IP Library › Granted Patent US 10,082,700
Granted Patent B2
US 10,082,700 · App. 14/757,849 · Granted Sep 25, 2018

Antireflection film and organic light emitting diode device including the same

Inventors: Tsuyoshi Ohyama (Suwon-si, KR); Koh Kamada (Suwon-si, KR); Eun Sung Lee (Gyeonggi-do, KR)
Assignee: SAMSUNG ELECTRONICS CO., LTD.
G02F1/13363G02B1/11G02B5/3016G02F1/133634G02F1/133528H01L51/5281
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,082,700
App. No.
14/757,849
Granted
Sep 25, 2018
Kind
B2
Abstract

An antireflection film includes a polarizer, a first phase delay layer, and a second phase delay layer, where at least one of the first phase delay layer and the second phase delay layer includes a liquid crystal layer, and the liquid crystal layer includes liquid crystals oriented in a direction tilting obliquely with respect to a surface thereof.

Claims (71)

1. An antireflection film comprising

a polarizer;

a first phase delay layer, the first phase delay layer being a λ/2 phase delay layer; and

a second phase delay layer, the second phase delay layer being a λ/4 phase delay layer,

wherein the second phase delay layer comprises a liquid crystal layer having a first surface and a second surface opposite to the first surface,

wherein the liquid crystal layer comprises liquid crystals oriented in a direction tilting obliquely with respect to a surface thereof,

tilt angles of the liquid crystals becomes gradually increased from the first surface to the second surface,

in-plane retardation (R e0 ) of a combination of the first phase delay layer and the second phase delay layer for about 450 nm, about 550 nm and about 650 nm wavelengths satisfies the following inequation: R e0 (450 nm)≤R e0 (550 nm)≤R e0 (650 nm),

wherein R e0 (450 nm) denotes in-plane retardation of the combination of the first phase delay layer and the second phase delay layer for incident light of about 450 nm wavelength,

R e0 (550 nm) denotes in-plane retardation of the combination of the first phase delay layer and the second phase delay layer for incident light of about 550 nm wavelength, and

R e0 (650 nm) denotes in-plane retardation of the combination of the first phase delay layer and the second phase delay layer for incident light of about 650 nm wavelength.

2. The antireflection film of claim 1 , wherein a maximum tilt angle of the liquid crystals is in a range from about 30 degrees to about 75 degrees.

3. The antireflection film of claim 1 , wherein a tilt angle of the liquid crystals near the first surface is greater than about zero degree)(0°) and less than or equal to about 5 degrees.

4. The antireflection film of claim 3 , wherein the second phase delay layer further comprises an alignment layer contacting the first surface of the liquid crystal layer.

5. The antireflection film of claim , wherein in-plane retardation (R e2 ) of the liquid crystal layer for about 450 nm, about 550 nm and about 650 nm wavelengths satisfies the following inequations: 0.95 ≤R e2 (450 nm)/R e2 (550 nm); and 0.95≤R e2 (550 nm)/R e2 (650 nm),

wherein

R e2 (450 nm) denotes in-plane retardation of the liquid crystal layer for incident light of about 450 nm wavelength,

R e2 (550 nm) denotes in-plane retardation the liquid crystal layer for incident light of about 550 nm wavelength, and

R e2 (650 nm) denotes in-plane retardation of the liquid crystal layer for incident light of about 650 nm wavelength.

6. The antireflection film of claim , wherein the wavelength dispersion of the liquid crystal layer satisfies the following inequation: 1.0≤R e2 (450 nm)/R e2 (550 nm) ≤1.2,

Wherein R e2 (450 nm) denotes in-plane retardation of the liquid crystal layer for incident light of about 450 nm wavelength, and R e2 (550 nm) denotes in-plane retardation of the liquid crystal layer for incident light of about 550 nm wavelength.

7. The antireflection film of claim , wherein short wavelength dispersion of a combination of the first phase delay layer and the second phase delay layer satisfies the following inequation: 0.7≤R e0 (450 nm)/R e0 (550 nm)≤1.0,

Wherein R e0 (450 nm) denotes in-plane retardation of the combination of the first phase delay layer and the second phase delay layer for incident light of about 450 nm wavelength, and

R e0 (550 nm) denotes in-plane retardation of the combination of the first phase delay layer and the second phase delay layer for incident light of about 550 nm wavelength.

8. The antireflection film of claim 1 , wherein an angle (θ a ) between an optical axis of the first phase delay layer and an optical axis of the polarizer and an angle (θ b ) between an optical axis of the second phase delay layer and an optical axis of the polarizer satisfy the following equation: θ b =2θ a +45°.

9. The antireflection film of claim 1 , wherein the first phase delay layer has refractive indices satisfying the following inequations: n x1 >n y1 ;

and n x1 ≤n z1 ,

Wherein n x1 denotes a refractive index at a slow axis of the first phase delay layer,

n y1 denotes a refractive index at a fast axis of the first phase delay layer, and

n z1 denotes a refractive index in a direction perpendicular to the slow and fast axes of the first phase delay layer.

10. The antireflection film of claim 9 , wherein the first phase delay layer comprises an elongated polymer layer.

11. The antireflection film of claim 1 , wherein the antireflection film comprises the polarizer, the first phase delay layer disposed on the polarizer, and the second phase delay layer disposed between the polarizer and the first phase delay layer.

12. The antireflection film of claim 1 , wherein the antireflection film comprises the polarizer, the first phase delay layer, and the second phase delay stacked sequentially.

13. An organic light emitting diode device comprising:

an organic light emitting display panel; and

an antireflection film on the organic light emitting display panel, the antireflection film comprising:

a polarizer;

a first phase delay layer, the first phase delay layer being a λ/2 phase delay layer; and

a second phase delay layer, the second phase delay layer being a λ/4 phase delay layer,

wherein the second phase delay layer comprises a liquid crystal layer having a first surface and a second surface opposite to the first surface, and

the liquid crystal layer comprises liquid crystals oriented in a direction tilting obliquely with respect to a surface thereof,

tilt angles of the liquid crystals becomes gradually increased from the first surface to the second surface,

in-plane retardation (R e0 ) of a combination of the first phase delay layer and the second phase delay layer for about 450 nm, about 550 nm and about 650 nm wavelengths satisfies the following inequation: R e0 (450 nm)≤ e0 (550 nm)≤ e0 (650 nm),

wherein R e0 (450 nm) denotes in-plane retardation of the combination of the first phase delay layer and the second phase delay layer for incident light of about 450 nm wavelength,

R e0 (550 nm) denotes in-plane retardation of the combination of the first phase delay layer and the second phase delay layer for incident light of about 550 nm wavelength, and

R e0 (650 nm) denotes in-plane retardation of the combination of the first phase delay layer and the second phase delay layer for incident light of about 650 nm wavelength.

14. The organic light emitting diode device of claim 13 wherein

the first surface of the liquid crystal layer is disposed closer to the polarizer than the organic light emitting display panel, and

the second surface of the liquid crystal layer is disposed closer to the organic light emitting display panel than the polarizer.

15. The organic light emitting diode device of claim 13 , wherein a maximum tilt angle of the liquid crystals is in a range from about 30 degrees to about 75 degrees.

16. The organic light emitting diode device of claim 13 , wherein a tilt angle of the liquid crystals near the first surface is greater than about zero degree(0°) and less than or equal to about 5 degrees.

17. The organic light emitting diode device of claim 13 , wherein the second phase delay layer further comprises an alignment layer contacting the first surface of the liquid crystal layer.

18. The organic light emitting diode device of claim 13 , wherein in-plane retardation (R e2 ) of the liquid crystal layer for about 450 nm, about 550 nm, and about 650 nm wavelengths satisfies the following inequations: 0.95≤R e2 (450 nm)/R e2 (550 nm); and 0.95≤R e2 (550 nm)/R e2 (650 nm),

wherein R e2 (450 nm) denotes in-plane retardation of the liquid crystal layer for incident light of about 450 nm wavelength,

R e2 (550 nm) denotes in-plane retardation the liquid crystal layer for incident light of about 550 nm wavelength, and

R e2 (650 nm) denotes in-plane retardation of the liquid crystal layer for incident light of about 650 nm wavelength.

19. The organic light emitting diode device of claim 13 , wherein wavelength dispersion of the liquid crystal layer satisfies the following inequation: 1.0≤R e2 (450 nm)/R e2 (550 nm)≤1.2,

Wherein R e2 (450nm) denotes in-plane retardation of the liquid crystal layer for incident light of about 450nm wavelength, and

R e2 (550 nm) denotes in-plane retardation of the liquid crystal layer for incident light of about 550 nm wavelength.

20. The organic light emitting diode device of claim 13 , wherein short wavelength dispersion of a combination of the first phase delay layer and the second phase delay layer satisfies the following inequation: 0.7≤R e0 (450 nm)/R e0 (550 nm)≤1.0,

Wherein R e0 (450 nm) denotes in-plane retardation of the combination of the first phase delay layer and the second phase delay layer for incident light of about 450 nm wavelength, and

R e0 (550 nm) denotes in-plane retardation of the combination of the first phase delay layer and the second phase delay layer for incident light of about 550 nm wavelength.

21. The organic light emitting diode device of claim 13 , wherein an angle (θ a ) between an optical axis of the first phase delay layer and an optical axis of the polarizer and an angle (θ b ) between an optical axis of the second phase delay layer and an optical axis of the polarizer satisfy the following equation: θ b =2θ a +45°.

22. The organic light emitting diode device of claim 13 , wherein the first phase delay layer has a refractive index that simultaneously satisfies the following inequations: n x1 >n y1 ; and n x1 >n z1

wherein

n x1 denotes a refractive index at a slow axis of the first phase delay layer,

n y1 denotes a refractive index at a fast axis of the first phase delay layer, and

n z1 denotes a refractive index in a direction perpendicular to the slow and fast axes of the first phase delay layer.

23. The organic light emitting diode device of claim 13 , wherein the first phase delay layer comprises an elongated polymer layer.

24. The organic light emitting diode device of claim 13 , wherein the antireflection film comprises the polarizer, the first phase delay layer disposed on the polarizer, and the second phase delay layer disposed between the polarizer and the first phase delay layer.

25. The organic light emitting diode device of claim 13 , wherein the antireflection film comprises the polarizer, the first phase delay layer, and the second phase delay stacked sequentially.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 5, 2018
From: OHYAMA, TSUYOSHI; KAMADA, KOH; LEE, EUN SUNG
To: SAMSUNG ELECTRONICS CO., LTD.
Reel/Frame 044545/0680 →
Priority Claims (1)
KR 10-2014-0190805 · Dec 26, 2014 · national
Continuity (1)
Related Publication 20160211486A1 · Jul 21, 2016