IP Library › Granted Patent US 10,662,644
Granted Patent B2
US 10,662,644 · App. 15/564,761 · Granted May 26, 2020

Penetration firestop system

Inventors: John C. Hulteen (Afton, MN); George W. Frost (Afton, MN); Richard J. Haffner (New Richmond, WI); Ernst L. Schmidt (Hager City, WI)
Assignee: 3M Innovative Properties Company
E04B1/947A62C2/065E04B1/6801E04B1/6803E04B1/948F16L5/025F16L5/04
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,662,644
App. No.
15/564,761
Granted
May 26, 2020
Kind
B2
Abstract

Described herein is a firestop for construction assemblies comprising a penetration wherein a packing material and a non-porous adhesive article are used to fill and seal the opening.

Claims (28)

1. A method of using a first non-porous adhesive article and a first packing material on a construction assembly to provide a firestop system, the method comprising:

obtaining a construction assembly comprising a first major surface and an opposing second major surface and further comprising a first penetration which intersects the first major surface, the first major surface further comprises a first attachment area located about the perimeter of the first penetration, the construction assembly further comprising a penetrating object having a second attachment area, wherein the penetrating object passes through the first penetration and extends beyond the first major surface of the construction assembly and the first penetration comprises the packing material; and

using the first non-porous adhesive article to fixedly attach the first attachment area of the construction assembly to the second attachment area of the penetrating object via an adhesive, wherein the adhesive has a 90° peel strength according to ASTM D6252/6252M-98 (2011) at a strain rate of 12 inches/minute of at least 0.8 lb/in with a 1 inch overlap on concrete, and wherein the first non-porous adhesive article comprises a substrate and the adhesive disposed on a first major surface of the substrate and wherein the first non-porous adhesive article has a Gurley value greater than 10 Gurley seconds and wherein the substrate is selected from at least one of a polymeric film, a paper, a nonwoven matrix, a woven matrix, and a foam.

2. The method of claim 1 , wherein the second major surface comprises a second penetration which intersects the second major surface of the construction assembly, the second major surface further comprises a third attachment area located about the perimeter of the second penetration; wherein the second penetration comprises a second packing material; and wherein a second non-porous adhesive article is fixedly attached to the third attachment area.

3. The method of claim 2 , further comprising the penetrating object having a fourth attachment area, wherein the penetrating object passes through the second penetration and extends beyond the second major surface of the construction assembly, wherein the second non-porous adhesive article is fixedly attached to the third attachment area and the fourth attachment area.

4. The method of claim 1 , wherein the first non-porous adhesive article comprises an adhesive selected from at least one of an epoxy, an acrylic, a urethane, a silicone, and a rubber.

5. The method of claim 1 , wherein the adhesive is a pressure sensitive adhesive.

6. The method of claim 1 , wherein the adhesive comprises at least one of (i) an acrylic adhesive and (ii) a styrene block copolymer and a tackifier.

7. The method of claim 1 , wherein the first packing material is selected from at least one of mineral wool, ceramic fiber, glass fiber, and rockwool.

8. A firestop system comprising

(a) a non-porous adhesive article comprising a substrate and an adhesive disposed on a first major surface of the substrate wherein the non-porous adhesive article has a Gurley value greater than 10 Gurley seconds and wherein the substrate is selected from at least one of a polymeric film, a paper, a nonwoven matrix, a woven matrix, and a foam, and wherein the adhesive has a 90° peel strength according to ASTM D6252/6252M-98 (2011) at a strain rate of 12 inches/minute of at least 0.8 lb/in with a 1 inch overlap on concrete;

(b) a packing material; and

(c) a construction assembly comprising a first major surface and an opposing second major surface and a first penetration which intersects the first major surface, the first major surface comprising a first attachment area located about the perimeter of the first penetration;

wherein the first penetration comprises the packing material; and wherein the non-porous adhesive article is fixedly attached to the first attachment area.

9. A method of making a firestop system comprising

(a) providing a construction assembly comprising a first major surface and an opposing second major surface and further comprising a first penetration which intersects the first major surface, the first major surface further comprises a first attachment area located about the perimeter of the first penetration,

(b) inserting a packing material into the first penetration; and then

(c) sealing the first penetration by fixedly attaching a non-porous adhesive article to the first attachment area of the first major surface to form a firestop system, wherein the non-porous adhesive article has a Gurley value greater than 10 Gurley seconds and wherein the substrate is selected from at least one of a polymeric film, a paper, a nonwoven matrix, a woven matrix, and a foam, and wherein the adhesive has a 90° peel strength according to ASTM D6252/6252M-98 (2011) at a strain rate of 12 inches/minute of at least 0.8 lb/in with a 1 inch overlap on concrete.

10. The method of claim 1 , wherein the penetration has a smallest dimension of at least 6.4 mm.

11. The firestop system of claim 8 , further comprising a penetrating object having a second attachment area, wherein the penetrating object passes through the first penetration and extends beyond the first major surface of the construction assembly, wherein the non-porous adhesive article is fixedly attached to the first attachment area and the second attachment area.

12. The firestop system of claim 8 , wherein the non-porous adhesive article comprises an adhesive selected from at least one of an epoxy, an acrylic, a urethane, a silicone, and a rubber.

13. The firestop system of claim 8 , wherein the adhesive is a pressure sensitive adhesive.

14. The firestop system of claim 8 , wherein the adhesive comprises at least one of (i) an acrylic adhesive and (ii) a styrene block copolymer and a tackifier.

15. The firestop system of claim 8 , wherein the packing material is selected from at least one of mineral wool, ceramic fiber, glass fiber, and rockwool.

16. The firestop system of claim 8 , wherein the firestop system passes Fire Test 1.

17. The firestop system of claim 8 , wherein the non-porous adhesive article can withstand differential movement between the penetrating object and the construction assembly.

18. The method of claim 1 , wherein the substrate is a polymeric film.

19. The method of claim 9 , wherein the substrate is a polymeric film.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 22, 2017
From: HULTEEN, JOHN C.; FROST, GEORGE W.; HAFFNER, RICHARD J.; SCHMIDT, ERNST L.
To: 3M INNOVATIVE PROPERTIES COMPANY
Reel/Frame 044196/0887 →
Continuity (2)
Provisional Application 62149122 · Apr 17, 2015
Related Publication 20180112395A1 · Apr 26, 2018