METHOD FOR REPAIRING HOLLOW FIBER MEMBRANE
A method for repairing a hollow fiber membrane in a module in which ends of a plurality of hollow fiber membranes are secured to a side of the module. A method for repairing a hollow fiber membrane in a module includes bringing a filler material that is in a solid phase into contact with a damaged portion of the hollow fiber membrane, and heating a filler contact site to join the filler material to the hollow fiber membrane, and the filler material is in solid phase.
1 . A method for repairing a hollow fiber membrane in a module in which ends of a plurality of hollow fiber membranes are secured to a side of the module, the method comprising:
bringing a filler material into contact with a damaged portion of the hollow fiber membrane; and
heating a filler contact site to join the filler material to the hollow fiber membrane, wherein the filler material is in a solid phase.
2 . The method according to claim 1 , wherein the filler material comprises at least one of a powder, a bead, a pellet, a spherical particle, a gel, or a paste.
3 . The method according to claim 2 , wherein the filler material comprises at least one of natural rubber, natural silicone, gelatin, agar, chicle, starch glue, or solid wax.
4 . The method according to claim 1 , wherein the filler material is brought into direct contact with the damaged portion of the hollow fiber membrane.
5 . The method according to claim 1 , wherein the filler contact site is heated to a temperature of about 80° C. to about 140° C.
6 . The method according to claim 1 , wherein the module is a pressurized hollow fiber membrane module.
7 . The method according to claim 1 , wherein the hollow fiber membrane is a filament-reinforced hollow fiber membrane.
8 . A method for repairing a hollow fiber membrane in a module in which ends of a plurality of hollow fiber membranes are secured to a side of the module, the method comprising:
cutting a damaged portion of the hollow fiber membrane;
inserting a filler material into a cut face of the hollow fiber membrane to contact the hollow fiber membrane; and
heating a filler contact site to join the filler material to the hollow fiber membrane, wherein the filler material is in a solid phase.
9 . The method according to claim 8 , wherein the filler material comprises at least one of a powder, a bead, a pellet, a spherical particle, a gel, or a paste.
10 . The method according to claim 9 , wherein the filler material comprises at least one of natural rubber, natural silicone, gelatin, agar, chicle, starch glue, or solid wax.
11 . The method according to claim 8 , wherein the filler contact site is heated to a temperature of about 80° C. to about 140° C.
12 . The method according to claim 8 , wherein the module is a pressurized hollow fiber membrane module.