IP Library Granted Patent US 9,896,346
Granted Patent B2
US 9,896,346 · App. 15/079,837 · Granted Feb 20, 2018

Synthesis method of lithium-titanium oxide using solid-state method

Inventors: Yi-Hyun Park (Daejeon, KR); Seungyon Cho (Daejeon, KR); Mu-Young Ahn (Daejeon, KR); Kyung-Mi Min (Incheon, KR)
Assignee: KOREA BASIC SCIENCE INSTITUTE
C01G23/005G21B1/13C01P2002/72C01P2004/03Y02E30/128
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,896,346
App. No.
15/079,837
Granted
Feb 20, 2018
Kind
B2
Abstract

A method for synthesizing lithium-titanium oxide using a solid state method includes: mixing lithium oxide (Li 2 O) and titanium oxide (TiO 2 ) in a solvent; separating a solid material which includes lithium oxide and titanium oxide from the solvent; drying the solid material separated from the solvent; and performing a heat treatment on the solid material.

Claims (15)

1. A method for synthesizing a lithium-titanium oxide using a solid state method, comprising:

mixing lithium oxide (Li 2 O) and titanium oxide (TiO 2 ) in a solvent;

separating a solid material which includes lithium oxide and titanium oxide from the solvent;

drying the solid material separated from the solvent; and

performing a heat treatment on the solid material,

wherein a molar ratio of lithium oxide to titanium oxide is 1:0.940 or more to less than 1:1.

2. The method of claim 1 , wherein a molar ratio of lithium oxide to titanium oxide is in the range of 1:0.940 to 1:0.944.

3. The method of claim 2 , wherein the titanium oxide has an anatase crystal structure.

4. The method of claim 1 , wherein titanium oxide has a rutile crystal structure and a molar ratio of lithium oxide to titanium oxide is 1:0.942.

5. The method of claim 1 , wherein the heat treatment is performed at 600° C. or more to less than 800° C.

6. The method of claim 1 , wherein the heat treatment is performed at 670° C. or more to less than 800° C.

7. The method of claim 1 , wherein the heat treatment is performed for 12 hours or more.

8. The method of claim 1 , wherein the titanium oxide has an anatase crystal structure.

9. The method of claim 1 , wherein lithium-titanium oxide prepared in the performing of the heat treatment has a Li 2 TiO 3 structure.

10. The method of claim 1 , wherein the solvent includes an alcohol.

Assignments (3)
CORRECTIVE ASSIGNMENT TO CORRECT THE RECEIVING PARTY POSTAL CODE PREVIOUSLY RECORDED ON REEL 055585 FRAME 0627. ASSIGNOR(S) HEREBY CONFIRMS THE ASSIGNMENT. Recorded Mar 24, 2021
From: KOREA BASIC SCIENCE INSTITUTE
To: KOREA INSTITUTE OF FUSION ENERGY
Reel/Frame 055695/0192 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 15, 2021
From: KOREA BASIC SCIENCE INSTITUTE
To: KOREA INSTITUTE OF FUSION ENERGY
Reel/Frame 055585/0627 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 24, 2016
From: PARK, YI-HYUN; CHO, SEUNGYON; AHN, MU-YOUNG; MIN, KYUNG-MI
To: KOREA BASIC SCIENCE INSTITUTE
Reel/Frame 038094/0238 →
Priority Claims (1)
KR 10-2015-0052214 · Apr 14, 2015 · national
Continuity (1)