Extended-life settable compositions comprising red mud

Inventors: Juan Humberto Martinez (Houston, TX); Thomas Jason Pisklak (Cypress, TX); Jiten Chatterji (Duncan, OK); Darrell Chad Brenneis (Marlow, OK)
Assignee: Halliburton Energy Services, Inc.
E21B33/14C04B24/003C04B28/18C09K8/467C04B2103/22
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,323,479
App. No.
15/540,554
Granted
Jun 18, 2019
Kind
B2
Abstract

A method for using an extended-life settable composition is disclosed. The method includes providing an extended-life settable composition comprising red mud, calcium hydroxide, water, and a cement set retarder. The method further includes activating the extended-life settable composition. The method additionally includes introducing the extended-life settable composition into a subterranean formation and allowing the extended-life settable composition to set in the subterranean formation.

Claims (14)

1. A method comprising:

providing an extended-life settable composition comprising red mud, calcium hydroxide, water, and a cement set retarder wherein the red mud is present in a red mud-to-calcium hydroxide weight ratio of about 3:1 to about 5:1 and wherein the red mud is a product of refining bauxite ore, the refining comprising sodium hydroxide digestion of the bauxite ore followed by filtration of solid impurities generated by the digestion;

activating the extended-life settable composition;

introducing the extended-life settable composition into a subterranean formation; and

allowing the extended-life settable composition to set in the subterranean formation.

2. A method according to claim 1 , wherein the red mud is an insoluble residue from the refining.

3. A method according to claim 1 , wherein the water is present in the extended-life settable composition in an amount of at least 40% by weight of the red mud.

4. A method according to claim 1 , wherein the red mud comprises at least 20% calcite.

5. A method according to claim 1 , wherein the cement set retarder is selected from the group consisting of a phosphonic acid, a phosphonic acid derivative, a lignosulfonate, a salt, an organic acid, a cellulose derivative, a synthetic co- or ter-polymer comprising sulfonate and carboxylic acid groups, a borate compound, and any combination thereof.

6. A method according to claim 1 , wherein the extended-life settable composition further comprises a dispersant.

7. A method according to claim 1 , wherein the cement set retarder comprises a phosphonic acid derivative, and wherein the extended-life settable composition further comprises a polycarboxylated ether dispersant.

8. A method according to claim 1 , further comprising storing the extended-life settable composition for a period of 1 day or longer prior to the step of introducing the cement composition into the subterranean formation.

9. A method according to claim 1 , wherein the step of activating the extended-life settable composition comprises adding a cement set activator to the extended-life settable composition.

10. A method according to claim 1 , wherein the step of introducing the extended-life settable composition comprises pumping the extended-life settable composition through a feed pipe and into a wellbore annulus.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 29, 2017
From: MARTINEZ, JUAN HUMBERTO; PISKLAK, THOMAS JASON; CHATTERJI, JITEN; BRENNEIS, DARRELL CHAD
To: HALLIBURTON ENERGY SERVICES, INC.
Reel/Frame 042863/0025 →
Continuity (1)
Related Publication 20170369762A1 · Dec 28, 2017