/943,708
Granted
Oct 7, 2014
Kind
B2
Abstract

Doped luminescent materials are provided for converting excited triplet states to radiative hybrid states. The doped materials may be used to conduct pulse shape discrimination (PSD) using luminescence generated by harvested excited triplet states. The doped materials may also be used to detect particles using spectral shape discrimination (SSD).

Claims (46)

1. A method of making a material for particle detection, the method comprising:

providing a host material, wherein the host material is configured to generate excited singlet and triplet states responsive to excitation; and

doping the host material with a quantity of heavy atoms wherein the quantity of heavy atoms are configured to generate luminescence from at least a portion of the excited triplet states, and wherein the quantity is sufficient to generate detectable luminescence from the excited triplet states, and wherein the quantity is insufficient to quench substantially all luminescence from the excited singlet states

wherein the host material is configured to generate luminescence from the excited singlet states at a first wavelength, and wherein the heavy atoms are configured to generate luminescence from the excited triplet states at a second wavelength, different from the first wavelength.

2. The method of claim 1 , wherein the doping comprises mixing the quantity of heavy atoms with the host material to disperse the heavy atoms into the host material.

3. The method of claim 1 , wherein the host material comprises a metal organic framework material and wherein the doping comprises synthesizing the metal organic framework material in the presence of the heavy atoms.

4. The method of claim 1 , wherein the host material comprises a metal organic framework material and wherein the doping comprises infiltrating the metal organic framework with a solvent containing at least a portion of the quantity of heavy atoms.

5. The method of claim 1 , wherein the heavy atoms are selected from a group consisting of iridium atoms, platinum atoms, osmium atoms, and combinations thereof.

6. A material for particle detection, the material comprising:

a host material;

a first luminophore dispersed in the host material, wherein the first luminophore is configured to generate luminescence at a first wavelength responsive to excited singlet states; and

a second luminophore dispersed in the host material, wherein the second luminophore is configured to generate luminescence at a second wavelength, different from the first wavelength, responsive to excited triplet states;

wherein a quantity of the second luminophore is insufficient to quench substantially all luminescence at the first wavelength.

7. The material of claim 6 , wherein the second luminophore comprises a heavy atom.

8. The material of claim 6 , wherein first luminophore is intrinsic to the host material and the second luminophore comprises an extrinsic dopant.

9. The material of claim 6 , wherein the first luminophore comprises an extrinsic dopant and the second luminophore is intrinsic to the host material.

10. The material of claim 6 , wherein the first and second luminophores comprise extrinsic dopants.

11. The material of claim 6 , wherein the host material is selected from a group consisting of crystalline materials, liquid materials, and plastic materials.

12. The method of claim 6 , wherein the host material comprises PVK.

13. The method of claim 6 , wherein the second luminophore is selected form a group consisting of iridium atoms, platinum atoms, osmium atoms, and combinations thereof.

14. A method for detecting a particle, the method comprising:

exciting a material with the particle, wherein the material is configured to generate excited singlet and triplet states responsive to excitation by the particle, and wherein the material includes a luminophore configured to harvest luminescence from excited triplet states;

measuring a temporal luminescence response generated by the material including a magnitude of luminescence at a plurality of times; and

detecting the particle, based at least in part, on the temporal response.

15. The method of claim 14 wherein the particle comprises an energetic electron, proton or ion.

16. The method of claim 14 wherein the luminophore comprises a metal organic ligand.

17. The method of claim 14 wherein the temporal luminescence response comprises a first intensity of luminescence generated at a first time based primarily on excited singlet states and a second intensity of luminescence generated at a second time based primarily on excited triplet states facilitated by the luminophore.

18. The method of claim 14 wherein the temporal luminescence response comprises integrating luminescence generated by the material over time.

19. A method for detecting a particle, the method comprising:

exciting a material with the particle, wherein the material is configured to generate states responsive to excitation by the particle, and wherein the material includes a luminophore configured to facilitate luminescence from excited triplet states responsive to exposure to the excited triplet states in the material;

measuring a wavelength spectral signature of luminescence generated by the material including a magnitude of luminescence at a plurality of wavelengths; and

detecting the particle, based at least in part, on the wavelength spectral signature.

20. The method of claim 19 , wherein the material is configured to generate luminescence from the excited singlet states at a first wavelength, and wherein the luminophore is further configured to generate luminescence from the excited triplet states at a second wavelength, different from the first wavelength; and wherein the spectral signature includes luminescence at the first and second wavelengths.

21. The method of claim 19 , wherein the particle comprises an electron or a proton.

22. The method of claim 19 , wherein the luminophore comprises a metal-organic complex.

23. The method of claim 19 , wherein the spectral response comprises an integral of luminescence generated by the material over a plurality of wavelengths.

24. A system comprising:

a material, wherein the material is configured to generate excited singlet and triplet states responsive to excitation by a particle, and wherein the material includes a luminophore configured to luminescence responsive to exposure to excited triplet states in the material, and wherein the material is further configured to generate luminescence from the excited singlet states at a first wavelength, and wherein the luminophore is further configured to generate luminescence from the excited triplet states at a second wavelength, different from the first wavelength;

a first luminescence detector configured to receive at least a portion of luminescence generated by the material and further configured to generate a first signal corresponding to a magnitude of luminescence at the first wavelength; and

a second luminescence detector configured to receive at least a portion of luminescence generated by the material and further configured to generate a second signal corresponding to a magnitude of luminescence at the second wavelength.

25. The system of claim 24 , further comprising:

a first filter disposed between the material and the first luminescence detector and configured to provide luminescence at the first wavelength to the first luminescence detector and block luminescence at the second wavelength; and

a second filter disposed between the material and the second luminescence detector and configured to provide luminescence at the second wavelength to the second luminescence detector and block luminescence at the first wavelength.

26. The system of claim 24 , further comprising a processing device coupled to the first and second luminescence detectors and configured to receive the first and second signals, wherein the processing device is further configured to detect a particle based, at least in part, on the first and second signals.

27. The system of claim 24 , wherein the particle comprises an energetic electron, proton or ion.

28. The system of claim 24 , wherein the luminophore comprises a metal-organic complex.

Assignments (3)
CHANGE OF NAME Recorded May 22, 2018
From: SANDIA CORPORATION
To: NATIONAL TECHNOLOGY & ENGINEERING SOLUTIONS OF SANDIA, LLC
Reel/Frame 046207/0342 →
CONFIRMATORY LICENSE Recorded Feb 3, 2011
From: SANDIA CORPORATION
To: U.S. DEPARTMENT OF ENERGY
Reel/Frame 025738/0344 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 20, 2010
From: ALLENDORF, MARK D.; DOTY, F. PATRICK; FENG, PATRICK L.
To: SANDIA CORPORATION
Reel/Frame 025530/0697 →
Continuity (5)
Provisional Application 61260665 · Nov 12, 2009
Provisional Application 61347501 · May 24, 2010
Provisional Application 61392321 · Oct 12, 2010
Provisional Application 61392732 · Oct 13, 2010
Related Publication 20110108738A1 · May 12, 2011