Electromagnetic assisted ceramic materials for heavy oil recovery and in-situ steam generation

Inventor: Sameeh Issa Batarseh (Dhahran, SA)
Assignee: Saudi Arabian Oil Company
E21B43/24E21B43/2401E21B43/2406H01Q1/04H05B6/108H05B6/36
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,353,612
App. No.
14/147,914
Granted
May 31, 2016
Kind
B2
Abstract

The disclosure provides a downhole tool, and method of using the downhole tool, for enhancing recovery of heavy oil from a formation. A method for enhancing recovery of heavy oil from a formation includes placing a downhole tool in a first wellbore. The downhole tool has an outer core having at least one ceramic portion and at least one electromagnetic antenna located within the outer core. Electromagnetic radiation is emitted from the at least one electromagnetic antenna to heat the at least one ceramic portion.

Claims (45)

1. A method for enhancing recovery of heavy oil from a formation, comprising the steps of:

suspending a downhole tool with a connector above a first wellbore;

removeably lowering the downhole tool in the first wellbore, the downhole tool comprising an outer core having at least one ceramic portion, the at least one ceramic portion comprising at least one mesh ceramic portion and at least one solid ceramic portion,

the downhole tool further comprising an inner core,

and at least one electromagnetic antenna disposed between the inner core and the outer core;

injecting fluid into the inner core of the downhole tool through the wellbore;

allowing the fluid to flow from the inner core through the at least one mesh ceramic portion of the downhole tool; and

emitting electromagnetic radiation from the at least one electromagnetic antenna to heat the at least one ceramic portion.

2. The method of claim 1 , further comprising converting the fluid from liquid to steam as it flows through the at least one mesh ceramic portion.

3. The method of claim 1 , wherein the fluid is water.

4. The method of claim 1 , wherein the step of heating the at least one ceramic portion comprises heating the at least one ceramic portion to at least about 1000° C.

5. The method of claim 1 , wherein the step of emitting electromagnetic radiation comprises emitting electromagnetic radiation with frequency ranges from 300 MHz to 300 GHz.

6. The method of claim 1 , the method further comprising:

converting the fluid from liquid to steam as it flows through the at least one mesh ceramic portion;

placing production tubing in a second wellbore below the first wellbore;

reducing the viscosity of heavy oil located in the formation with the steam to produce a reduced viscosity heavy oil;

draining the reduced viscosity heavy oil to a region containing the second wellbore; and

flowing the reduced viscosity heavy oil into the production tubing to be produced from the formation.

7. The method of claim 1 , wherein the at least one ceramic portion comprises silica, alumina, magnesium oxide, potassium, iron III oxide, calcium oxide, sodium oxide, and titanium oxide.

8. The method of claim 1 , the method further comprising:

injecting a proppant comprising ceramic particles into the inner core; and

heating the ceramic particles in the proppant with the electromagnetic radiation from the at least one electromagnetic antenna as the proppant flows from the inner core through the at least one mesh ceramic portion to the formation.

9. The method of claim 8 , wherein the ceramic particles range in size from about 106 micrometers to about 2.36 millimeters.

10. The method of claim 8 , wherein the ceramic particles are less than 2 micrometers.

11. A method for enhancing recovery of heavy oil from a formation, comprising the steps of:

suspending a downhole tool with a connector above a wellbore;

removeably lowering the downhole tool in the wellbore, the downhole tool comprising an inner core that is operable to allow the flow of fluid, an outer core comprising at least one mesh ceramic portion and at least one solid ceramic portion, and at least one electromagnetic antenna disposed between the inner core and outer core;

emitting electromagnetic radiation from the at least one electromagnetic antenna to heat the at least one mesh ceramic portion and the at least one solid ceramic portion to a temperature higher than the boiling point of the fluid;

injecting the fluid into the inner core;

flowing the fluid from the inner core through the at least one mesh ceramic portion to the formation; and

converting the fluid to steam as it flows through the at least one mesh ceramic portion.

12. The method of claim 11 , wherein the fluid is water.

13. The method of claim 11 , wherein the step of heating the at least one mesh ceramic portion and the at least one solid ceramic portion comprises heating the at least one mesh ceramic portion and the at least one solid ceramic portion to at least about 1000° C.

14. The method of claim 11 , wherein the step of emitting electromagnetic radiation comprises emitting electromagnetic radiation with frequency ranges from 300 MHz to 300 GHz.

15. The method of claim 11 , further comprising:

placing production tubing in a second wellbore below the first wellbore;

reducing the viscosity of heavy oil located in the formation with the steam to produce a reduced viscosity heavy oil;

draining the reduced viscosity heavy oil to a region containing the second wellbore; and

flowing the reduced viscosity heavy oil into the production tubing to be produced from the formation.

16. The method of claim 11 , wherein the at least one ceramic portion comprises silica, alumina, magnesium oxide, potassium, iron III oxide, calcium oxide, sodium oxide, and titanium oxide.

17. The method of claim 11 , further comprising:

injecting a proppant comprising ceramic particles into the inner core; and

heating the ceramic particles in the proppant with the electromagnetic radiation from the at least one electromagnetic antenna as the proppant flows from the inner core through the at least one mesh ceramic portion to the formation.

18. The method of claim 17 , wherein the ceramic particles range in size from about 106 micrometers to about 2.36 millimeters.

19. The method of claim 17 , wherein the ceramic particles are less than 2 micrometers.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 3, 2014
From: BATARSEH, SAMEEH ISSA
To: SAUDI ARABIAN OIL COMPANY
Reel/Frame 032117/0640 →
Continuity (2)
Provisional Application 61847681 · Jul 18, 2013
Related Publication 20150021013A1 · Jan 22, 2015