IP Library › Granted Patent US 11,434,388
Granted Patent B2
US 11,434,388 · App. 15/025,632 · Granted Sep 6, 2022

Refill for writing, drawing and/or painting devices and method for the production thereof

Inventors: Andreas Thies (Effeltrich, DE); Martin Jakob (Hallstadt, DE); Jürgen Adler (Kleinseebach, DE)
Assignee: STAEDTLER MARS GMBH & CO. KG
C09D13/00C08L67/04C08L91/06C08K3/013C08K3/04
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,434,388
App. No.
15/025,632
Granted
Sep 6, 2022
Kind
B2
Abstract

A polymer-bound refill for writing, drawing and/or painting devices, in particular for pencils or coloured pencils, including at least one binder, at least one wax, at least one colouring agent and at least one filler. The refill includes polylactide as binder.

Claims (13)

1. A polymer-bonded refill for writing, drawing and/or painting tools, comprising: a binder; a wax; graphite as a colorant; and a filler, wherein the filler includes graphite, wherein the binder is formed by 10-25% by weight of polylactide based on weight of the entire polymer-bonded refill composition, wherein the polymer-bonded refill is a pencil lead refill and includes the following:

5% to 15% by weight

wax

0.1% to 2.5% by weight

palm oil

remainder

graphite.

2. The polymer-bonded refill as claimed in claim 1 , wherein the wax is at least one wax selected from the group consisting of fatty acids, stearates, montan waxes, amide waxes and paraffin waxes.

3. The polymer-bonded refill as claimed in claim 1 , wherein the wax is ethylene-bis-stearamide (EBS) and/or calcium stearate.

4. A method for manufacturing the polymer-bonded refill as claimed in claim 1 , comprising the steps of:

mixing and granulating the binder, the wax, the colorant and the filler to form a refill granulate; and

extruding the refill granulate to form the polymer-bonded refill.

5. The method according to claim 4 , including extruding the refill granulate at a temperature in a range of 120° C. to 200° C.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 27, 2023
From: STAEDTLER MARS GMBH & CO. KG
To: STAEDTLER SE
Reel/Frame 065678/0156 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 29, 2016
From: THIES, ANDREAS; JAKOB, MARTIN; ADLER, JÜRGEN
To: STAEDTLER MARS GMBH & CO. KG
Reel/Frame 038122/0387 →
Priority Claims (1)
DE 10 2013 016 355.2 · Oct 1, 2013 · national
Continuity (1)
Related Publication 20160237295A1 · Aug 18, 2016