IP Library › Granted Patent US 10,343,376
Granted Patent B2
US 10,343,376 · App. 15/533,719 · Granted Jul 9, 2019

Glass resin laminate

Inventor: Takayuki Noda (Shiga, JP)
Assignee: NIPPON ELECTRIC GLASS CO., LTD.
B32B17/10036B32B7/02B32B7/12B32B17/065B32B17/10752B32B17/10788B32B2307/54B32B2369/00
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,343,376
App. No.
15/533,719
Granted
Jul 9, 2019
Kind
B2
Abstract

Provided is a glass resin laminate ( 1 ) obtained laminating glass sheets ( 5, 6 ) on both surfaces of a resin, plate ( 2 ) through intermediation of adhesive layers ( 3, 4 ) to integrate the plate and the sheets, in which an intermediate sheet ( 7 ) is interposed in the adhesive layer ( 3 ) on one surface side of the resin plate ( 2 ). In addition, on the side where the intermediate sheet ( 7 ) is interposed, the glass sheet ( 5 ) has a thickness of: from 0.01 mm to 1 mm, and the thickness of the adhesive layer ( 3 ) excluding the intermediate sheet ( 7 ) is smaller than the thickness of the resin plate ( 2 ). In addition, the intermediate sheet ( 7 ) has a tensile modulus larger than the tensile modulus of the adhesive layer ( 3 ).

Claims (22)

1. A glass resin laminate, comprising:

a resin plate;

a first glass sheet disposed on a first surface side of the resin plate;

a second glass sheet disposed on a second surface side of the resin plate;

a first intermediate sheet disposed between the resin plate and the first glass sheet a first adhesive layer disposed between the first glass sheet and the first intermediate sheet; and

a second adhesive layer disposed between the resin plate and the first intermediate sheet,

wherein:

the first glass sheet has a thickness of from 0.01 mm to 1 mm,

a total sum of a thickness of the first adhesive layer and a thickness of the second adhesive layer excluding the first intermediate sheet is smaller than a thickness of the resin plate,

a thickness of the first adhesive layer is larger than a thickness of the second adhesive layer such that the first intermediate sheet is arranged to be closer to the resin plate than to the first glass sheet, and

the first intermediate sheet has a tensile modulus larger than a tensile modulus of the first adhesive layer and the second adhesive layer.

2. The glass resin laminate according to claim 1 , wherein, the total sum of the thickness of the first adhesive layer and the thickness of the second adhesive layer excluding the first intermediate sheet is larger than the thickness of the glass sheet.

3. The glass resin laminate according to claim 1 , further comprising:

a second intermediate sheet disposed between the resin plate and the second glass sheet;

a third adhesive layer disposed between the second glass sheet and the second intermediate sheet; and

a fourth adhesive layer disposed between the resin plate and the second intermediate sheet,

wherein:

the second glass sheet has a thickness of from 0.01 mm to 1 mm,

a total sum of a thickness of the third adhesive layer and a thickness of the fourth adhesive layer excluding the second intermediate sheet is smaller than a thickness of the resin plate,

a thickness of the third adhesive layer is larger than a thickness of the fourth adhesive layer such that the second intermediate sheet is arranged to be closer to the resin plate than to the second glass sheet, and

the second intermediate sheet has a tensile modulus larger than a tensile modulus of the third adhesive layer and the forth adhesive layer.

4. The glass resin laminate according to claim 1 , wherein the first intermediate sheet comprises a resin sheet.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 7, 2017
From: NODA, TAKAYUKI
To: NIPPON ELECTRIC GLASS CO., LTD.
Reel/Frame 042635/0772 →
Priority Claims (1)
JP 2014-257335 · Dec 19, 2014 · national
Continuity (1)