IP Library Granted Patent US 10,301,180
Granted Patent B2
US 10,301,180 · App. 15/541,145 · Granted May 28, 2019

Activated carbon regeneration method and gold recovery method

Inventors: Kazuhiro Hatano (Tsuruga, JP); Akira Yoshimura (Hitachi, JP); Ryosuke Tatsumi (Hitachi, JP)
Assignee: JX NIPPON MINING & METALS CORPORATION
C01B32/36B01J20/20B01J20/3416B01J20/3475C01G7/003C22B3/24C22B11/04Y02P10/234
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,301,180
App. No.
15/541,145
Granted
May 28, 2019
Kind
B2
Abstract

An activated carbon regeneration method of the present invention is for eluting gold from activated carbon on which the gold has been adsorbed and thereafter recycling, in adsorption of the gold, the used activated carbon from which the gold has been eluted, the method including: washing the used activated carbon with an acidic washing liquid, alkaline washing liquid or neutral washing liquid; and when the used activated carbon is washed with the acidic washing liquid, keeping the acidic washing liquid after the washing in an acidic region, or when the used activated carbon is washed with the alkaline washing liquid or neutral washing liquid, keeping the alkaline washing liquid or neutral washing liquid after the washing in an alkaline region or neutral region.

Claims (15)

1. A method for regenerating used activated carbon from which gold has been eluted, the method comprising:

after eluting the gold from the activated carbon thus providing the used activated carbon;

washing the used activated carbon with an acidic washing liquid or alkaline washing liquid; and

when the used activated carbon is washed with the acidic washing liquid, keeping a pH of the acidic washing liquid after the washing at 2.7 or lower, or when the used activated carbon is washed with an alkaline washing liquid, keeping a pH of the alkaline washing liquid after the washing at 8 or more, wherein an aqueous caustic soda solution is used as the alkaline washing liquid and a molar concentration of the aqueous caustic soda solution is 0.1 mol/L to 2.0 mol/L.

2. The method of claim 1 , wherein the used activated carbon is washed with the acidic washing liquid, and a hydrochloric acid solution is used as the acidic washing liquid.

3. The method of claim 1 , wherein the used activated carbon is washed with the alkaline washing liquid, and pH of the alkaline washing liquid after the washing is 8 to 12.

4. The method of any one of claims 1 , 2 , and 3 , wherein, when the used activated carbon is washed with the acidic washing liquid or alkaline washing liquid, a column is filled with the used activated carbon, and the acidic washing liquid or alkaline washing liquid is allowed to flow into the column.

5. The method of any one of claims 1 , 2 , and 3 , wherein providing the used activated carbon comprises providing the used activated carbon after eluting the gold from the activated carbon by using a cyanide solution.

6. The method of any one of claims 1 , 2 , and 3 , wherein providing the used activated carbon comprises providing the used activated carbon after eluting the gold from the activated carbon, the activated carbon having been used for adsorption of the gold in a gold-containing liquid,

wherein the gold-containing liquid is a liquid obtained by leaching the gold contained in a gold-containing metal sulfide ore, while warming, into an acidic leachate containing chloride ions and/or bromide ions as an anion and copper and iron as a cation.

7. A gold recovery method, comprising:

a gold leaching step of leaching the gold in a gold-containing metal sulfide ore, while warming, into an acidic leachate containing chloride ions and/or bromide ions as an anion and copper and iron as a cation;

a gold adsorption step of adsorbing the gold leached into the acidic leachate on activated carbon; and

a gold elution step of eluting the gold adsorbed on the activated carbon,

wherein the activated carbon regenerated by the method of any one of claims 1 , 2 , and 3 is used as the activated carbon.

Assignments (2)
CHANGE OF ADDRESS Recorded Aug 11, 2021
From: JX NIPPON MINING & METALS CORPORATION
To: JX NIPPON MINING & METALS CORPORATION
Reel/Frame 057160/0114 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 3, 2017
From: HATANO, KAZUHIRO; YOSHIMURA, AKIRA; TATSUMI, RYOSUKE
To: JX NIPPON MINING & METALS CORPORATION
Reel/Frame 042882/0627 →
Priority Claims (2)
JP 2015-045097 · Mar 6, 2015 · national
JP 2015-045107 · Mar 6, 2015 · national
Continuity (1)
Related Publication 20170369324A1 · Dec 28, 2017