Aluminum cylinder block and method of manufacture
A cast cylinder block for an internal combustion engine includes a first and a second cylinder bore and a shared bore wall. The first cylinder bore includes a first bore wall and the second cylinder bore includes a second bore wall. The shared cylinder bore wall includes a first portion and a second portion. A portion of the first bore wall combines with a portion of the second bore wall to form the shared cylinder bore wall. The first portion of the shared bore wall is an as-cast portion. The second portion of the shared bore wall is a metal matrix composite.
1. A method of manufacturing a cylinder block having a shared cylinder bore wall with a portion of the shared cylinder bore wall including a metal matrix composite, the method comprising:
providing a preform of a compacted powder;
disposing the preform into a prescribed position of a sand core tool cavity;
depositing a sand and resin mixture into the sand core tool cavity, curing the sand and resin mixture into a cured sand core, and removing the cured sand core from the tool cavity;
assembling the cured sand core into a sand core assembly and placing the sand core assembly into a mold;
pouring an aluminum alloy into the mold to form the cylinder block;
cleaning the cylinder block after allowing the aluminum alloy to solidify; and
executing a friction stir process for mixing the preform with a portion of the aluminum alloy that is adjacent to the preform to form a metal matrix composite.
2. The method of manufacturing the cylinder block of claim 1 further comprising heat treating the cylinder block.
3. The method of manufacturing the cylinder block of claim 1 wherein providing a preform of a compacted powder further comprises providing a preform of a compacted powder including at least one of an intermetallic powder, an oxide, a carbide, and a nitride.
4. The method of manufacturing the cylinder block of claim 1 wherein the executing of the friction stir process further comprises executing the friction stir process using a friction stir process tool having a flat shoulder and a threaded cylindrical pin for mixing the preform with the adjacent aluminum alloy to form the metal matrix composite.
5. The method of manufacturing the cylinder block of claim 1 wherein the executing of the friction stir process further comprises inserting a friction stir process tool into the shared cylinder bore wall and generating heat for mixing the preform with the adjacent aluminum alloy to form the metal matrix composite.
6. The method of manufacturing the cylinder block of claim 1 wherein depositing a sand and resin mixture into the sand core tool cavity, curing the sand and resin mixture into a cured sand core, and removing the cured sand core from the tool cavity further comprises depositing a sand and resin mixture into the sand core tool cavity, curing the sand and resin mixture into a cured water jacket sand core, and removing the cured water jacket sand core from the tool cavity.
7. The method of manufacturing the cylinder block of claim 1 wherein providing a preform of a compacted powder further comprises providing a preform of a compacted powder having at least one retainer.
8. A method of manufacturing a cylinder block having a shared cylinder bore wall with a portion of the shared cylinder bore wall including a metal matrix composite, the method comprising:
providing a preform of a compacted powder including at least one of an intermetallic powder, an oxide, a carbide, and a nitride;
disposing the preform into a prescribed position of a sand core tool cavity;
depositing a sand and resin mixture into the sand core tool cavity, curing the sand and resin mixture into a cured sand core, and removing the cured sand core from the tool cavity;
assembling the cured sand core into a sand core assembly and placing the sand core assembly into a mold;
pouring an aluminum alloy into the mold to form the cylinder block;
cleaning the cylinder block after allowing the aluminum alloy to solidify; and
executing a friction stir process for mixing the preform with adjacent aluminum alloy to form a metal matrix composite.
9. The method of manufacturing the cylinder block of claim 8 wherein executing a friction stir process for mixing the preform with adjacent aluminum alloy to form a metal matrix composite further comprises heat treating the cylinder block and executing a friction stir process for mixing the preform with adjacent aluminum alloy to form a metal matrix composite.
10. The method of manufacturing the cylinder block of claim 8 wherein executing a friction stir process for mixing the preform with adjacent aluminum alloy to form a metal matrix composite further comprises executing a friction stir process using a friction stir process tool having a flat shoulder and a threaded cylindrical pin for mixing the preform with adjacent aluminum alloy to form a metal matrix composite further comprises.
11. The method of manufacturing the cylinder block of claim 8 wherein executing a friction stir process for mixing the preform with adjacent aluminum alloy to form a metal matrix composite further comprises executing a friction stir process, inserting a friction stir process tool into the shared cylinder bore wall and generating heat for mixing the preform with adjacent aluminum alloy to form a metal matrix.
12. The method of manufacturing the cylinder block of claim 8 wherein depositing a sand and resin mixture into the sand core tool cavity, curing the sand and resin mixture into a cured sand core, and removing the cured sand core from the tool cavity further comprises depositing a sand and resin mixture into the sand core tool cavity, curing the sand and resin mixture into a cured water jacket sand core, and removing the cured water jacket sand core from the tool cavity.
13. The method of manufacturing the cylinder block of claim 8 wherein providing a preform of a compacted powder further comprises providing a preform of a compacted powder having at least one retainer.