Chloroprene rubber, method for producing same, chloroprene rubber composition and vulcanized product of chloroprene rubber composition

Inventors: Sachiyo Kishi (Itoigawa, JP); Hiroyuki Yashima (Itoigawa, JP); Hidehiro Matsuda (Itoigawa, JP)
Assignee: DENKA COMPANY LIMITED
C08F36/18C08F136/18C08F236/18C08L11/00C08L93/04
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,464,146
App. No.
14/417,007
Granted
Oct 11, 2016
Kind
B2
Abstract

Provided are a chloroprene rubber that is less adhesive to rolls and gives a vulcanized product superior in physical properties, a production method thereof, a chloroprene rubber composition and a vulcanized product thereof. A chloroprene rubber comprising a steroid skeleton-containing compound. The chloroprene rubber may contain a steroid skeleton-containing compound in an amount of 0.01 to 1 mass %. A vulcanized product is prepared by vulcanizing a composition containing the chloroprene rubber. The chloroprene rubber can be prepared, for example, by emulsion-polymerizing chloroprene alone or chloroprene and other monomers in combination in the presence of a rosin containing a steroid skeleton-containing compound.

Claims (7)

1. A chloroprene rubber comprising a steroid skeleton-containing compound;

wherein the chloroprene rubber comprises the steroid skeleton-containing compound in an amount of 0.05 to 0.832 mass %.

2. A method for producing a chloroprene rubber, comprising emulsion-polymerizing chloroprene alone or chloroprene and other monomers in the presence of a rosin containing a steroid skeleton-containing compound, wherein the chloroprene rubber comprises the steroid skeleton-containing compound in an amount of 0.05 to 0.832 mass %.

3. The method for producing a chloroprene rubber according to claim 2 , wherein the rosin contains a steroid skeleton-containing compound in an amount of 0.2 to 20 mass %.

4. A chloroprene rubber composition comprising the chloroprene rubber according to claim 1 .

5. A vulcanized product prepared by vulcanizing the chloroprene rubber composition according to claim 4 .

6. The method for producing a chloroprene rubber according to claim 3 , wherein the rosin contains a steroid skeleton-containing compound in an amount of 0.3 to 8.0 mass %.

Assignments (2)
CHANGE OF NAME Recorded Aug 4, 2016
From: DENKI KAGAKU KOGYO KABUSHIKI KAISHA
To: DENKA COMPANY LIMITED
Reel/Frame 039626/0832 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 26, 2015
From: KISHI, SACHIYO; YASHIMA, HIROYUKI; MATSUDA, HIDEHIRO
To: DENKI KAGAKU KOGYO KABUSHIKI KAISHA
Reel/Frame 034810/0886 →
Priority Claims (1)
JP 2012-164574 · Jul 25, 2012 · national
Continuity (1)