IP Library › Granted Patent US 9,972,445
Granted Patent B2
US 9,972,445 · App. 14/744,932 · Granted May 15, 2018

Electrolytic capacitor and method of manufacturing the same

Inventors: Kazuya Koseki (Kawasaki, JP); Kouichi Kuroda (Sukagawa, JP); Masao Sakakura (Sukagawa, JP); Tomohiro Matsuzaki (Sukagawa, JP); Takayuki Nakaji (Osaki, JP)
Assignee: NIPPON CHEMI-CON CORPORATION
H01G9/145H01G9/0036H01G9/028H01G9/035H01G9/042H01G9/151
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,972,445
App. No.
14/744,932
Granted
May 15, 2018
Kind
B2
Abstract

Provided are an electrolytic capacitor with high withstand voltage capable of preventing deterioration of withstand voltage characteristics caused by lead-free reflow or the like and improving ESR characteristics, and a manufacturing method thereof. The electrolytic capacitor is obtained by impregnating a capacitor element in which an anode electrode foil and a cathode electrode foil are wound with a separator interposed, with a dispersion containing: particles of a conductive polymer; sorbitol or sorbitol and polyalcohol; and a solvent so as to form a solid electrolyte layer containing 60 to 92 wt % of the sorbitol or the sorbitol and polyalcohol, and by filling an electrolytic solution containing ethylene glycol in a gap portion in the capacitor element on which the solid electrolyte layer is formed.

Claims (32)

1. An electrolytic capacitor comprising:

a capacitor element including an anode electrode foil and a cathode electrode foil that are wound with a separator interposed therebetween;

a solid electrolyte layer formed on the capacitor element and containing conductive polymer and sorbitol and polyalcohol, a content of sorbitol and polyalcohol contained in the solid electrolyte layer being 60 to 92 wt %; and

an electrolytic solution containing ethylene glycol and filled in a gap portion in the capacitor element on which the solid electrolyte layer is formed,

a content of ethylene glycol contained in the electrolytic solution being 10 wt % or more with respect to a solvent in the electrolytic solution.

2. The electrolytic capacitor according to claim 1 , wherein

the content of ethylene glycol contained in the electrolytic solution is 40 wt % or more with respect to the solvent in the electrolytic solution.

3. The electrolytic capacitor according to claim 2 , wherein

the polyalcohol is ethylene glycol.

4. The electrolytic capacitor according to claim 2 , wherein

the electrolytic solution contains γ-butyrolactone as the solvent and contains a solute selected from ammonium salt, quaternary ammonium salt, quaternized amidinium salt and amine salt of at least one type of organic acids, inorganic acids as well as composite compounds of organic acids and inorganic acids.

5. The electrolytic capacitor according to claim 2 , wherein

the solvent of the electrolytic solution includes at least one type of solvent selected from sulfolane, 3-methyl sulfolane and 2,4-dimethyl sulfolane.

6. The electrolytic capacitor according to claim 1 , wherein the polyalcohol is ethylene glycol.

7. The electrolytic capacitor according to claim 6 , wherein

the electrolytic solution contains γ-butyrolactone as the solvent and contains a solute selected from ammonium salt, quaternary ammonium salt, quaternized amidinium salt and amine salt of at least one type of organic acids, inorganic acids as well as composite compounds of organic acids and inorganic acids.

8. The electrolytic capacitor according to claim 6 , wherein

the solvent of the electrolytic solution includes at least one type of solvent selected from sulfolane, 3-methyl sulfolane and 2,4-dimethyl sulfolane.

9. The electrolytic capacitor according to claim 1 , wherein the electrolytic solution contains sorbitol.

10. The electrolytic capacitor according to claim 9 , wherein

a content of sorbitol contained in the electrolytic solution is 1 to 10 wt % with respect to the solvent in the electrolytic solution.

11. The electrolytic capacitor according to claim 1 , wherein

the electrolytic solution contains γ-butyrolactone as the solvent and contains a solute selected from ammonium salt, quaternary ammonium salt, quaternized amidinium salt and amine salt of at least one type of organic acids, inorganic acids as well as composite compounds of organic acids and inorganic acids.

12. The electrolytic capacitor according to claim 1 , wherein

the solvent of the electrolytic solution includes at least one type of solvent selected from sulfolane, 3-methyl sulfolane and 2,4-dimethyl sulfolane.

13. A method for manufacturing an electrolytic capacitor, including:

an impregnation process impregnating a conductive polymer compound dispersion containing particles of a conductive polymer, sorbitol and polyalcohol and a solvent into a capacitor element including an anode electrode foil and a cathode electrode foil wound with a separator interposed therebetween;

a solid electrolyte formation process forming a solid electrolyte layer in the capacitor element by drying the capacitor element after the impregnation process, a content of the sorbitol and polyalcohol contained in the solid electrolyte layer being 60 to 92 wt %; and

an electrolytic solution filling process filling an electrolytic solution containing ethylene glycol in a gap portion in the capacitor element in which the solid electrolyte layer is formed,

a content of ethylene glycol contained in the electrolytic solution being 10 wt % or more with respect to a solvent in the electrolytic solution.

14. A method for manufacturing an electrolytic capacitor according to claim 13 , wherein

the content of ethylene glycol contained in the electrolytic solution is 40 wt % or more with respect to a solvent in the electrolytic solution.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 21, 2015
From: KOSEKI, KAZUYA; KURODA, KOUICHI; SAKAKURA, MASAO; MATSUZAKI, TOMOHIRO; NAKAJI, TAKAYUKI
To: NIPPON CHEMI-CON CORPORATION
Reel/Frame 035873/0281 →
Priority Claims (1)
JP 2012-280278 · Dec 21, 2012 · national
Continuity (2)
Continuation PCTJP2013083567 · Dec 16, 2013
Related Publication 20150287540A1 · Oct 8, 2015