IP Library Granted Patent US 10,076,773
Granted Patent B2
US 10,076,773 · App. 13/817,218 · Granted Sep 18, 2018

Method for washing reactor

Inventors: Shinya Takahashi (Tokyo, JP); Kazuhiko Tasaka (Tokyo, JP); Yuichi Tanaka (Tokyo, JP); Marie Iwama (Tokyo, JP)
Assignees: JAPAN OIL, GAS AND METALS NATIONAL CORPORATION; INPEX CORPORATION; JX NIPPON OIL & ENERGY CORPORATION; JAPAN PETROLEUM EXPLORATION CO., LTD.; COSMO OIL CO., LTD.; NIPPON STEEL & SUMIKIN ENGINEERING CO., LTD.
B08B3/04B01J38/52B01J38/56B08B9/08C10G1/06C10G2/32C10G21/12C10G47/00C10G47/22C10G47/36C10G2300/1014C10G2300/1022C10G2300/4031C10G2300/44Y02P30/20
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,076,773
App. No.
13/817,218
Granted
Sep 18, 2018
Kind
B2
Abstract

The method for cleaning a reactor of the present invention comprises passing a solvent through a wax-fraction hydrocracking apparatus which is charged with a catalyst and to which supply of a wax fraction is stopped, wherein the solvent comprising at least one oil selected from a group consisting of hydrocarbon and vegetable oils, and having a sulfur content of less than 5 ppm and being in a liquid state at 15° C.

Claims (28)

1. A method for regenerating a catalyst, to which wax and oil are attached, comprising:

stopping the supply of a wax fraction through a fixed-bed flow reactor charged with a catalyst for hydrocracking a wax fraction;

passing a solvent comprising at least one oil selected from the group consisting of hydrocarbon and vegetable oils, wherein the oil has a sulfur content of less than 5 ppm and is in a liquid state at 15° C., through a fixed-bed flow reactor charged with the catalyst for hydrocracking the wax fraction, said wax fraction being dissolved in the solvent;

picking a check-up sample from the solvent discharged from the fixed-bed flow reactor;

visually checking, at a temperature at or below the temperature at which the wax deposits from the solvent with a desired level of wax concentration, for the presence or absence of wax deposition in the check-up sample;

continuing the passage of the solvent through the fixed-bed flow reactor if wax deposition is present in the check-up sample, but discontinuing the passage of the solvent through the fixed-bed flow reactor if wax deposition is absent in the check-up sample;

discharging the catalyst from the reactor when wax deposition is absent in the check-up sample and the flow passage of the solvent through the reactor is stopped; and

removing oil on the catalyst discharged from the fixed-bed flow reactor after the wax fraction present on and around the catalyst is removed by the solvent, by heating the catalyst under an inert gas atmosphere to evaporate the oil an obtain a deoiled catalyst.

2. The method according to claim 1 , wherein the solvent passed through the fixed-bed flow reactor is then fractionated in a rectifying tower positioned downstream of the fixed-bed flow reactor, and again passed through the fixed-bed flow reactor prior to said discontinuing of the passage of the solvent through the fixed-bed flow reactor.

3. The method according to claim 1 , wherein the solvent is a hydrocarbon produced by a GTL process.

4. The method according to claim 1 , wherein the solvent is a light oil fraction produced by a GTL process.

5. The method according to claim 1 , wherein the temperature at or below the temperature at which the wax deposits from the solvent with a desired level of wax concentration is between −20° C. to 40° C.

6. The method according to claim 1 , wherein the inert gas atmosphere comprises nitrogen gas.

7. The method according to claim 6 , wherein the deoiled catalyst is heated under an air atmosphere to obtain a regenerated catalyst.

8. A method for regenerating a catalyst, to which wax and oil are attached, comprising:

stopping the supply of a wax fraction through a fixed-bed flow reactor charged with a catalyst for hydrocracking a wax fraction;

passing a solvent comprising at least one oil selected from the group consisting of hydrocarbon and vegetable oils, wherein the oil has a sulfur content of less than 5 ppm and is in a liquid state at 15° C., through a fixed-bed flow reactor charged with the catalyst for hydrocracking the wax fraction, said wax fraction being dissolved in the solvent;

picking a check-up sample from the solvent discharged from the fixed-bed flow reactor;

checking, at a temperature at or below the temperature at which the wax deposits from the solvent with a desired level of wax concentration, for the presence or absence of wax deposition in the check-up sample;

continuing the passage of the solvent through the fixed-bed flow reactor if wax deposition is present in the check-up sample, but discontinuing the passage of the solvent through the fixed-bed flow reactor if wax deposition is absent in the check-up sample;

discharging the catalyst from the reactor when wax deposition is absent in the check-up sample and the flow passage of the solvent through the reactor is stopped; and

removing oil on the catalyst discharged from the fixed-bed flow reactor after the wax fraction present on and around the catalyst is removed by the solvent, by heating the catalyst under an inert gas atmosphere in order to evaporate the oil and obtain a deoiled catalyst,

wherein the temperature is set such that the concentration of the wax in the solvent is confirmed to be decreasing, between each pass-through of the solvent, to a desired level based on a previously obtained relationship between the concentration of the wax in the solvent and a temperature at which the wax starts depositing.

9. The method according to claim 8 , wherein the solvent passed through the fixed-bed flow reactor is then fractionated in a rectifying tower positioned downstream of the fixed-bed flow reactor, and again passed through the fixed-bed flow reactor prior to said discontinuing of the passage of the solvent through the fixed-bed flow reactor.

10. The method according to claim 8 , wherein the solvent is a hydrocarbon produced by a GTL process.

11. The method according to claim 8 , wherein the temperature at or below the temperature at which the wax deposits from the solvent with a desired level of wax concentration is between −20° C. to 40° C.

12. The method according to claim 8 , wherein the inert gas atmosphere comprises nitrogen gas.

13. The method according to claim 12 , wherein the deoiled catalyst is heated under an air atmosphere to obtain a regenerated catalyst.

Assignments (3)
CHANGE OF NAME Recorded Jul 1, 2019
From: NIPPON STEEL & SUMIKIN ENGINEERING CO., LTD.
To: NIPPON STEEL ENGINEERING CO., LTD.
Reel/Frame 049646/0648 →
CORRECTIVE ASSIGNMENT TO CORRECT THE PORTION OF THE FIRST ASSIGNEE'S NAME PREVIOUSLY RECORDED ON REEL 029831 FRAME 0958. ASSIGNOR(S) HEREBY CONFIRMS THE THE FIRST ASSIGNEE'S NAME SHOULD READ JAPAN OIL, GAS AND METALS NATIONAL CORPORATION. Recorded May 15, 2013
From: TAKAHASHI, SHINYA; TASAKA, KAZUHIKO; TANAKA, YUICHI; IWAMA, MARIE
To: JAPAN OIL, GAS AND METALS NATIONAL CORPORATION; INPEX CORPORATION; JX NIPPON OIL & ENERGY CORPORATION; JAPAN PETROLEUM EXPLORATION CO., LTD.; COSMO OIL CO., LTD.; NIPPON STEEL & SUMIKIN ENGINEERING CO., LTD.
Reel/Frame 030418/0623 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 19, 2013
From: TAKAHASHI, SHINYA; TASAKA, KAZUHIKO; TANAKA, YUICHI; IWAMA, MARIE
To: JAPAN OIL, GAS, AND METAL NATIONAL CORPORATION; INPEX CORPORATION; JX NIPPON OIL & ENERGY CORPORATION; JAPAN PETROLEUM EXPLORATION CO., LTD.; COSMO OIL CO., LTD.; NIPPON STEEL & SUMIKIN ENGINEERING CO., LTD.
Reel/Frame 029831/0958 →
Priority Claims (1)
JP 2010-184183 · Aug 19, 2010 · national
Continuity (1)
Related Publication 20130146088A1 · Jun 13, 2013