Abstract

The invention relates to a method for recovering lithium from lithium-sulfur accumulators, wherein the accumulators are discharged, shredded, and pre-cleaned by sieves or screens to separate housing and electricity collector parts, the remaining material is dispersed in an aqueous medium, the insoluble components are removed by filtration and the electrolyte by phase separation, followed by a method for separating the lithium from the remaining filtrate.

Claims (11)

1 . A process for recovering lithium from lithium-sulfur rechargeable batteries, characterized in that the rechargeable batteries are discharged, shredded and precleaned by sifting or sieving for the separation of the housing and current collector parts, the remaining material is dispersed in an aqueous medium, the insoluble components are removed by filtration, and the electrolyte is removed by phase separation, followed by a process for the separation of the lithium from the remaining filtrate.

2 . The process according to claim 1 , characterized in that the aqueous medium has a pH≧7.

3 . The process according to claim 1 or 2 , characterized in that the separation of the lithium from the filtrate is carried out by thermal processing.

4 . The process according to claim 1 or 2 , characterized in that the separation of the lithium from the filtrate is carried out by chemical oxidation.

5 . The process according to claim 1 or 2 , characterized in that the separation of the lithium from the filtrate is carried out by processing under acidic conditions.

6 . The process according to claim 1 or 2 , characterized in that the separation of the lithium from the filtrate is carried out by precipitation.

7 . The process according to claim 3 , characterized in that the thermal processing is carried out in the temperature range from 100 to 1500° C. in the presence of oxygen.

8 . The process according to claim 3 , characterized in that the thermal processing is carried out in the temperature range from 100 to 1500° C. with exclusion of oxygen.

9 . The process according to claim 4 , characterized in that the chemical oxidation is carried out by reaction with hydrogen peroxide, ozone or hydroxyl radicals.

10 . The process according to claim 5 , characterized in that the processing is carried out under acidic conditions by adding sulfuric acid or hydrochloric acid, the lithium obtained is converted into the corresponding salts, and the polysulfur compounds formed are separated by extraction.

11 . The process according to claim 6 , characterized in that the lithium is precipitated from the filtrate by the addition of water-soluble carbonates.

Assignments (1)
CHANGE OF NAME Recorded Jul 22, 2019
From: ROCKWOOD LITHIUM GMBH
To: ALBEMARLE GERMANY GMBH