Processes for extracting aluminum from aluminous ores

Assignee: Orsite Aluminae Inc.
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,337,789
App. No.
13/471,901
Granted
Dec 25, 2012
Kind
B2
Abstract

There are provided processes for extracting aluminum ions from aluminous ores and for preparing alumina. Such processes can be used with various types of aluminous ores such as aluminous ores comprising various types of metals such as Fe, K, Mg, Na, Ca, Mn, Ba, Zn, Li, Sr, V, Ni, Cr, Pb, Cu, Co, Sb, As, B, Sn, Be, Mo, or mixtures thereof.

Claims (35)

1. A process for preparing alumina comprising:

leaching an aluminous ore with an acid to obtain a leachate and a solid residue, and separating said leachate from said solid residue;

removing at least a portion of iron ions contained in said leachate by reacting said leachate with a base to obtain a pH of at least 10 and substantially selectively precipitating said at least a portion of iron ions and separating said precipitated at least a portion of iron ions from said leachate to obtain an Al-rich composition;

purifying said Al-rich composition; and

converting said purified Al-rich composition into alumina.

2. The process of claim 1 , wherein said acid is HCl.

3. The process of claim 2 , wherein said aluminous ore is leached with HCl at a temperature of at least 100° C.

4. The process of claim 3 , wherein aluminum ions in the form of Al(OH) 3 are converted into alumina.

5. The process of claim 1 , wherein purifying said Al-rich composition is carried out by precipitating aluminum ions and/or by means of a hollow fiber membrane.

6. The process of claim 5 , wherein said pH is at least 11.

7. The process of claim 5 , wherein said pH is at least 12.

8. The process of claim 5 , wherein said pH is about 11.5 to about 12.5.

9. The process of claim 5 , wherein said pH is between 10.5 and 11.0.

10. The process of claim 5 , wherein said pH is between 10 and 11.

11. A process for preparing alumina comprising:

leaching an aluminous ore with an acid to obtain a leachate and a solid residue, and separating said leachate from said solid residue;

at least partially removing iron ions from said leachate by substantially selectively precipitating said iron ions at a pH greater than 10 by reacting said leachate with a base and at least partially removing said precipitated iron ions from said leachate, thereby obtaining an Al-rich composition comprising Al 3+ ions;

purifying said Al 3+ ions; and

converting said Al 3+ ions into alumina.

12. The process of claim 11 , wherein said acid is HCl.

13. The process of claim 12 , wherein said aluminous ore is leached with HCl at a temperature of at least 100° C.

14. The process of claim 13 , wherein aluminum ions in the form of Al(OH) 3 are converted into alumina.

15. The process of claim 11 , wherein purifying said Al 3+ ions comprises reacting said Al 3+ ions with HCl.

16. The process of claim 11 , wherein purifying said Al 3+ ions is carried out by selectively precipitating said Al 3+ ions and/or by using a hollow fiber membrane.

17. The process of claim 11 , wherein purifying said Al 3+ ions is carried out by selectively precipitating said Al 3+ ions.

18. A process for extracting aluminum ions from an aluminous ore, said process comprising:

leaching said aluminous ore with an acid to obtain a composition comprising aluminum ions and iron ions;

at least partially removing said iron ions from said composition by substantially selectively precipitating said iron ions at a pH of at least 10 by reacting said composition with a base and at least partially removing said precipitated iron ions, thereby obtaining an Al-rich composition comprising Al 3+ ions; and

purifying said Al 3+ ions.

19. The process of claim 18 , wherein said pH is between 10 and 11.

20. A process for extracting aluminum ions from argillite, said process comprising:

leaching said argillite with HCl to obtain a composition comprising a leachate and a solid residue;

separating said leachate and said solid residue from one another;

at least partially removing iron from said leachate by substantially selectively precipitating iron ions by reacting said leachate with a base and removing a so-formed precipitate, to obtain an Al-rich composition comprising Al 3+ ions; and

purifying said Al 3+ ions by substantially selectively precipitating said Al 3+ ions.

Assignments (11)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 18, 2024
From: AEM CANADA GROUP INC.
To: AEM TECHNOLOGIES INC.
Reel/Frame 067144/0314 →
CHANGE OF ADDRESS FOR ASSIGNEE Recorded Apr 18, 2024
From: AEM CANADA GROUP INC.
To: AEM CANADA GROUP INC.
Reel/Frame 067144/0371 →
RELEASE OF SECURITY INTEREST Recorded Apr 18, 2024
From: MIDCAP FINANCIAL TRUST
To: AEM CANADA GROUP INC.
Reel/Frame 067342/0789 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 17, 2024
From: ORBITE TECHNOLOGIES INC.
To: AEM CANADA GROUP INC.
Reel/Frame 067133/0176 →
SECURITY INTEREST Recorded Nov 5, 2015
From: ORBITE TECHNOLOGIES INC.
To: MIDCAP FINANCIAL TRUST
Reel/Frame 036969/0193 →
SECURITY INTEREST Recorded Nov 5, 2015
From: ORBITE TECHNOLOGIES INC.
To: MIDCAP FINANCIAL TRUST
Reel/Frame 036969/0065 →
CHANGE OF NAME Recorded Aug 20, 2015
From: ORBITE ALUMINAE INC.
To: ORBITE TECHNOLOGIES INC.
Reel/Frame 036407/0736 →
CORRECTIVE ASSIGNMENT TO CORRECT THE <ASSIGNEE COUNTRY> PREVIOUSLY RECORDED ON REEL 028303 FRAME 0839. ASSIGNOR(S) HEREBY CONFIRMS THE CORRECTION OF <ASSIGNEE COUNTRY> FROM <QUEBEC> TO <CANADA>. Recorded Oct 30, 2012
From: BOUDREAULT, RICHARD; ALEX, SERGE; BIASOTTO, FABIENNE
To: EXPLORATION ORBITE VSPA INC.
Reel/Frame 029209/0424 →
CORRECTIVE ASSIGNMENT TO CORRECT THE <DOC DATE> AND <ASSIGNEE COUNTRY>. PREVIOUSLY RECORDED ON REEL 028315 FRAME 0450. ASSIGNOR(S) HEREBY CONFIRMS THE CORRECTION OF <DOC DATE> FROM <11/19/2009> TO <10/11/2011> AND CORRECTION OF <ASSIGNEE COUNTRY> FROM <QUEBEC> TO <CANADA>.. Recorded Oct 29, 2012
From: EXPLORATION ORBITE VSPA INC.
To: ORBITE ALUMINAE INC.
Reel/Frame 029207/0856 →
NUNC PRO TUNC ASSIGNMENT Recorded Jun 1, 2012
From: BOUDREAULT, RICHARD; ALEX, SERGE; BIASOTTO, FABIENNE
To: EXPLORATION ORBITE VSPA INC.
Reel/Frame 028303/0839 →
CHANGE OF NAME Recorded Jun 1, 2012
From: EXPLORATION ORBITE VSPA INC.
To: ORBITE ALUMINAE INC.
Reel/Frame 028315/0450 →
Continuity (4)
Continuation 12900371 · Oct 7, 2010
Continuation 12601079
Provisional Application 60939254 · May 21, 2007
Related Publication 20120237418A1 · Sep 20, 2012