Treated geothermal brine compositions with reduced concentrations of silica, iron and manganese
This invention relates to treated geothermal brine compositions containing reduced concentrations of iron, silica, and manganese compared to the untreated brines. Exemplary compositions contain a concentration of manganese less than 10 mg/kg, a concentration of silica ranging from less than 10 mg/kg, and a concentration of iron less than 10 mg/kg, and the treated geothermal brine is derived from a Salton Sea geothermal reservoir.
1. A method of using an aqueous treated geothermal brine composition, the method comprising providing an aqueous treated geothermal brine comprising a concentration of dissolved manganese greater than zero and no more than 200 mg/kg, a concentration of dissolved silica of 0 mg/kg to 80 mg/kg, and a concentration of dissolved iron of 0 mg/kg to 300 mg/kg; and providing the aqueous treated geothermal brine composition to a process for mineral extraction, wherein the step of providing the aqueous treated geothermal brine composition comprises adding a silica precipitate seed to a natural or synthetic geothermal brine to form the aqueous treated geothermal brine composition.
2. A method of using an aqueous treated geothermal brine composition, the method comprising providing an aqueous treated geothermal brine comprising a concentration of dissolved manganese greater than zero and no more than 200 mg/kg, a concentration of dissolved silica of 0 mg/kg to 80 mg/kg, and a concentration of dissolved iron of 0 mg/kg to 300 mg/kg; and providing the aqueous treated geothermal brine composition to a process for mineral extraction, wherein the step of providing the aqueous treated geothermal brine composition comprises contacting a natural or synthetic geothermal brine with aluminum salts to form the aqueous treated geothermal brine composition.
3. A method of using an aqueous treated geothermal brine composition, the method comprising providing an aqueous treated geothermal brine comprising a concentration of dissolved manganese greater than zero and no more than 200 mg/kg, a concentration of dissolved silica of 0 mg/kg to 80 mg/kg, and a concentration of dissolved iron of 0 mg/kg to 300 mg/kg; and providing the aqueous treated geothermal brine composition to a process for mineral extraction, wherein the step of providing the aqueous treated geothermal brine composition comprises contacting a natural or synthetic geothermal brine with iron (III) hydroxide to form the aqueous treated geothermal brine composition.
4. A method of using an aqueous treated geothermal brine composition, the method comprising providing an aqueous treated geothermal brine comprising a concentration of dissolved manganese greater than zero and no more than 200 mg/kg, a concentration of dissolved silica of 0 mg/kg to 80 mg/kg, and a concentration of dissolved iron of 0 mg/kg to 300 mg/kg; and providing the aqueous treated geothermal brine composition to a process for mineral extraction, wherein the step of providing the aqueous treated geothermal brine composition comprises contacting a natural or synthetic geothermal brine with alumina absorbents to form the aqueous treated geothermal brine composition.