IP Library › Granted Patent US 10,574,122
Granted Patent B2
US 10,574,122 · App. 15/404,433 · Granted Feb 25, 2020

Method of forming a rotor

Inventors: Thomas A. Perry (Bruce Township, MI); James G. Schroth (Troy, MI); Sean R. Wagner (Shelby Township, MI)
Assignee: GM Global Technology Operations LLC
H02K15/03C21D6/008C21D7/06C21D9/0068C23C8/26C23C8/32C23C8/38C23C8/50H02K1/2766Y10T29/49009Y10T29/49012
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,574,122
App. No.
15/404,433
Granted
Feb 25, 2020
Kind
B2
Abstract

A method of forming a rotor includes isolating a bridge area of an electrical steel lamination. The bridge area is disposed between a first portion of the electrical steel lamination and a second portion of the electrical steel lamination that is adjacent to the first portion. Each of the first portion, the second portion, and the bridge area has an initial hardness, and the electrical steel lamination has an initial magnetic permeability. After isolating, the method includes hardening only the bridge area so that the bridge area has a treated hardness that is greater than the initial hardness. Concurrent to hardening, the method includes decreasing the initial magnetic permeability at only the bridge area.

Claims (49)

1. A method of forming a rotor, the method comprising:

isolating a bridge area of an electrical steel lamination;

wherein the bridge area is disposed between:

a first portion of the electrical steel lamination; and

a second portion of the electrical steel lamination that is adjacent to the first portion;

wherein each of the first portion, the second portion, and the bridge area has an initial hardness;

wherein the electrical steel lamination has an initial magnetic permeability;

after isolating, hardening only the bridge area so that the bridge area has a treated hardness that is greater than the initial hardness; and

concurrent to hardening, decreasing the initial magnetic permeability at only the bridge area.

2. The method of claim 1 , further including, concurrent to hardening, maintaining the initial hardness of the first portion and the second portion.

3. The method of claim 1 , further including, concurrent to decreasing, maintaining the initial magnetic permeability at the first portion and the second portion.

4. The method of claim 1 , wherein isolating includes masking off the first portion and the second portion from the bridge area.

5. The method of claim 1 , wherein hardening includes increasing a yield strength and an ultimate tensile strength of only the bridge area.

6. The method of claim 1 , wherein hardening includes nitriding only the bridge area.

7. The method of claim 6 , wherein hardening includes nitrocarburizing only the bridge area.

8. The method of claim 1 , wherein the electrical steel lamination has an interior edge and an outer edge spaced apart from the interior edge and further wherein the electrical steel lamination defines a slot therethrough between the interior edge and the outer edge; and

wherein hardening includes strengthening the bridge area at an end of the slot.

9. The method of claim 8 , wherein hardening includes strengthening the bridge area along a periphery of the slot.

10. The method of claim 1 , wherein the electrical steel lamination has a contact surface; and

further including applying a reactive material to the contact surface at only the bridge area.

11. The method of claim 10 , further including, after applying, thermally activating the reactive material.

12. The method of claim 1 , wherein hardening includes peening only the bridge area.

13. The method of claim 1 , wherein the electrical steel lamination has a contact surface; and

wherein hardening includes impinging a plurality of ions with the contact surface at only the bridge area.

14. The method of claim 1 , further including preventing a transformation from ferrite to austenite at the first portion and the second portion.

15. A method of forming a rotor, the method comprising:

isolating a first bridge area of a first electrical steel lamination;

wherein the first bridge area is disposed between:

a first portion of the first electrical steel lamination; and

a second portion of the first electrical steel lamination that is adjacent to the first portion;

wherein each of the first portion, the second portion, and the first bridge area has a first initial hardness;

wherein the first electrical steel lamination has a first initial magnetic permeability;

isolating a second bridge area of a second electrical steel lamination;

wherein the second bridge area is disposed between:

a third portion of the second electrical steel lamination; and

a fourth portion of the second electrical steel lamination that is adjacent to the third portion;

wherein each of the third portion, the fourth portion, and the second bridge area has a second initial hardness;

wherein the second electrical steel lamination has a second initial magnetic permeability;

after isolating the first bridge area and the second bridge area, hardening only the first bridge area and the second bridge area so that the first bridge area has a first treated hardness that is greater than the first initial hardness and the second bridge area has a second treated hardness that is greater than the second initial hardness; and

concurrent to hardening, decreasing the first initial magnetic permeability at only the first bridge area and decreasing the second initial magnetic permeability at only the second bridge area.

16. The method of claim 15 , further including, after hardening, stacking the first electrical steel lamination adjacent and in contact with the second electrical steel lamination.

17. The method of claim 15 , further including, prior to hardening, stacking the first electrical steel lamination adjacent and in contact with the second electrical steel lamination.

18. The method of claim 15 , further including, isolating a third bridge area of a third electrical steel lamination;

wherein the third bridge area is disposed between:

a fifth portion of the third electrical steel lamination; and

a sixth portion of the third electrical steel lamination that is adjacent to the fifth portion;

wherein each of the fifth portion, the sixth portion, and the third bridge area has a third initial hardness;

maintaining the third initial hardness of the third bridge area by not hardening any of the fifth portion, the sixth portion, and the third bridge area; and

stacking the third electrical steel lamination between the first electrical steel lamination and the second electrical steel lamination.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 30, 2017
From: PERRY, THOMAS A.; SCHROTH, JAMES G.; WAGNER, SEAN R.
To: GM GLOBAL TECHNOLOGY OPERATIONS LLC
Reel/Frame 041123/0178 →
Continuity (1)
Related Publication 20180198352A1 · Jul 12, 2018
Cited By (1)
US 12,656,204