Vitreous silica crucible
The present invention provides a vitreous silica crucible which can restrain deterioration of crystallinity of a silicon ingot in multi-pulling. Provided is a vitreous silica crucible for pulling a silicon single crystal, the crucible has a wall having, from an inner surface toward an outer surface of the crucible, a synthetic vitreous silica layer, a natural vitreous silica layer, an impurity-containing vitreous silica layer and a natural vitreous silica layer.
1. A vitreous silica crucible for pulling a silicon single crystal, the crucible has a wall having, from an inner surface toward an outer surface of the crucible, a synthetic vitreous silica layer, a natural vitreous silica layer, an impurity-containing vitreous silica layer and a natural vitreous silica layer, wherein the natural vitreous silica layers are no-impurity-added layers, and the thickness of the impurity-containing vitreous silica layer at a bottom portion of the crucible is not zero but smaller than that of the impurity-containing vitreous silica layer at a sidewall portion of the crucible.
2. The crucible of claim 1 , wherein the thickness of the impurity-containing vitreous silica layer at a sidewall portion and a corner portion is 30% to 70% of the thickness of the wall.
3. The crucible of claim 1 , wherein the impurity-containing vitreous silica layer contains impurities in an amount of 20 to 500 ppm.