IP Library Patent Application 13058964
Patent Application
App. No. 13/058,964

RUBBER ARTICLES SUBJECTED TO REPEATED DEFORMATION AND COMPOSITIONS FOR MAKING THE SAME

Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US None
App. No.
13/058,964
Abstract

An air spring having an airsleeve, wherein at least one layer of said airsleeve includes the vulcanization product of an elastomer and syndiotactic 1,2-polybutadiene.

Claims (24)

1 . An air spring having an airsleeve, wherein at least one layer of said airsleeve includes the vulcanization product of

an elastomer; and

syndiotactic 1,2-polybutadiene.

2 . The air spring of claim 1 , wherein said elastomer includes polychloroprene or polychloroprene copolymers.

3 . The air spring of claim 2 , wherein said polychloroprene copolymer is a copolymer of chloroprene and 2,3-dichloro-1,3-butadiene.

4 . The air spring of claim 3 , wherein said copolymer has a Mooney Viscosity (M 1+4 at 100° C.) of 100-120.

5 . The air spring of claim 4 , further comprising a second copolymer of chloroprene and 2,3-dichloro-1,3-butadiene having a Mooney Viscosity (M 1+4 at 100° C.) of 41-51.

6 . The air spring of claim 1 , where said syndiotactic 1,2-polybutadiene has a melt temperature of at least 60° C., and less than 130° C.

7 . The air spring of claim 1 , where said syndiotactic 1,2-polybutadiene has a melt temperature of at least 90° C., and less than 110° C.

8 . The air spring of claim 1 , where said syndiotactic polybutadiene is characterized by a 1,2-linkage content of at least 70%, and less than 90%.

9 . The air spring of claim 1 , where said syndiotactic polybutadiene is characterized by syndiotacticity of at least 60%, and less than 90%.

10 . A method for the production of an air spring airsleeve comprising:

mixing an elastomer, syndiotactic 1,2-polybutadiene, and a curative in a masterbatch to form a rubber composition;

forming the rubber composition into the shape of an airsleeve; and

curing the rubber composition.

11 . An air spring having an airsleeve, wherein at least one layer of said airsleeve has a rubber component comprised of:

an elastomer; and

syndiotactic 1,2-polybutadiene.

12 . The air spring of claim 11 , wherein said elastomer contains at least one polymer of chloroprene.

13 . The air spring of claim 12 , wherein said at least one polymer includes at least one copolymer of chloroprene and 2,3-dichloro-1,3-butadiene.

14 . The air spring of claim 13 , wherein said at least one copolymer includes a first copolymer of chloroprene and 2,3-dichloro-1,3-butadiene having a Mooney Viscosity (ML 1+4 at 100° C.) of 100-120.

15 . The air spring of claim 14 , wherein said at least one copolymer includes a second copolymer of chloroprene and 2,3-dichloro-1,3-butadiene having a Mooney Viscosity (ML 1+4 at 100° C.) of 41-51.

16 . The air spring of claim 11 , where said syndiotactic polybutadiene is characterized by a 1,2-linkage content of at least 70%, and less than 90%.

17 . The air spring of claim 11 , where said syndiotactic polybutadiene is characterized by syndiotacticity of at least 60%, and less than 90%.

Assignments (4)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 22, 2016
From: BRIDGESTONE CORPORATION
To: FIRESTONE INDUSTRIAL PRODUCTS COMPANY, LLC
Reel/Frame 038061/0605 →
RE-RECORD TO CORRECT INVENTOR'S LAST NAME PREVIOUSLY RECORDED AT REEL 026193 FRAME 0283. Recorded Jul 26, 2011
From: AGARWAL, SHEEL; LUO, STEVEN; RENSEL, JOHN
To: BRIDGESTONE CORPORATION
Reel/Frame 026655/0029 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 21, 2011
From: BRIDGESTONE CORPORATION
To: FIRESTONE INDUSTRIAL PRODUCTS COMPANY, LLC
Reel/Frame 026472/0145 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 28, 2011
From: AGARWAL, SHEEL; LUO, STEVEN; RENSEL, JOHN
To: BRIDGESTONE CORPORATION
Reel/Frame 026193/0283 →