IP Library Patent Application 13424017
Patent Application
App. No. 13/424,017

SOLID-STATE MULTI-LAYER ELECTROLYTE, ELECTROCHEMICAL CELL AND BATTERY INCLUDING THE ELECTROLYTE, AND METHOD OF FORMING SAME

Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US None
App. No.
13/424,017
Abstract

An electrochemical cell including a multi-layer solid-state electrolyte, a battery including the cell, and a method of forming the battery and cell are disclosed. The electrolyte includes a first layer that is compatible with the anode of the cell and a second layer that is compatible with the cathode of the cell. The cell exhibits improved performance compared to cells including a single-layer electrolyte.

Claims (37)

1 . A solid-state electrochemical cell based on lithium ion transport, the cell comprising:

an anode;

a composite cathode comprising electroactive cathode material; and

a solid-state electrolyte interposed between the anode and cathode, wherein the solid-state electrolyte comprises:

a first electrolyte layer that is stable with regard to the anode; and

a second electrolyte layer that is stable with regard to the cathode.

2 . The solid-state electrochemical cell of claim 1 , wherein the anode material comprises a material selected from the group consisting of lithium metal, indium metal, nano-silicon composite material, silicon alloys, carbon, and combination of these materials.

3 . The solid-state electrochemical cell of claim 1 , wherein the cathode comprises an oxide material, an electrically-conducting carbon material, and second electrolyte layer material.

4 . The solid-state electrochemical cell of claim 1 , wherein the electroactive cathode material is selected from the group consisting of LiCoO 2 , Li 1 N 0.85 Co 0.1 Al 0.05 O 2 , LiNi 1/3 Co 1/3 Mn 1/3 O 2 , LiFePO 4 , LiMn 2 O 4 , and a combination of these materials.

5 . The solid-state electrochemical cell of claim 1 , wherein the cathode active material has an average particle size ranging from about 0.01 μm to about 20 μm.

6 . The solid-state electrochemical cell of claim 1 , wherein the cathode comprises cathode active material particles coated with between about 0.2 and about 5 nm of material.

7 . The solid-state electrochemical cell of claim 6 , wherein the particles are coated with the material using atomic layer deposition techniques.

8 . The solid-state electrochemical cell of claim 6 , wherein material comprises aluminum oxide, zirconium oxide, titanium oxide, or any combination thereof.

9 . The solid-state electrochemical cell of claim 6 , wherein the coated cathode is heat treated at a temperature between 250° C. and 600° C.

10 . The solid-state electrochemical cell of claim 6 , wherein the cathode is heat treated in a reducing atmosphere comprising one or more of argon, nitrogen, and hydrogen.

11 . The solid-state electrochemical cell of claim 6 , wherein the cathode is heat treated for about 1 hr to about 24 hrs.

12 . The solid-state electrochemical cell of claim 1 , wherein the first electrolyte layer is adjacent the anode and comprises xLi 2 S(1−x)P 2 S 5 , where x is a molar ratio and ranges from about 60 to about 80.

13 . The solid-state electrochemical cell of claim 1 , wherein the first electrolyte layer comprises particles with size of about 0.5 to about 20 μm.

14 . The solid-state electrochemical cell of claim 1 , wherein the second electrolyte layer comprises particles with size of about 0.5 to about 20 μm.

15 . The solid-state electrochemical cell of claim 1 , wherein the second electrolyte layer is adjacent the cathode and comprises Li x Ge y P z S 4 , where x, y, z are mole concentrations and range from 2.3<x<4, 0<y<1, and 0<z<1.

16 . The solid-state electrochemical cell of claim 1 , wherein the second electrolyte layer is heat treated at a temperature between 300° C. and 550° C.

17 . The solid-state electrochemical cell of claim 1 , wherein the second electrolyte layer is heat treated in a reducing atmosphere comprising one or more of argon, nitrogen, and hydrogen.

18 . The solid-state electrochemical cell of claim 1 , wherein the second electrolyte layer is heat treated for about 1 hr to about 24 hrs.

19 . A method of forming an electrochemical cell, the method comprising the steps of:

providing an anode;

providing a cathode comprising electroactive cathode material; and

providing a solid-state electrolyte, wherein the step of providing a solid-state electrolyte comprises the steps of

preparing a first electrolyte layer composition;

preparing a second electrolyte layer composition; and

forming a multi-layer electrolyte using the first electrolyte layer and the second electrolyte layer.

20 . A battery comprising;

a housing;

a first terminal;

an anode coupled to the first terminal;

a solid-state electrolyte comprising a first electrolyte layer stable with regard to the anode and a second electrolyte layer stable with regard to the cathode;

a cathode; and

a second terminal coupled to the cathode.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 5, 2012
From: TREVEY, JAMES; LEE, SE-HEE; WOO, JAE-HA
To: THE REGENTS OF THE UNIVERSITY OF COLORADO, A BODY CORPORATE
Reel/Frame 028322/0227 →