IP Library Granted Patent US 10,710,286
Granted Patent B2
US 10,710,286 · App. 15/437,042 · Granted Jul 14, 2020

In-mold carpet lamination

Inventors: Joseph Packett (Livonia, MI); Ray Pepper (Livonia, MI); Jodi Imler (Livonia, MI); Akbal Grewal (Livonia, MI); Greg Homann (Livonia, MI)
Assignee: NYX, INC.
B29C45/14065B29C45/14786B29C45/561B32B3/02B32B3/266B32B5/02B32B5/06B32B5/26B32B7/12B32B27/08B32B27/12B32B27/32D06N7/0076D06N7/0078B29C2045/14147B29K2715/006B29L2031/7322B32B2250/03B32B2250/24B32B2262/0253B32B2262/0276B32B2307/30B32B2307/50B32B2307/554B32B2307/5825B32B2471/02D06N2203/042
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,710,286
App. No.
15/437,042
Granted
Jul 14, 2020
Kind
B2
Abstract

A process for fabricating a molded carpet laminate includes supporting a carpet layer in a molding tool that has mold dies that define a mold cavity. The mold dies are then moved from an open position to a partially closed position. In the partially closed position, a heated polymer material is injected into the mold cavity. The heated polymer material incompletely fills the mold cavity on the working side of the carpet layer. The mold dies are then moved from the partially closed position to a closed position to spread the heated polymer material and fill the mold cavity on the working side of the carpet layer to form a molded polymer wall. The molded polymer wall adheres to the working side of the carpet layer to form a molded carpet laminate. The mold dies are then moved from the closed position and the molded carpet laminate is cooled.

Claims (20)

1. A process for fabricating a molded carpet laminate, comprising:

supporting a carpet layer in a molding tool that has first and second mold dies that define a mold cavity there between, at least one of the first or second mold dies being moveable such that the mold tool has a closed position, a partially closed position, and an open position relative to the mold cavity, and the carpet layer has a working side and a finish side, the finish side facing the first mold die, wherein the supporting of the carpet layer includes supporting the carpet layer on one or more eccentric pins in the molding tools, each of the eccentric pins including first and second offset pin sections;

with the carpet layer in the molding tool and the mold tool in the open position, moving the first and second mold dies from the open position to the partially closed position;

in the partially closed position, injecting a heated polymer material into the mold cavity against the working side of the carpet layer, the heated polymer material incompletely filling the mold cavity on the working side of the carpet layer;

moving the first and second mold dies from the partially closed position to the closed position to spread the heated polymer material and fill the mold cavity on the working side of the carpet layer to form a molded polymer wall, the molded polymer wall adhering to the working side of the carpet layer to form a molded carpet laminate; and

moving the first and second mold dies from the closed position and cooling the molded carpet laminate.

2. The process as recited in claim 1 , wherein the moving of the first and second mold dies from the partially closed position to the closed position slides the carpet layer along the one or more eccentric pins to pull the carpet layer taut.

3. The process as recited in claim 1 , wherein the one or more eccentric pins are rotationally adjustable.

4. The process as recited in claim 1 , where the working side of the carpet layer includes an adhesive film.

5. The process as recited in claim 4 , where the adhesive film is formed of polyolefin, and the carpet layer includes fibers secured to a backing, the adhesive film in contact with the backing.

6. The process as recited in claim 1 , wherein a difference of at least −30° F. is maintained between a maximum temperature of the second mold die and a maximum temperature of the first mold die.

7. The process as recited in claim 1 , wherein the mold cavity has a surface that contacts the carpet layer and the surface has outside corners, each outside corner having a respective outside corner radius of curvature, and all of the outside corner radii of curvature are 20 millimeters or greater.

8. The process as recited in claim 1 , wherein the mold cavity has a surface that contacts the carpet layer and the surface has inside corners, each inside corner having a respective inside corner radius of curvature, and all of the inside corner radii of curvature are 25 millimeters or greater.

9. The process as recited in claim 1 , including, after the moving the first and second mold dies from the closed position to the open position and prior to the removing of the molded carpet laminate from the molding tool, using the one or more eccentric pins to restrain thermal warping of the molded carpet laminate.

10. The process as recited in claim 9 , wherein the molded carpet laminate includes through-holes, and the one or more eccentric pins extend in the through-holes.

11. The process as recited in claim 1 , wherein the first and second mold dies form a groove in the molded polymer wall along a periphery of the molded carpet laminate, the groove having a depth ratio of about 0.3 to about 0.8.

12. The process as recited in claim 1 , wherein the second mold die includes one or more slots that define a depth (D) into the second mold die and a thickness (t) perpendicular to the depth, the slot having an aspect ratio of D/t of greater than one.

13. The process as recited in claim 12 , wherein the aspect ratio of D/t is greater than two.

14. The process as recited in claim 1 , wherein the mold cavity includes an interior cavity portion and a gutter circumscribing the interior cavity portion, the interior cavity portion having a substantially uniform interior cavity thickness from the first mold die to the second mold die, the gutter having a gutter thickness from the first mold die to the second mold die, and in the closed position the gutter thickness is 80% or less of the uniform interior cavity thickness.

15. The process as recited in claim 1 , wherein the first mold die of the mold tool includes a bead near an edge of the first mold die, the bead pinching the carpet layer when the mold tool is in the closed position.

Assignments (3)
SECURITY INTEREST Recorded Jul 8, 2019
From: NYX, LLC
To: COMERICA BANK, AS AGENT
Reel/Frame 049690/0890 →
CONVERSION FROM A CORPORATION TO A LIMITED LIABILITY COMPANY Recorded Jun 21, 2019
From: NYX, INC.
To: NYX, LLC
Reel/Frame 049632/0907 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 14, 2017
From: PACKETT, JOSPEH; PEPPER, RAY; GREWAL, AKBAL; IMLER, JODI; HOMANN, GREG
To: NYX, INC.
Reel/Frame 041571/0206 →
Continuity (2)
Provisional Application 62297427 · Feb 19, 2016
Related Publication 20170239859A1 · Aug 24, 2017