Asphalt composition containing ester bottoms
This invention involves the addition of ester bottoms to an asphalt paving composition to improve the usable temperature range (UTR). The ester bottoms are a byproduct of refining a feedstock containing all or a portion of vegetable oil or animal fat.
1. A modified asphalt composition comprising 50 wt % to about 99.9 wt % of an asphalt, 0 wt % to about 20 wt % of a polymer modifier, and 0.1 wt % to about 50 wt % of ester bottoms, wherein the ester bottoms are a byproduct of methyl ester refining.
2. The asphalt composition of claim 1 wherein the asphalt includes from 20 wt % to 60 wt % recycled asphalt.
3. The asphalt of claim 1 wherein the polymer modifier is selected from the group of Styrene Butadiene (SB), ethylene vinyl-acetate, ethylene-methyl-acrylate, ethylene butyl acrylate, poly-propylene, atactic polypropylene, polystyrene, polyethylene, LDPE, HDPE, oxidized high density poly-propylene, poly-phosphoric acid (PPA), natural rubber, polybutadiene, epoxy resins, polyurethane resins, acrylic resins, phenolic resins, gilsonite, lignin, diblock polymers, Styrene-Butadiene-Styrene (SBS), triblock polymers which may be either linear or radial, styrene-isoprene-styrene (SIS), diblocked polymers, hydrotreated SBS, Styrene Ethylene Butadiene Styrene polymers (SEBS), Styrene Butadiene Rubber (SBR), polyacrylamide.
4. The modified asphalt composition of claim 1 wherein the addition of ester bottoms increases the useable temperature range of the asphalt composition.
5. The modified asphalt composition of claim 1 wherein the ester bottoms have a melting point of less than 120° F.
6. The modified asphalt composition of claim 1 wherein the ester bottoms contain sodium soap.
7. A paving asphalt comprising:
50 wt % to about 99.9 wt % of an asphalt mixture;
0.1 wt % to about 50 wt % ester bottoms, wherein the ester bottoms are a byproduct of methyl ester refining; and,
0 wt % to about 20 wt % of a polymer modifier.
8. The paving asphalt of claim 7 wherein the addition of the ester bottoms increases the useable temperature range.
9. The modified asphalt composition of claim 7 wherein the ester bottoms have a melting point of less than 120° F.
10. The modified asphalt composition of claim 7 wherein the ester bottoms contain sodium soap.
11. A paving asphalt comprising 50 wt % to about 99.99 wt % of an asphalt mixture and 0.1 wt % to about 50 wt % of ester bottoms, wherein the ester bottoms are a byproduct of methyl ester refining.
12. The paving asphalt of claim 11 wherein the addition of the ester bottoms increases the lower temperature compliance of the paving asphalt.