IP Library › Granted Patent US 10,307,740
Granted Patent B2
US 10,307,740 · App. 15/597,184 · Granted Jun 4, 2019

Methods of regenerating aromatization catalysts with a decoking step between chlorine and fluorine addition

Inventors: Ryan W. Snell (Kingwood, TX); Gabriela D. Alvez-Manoli (Kingwood, TX)
Assignee: Chevron Phillips Chemical Company LP
B01J23/96B01J23/42B01J29/62B01J29/70B01J29/90B01J35/0006B01J38/02B01J38/04B01J38/10B01J38/12B01J38/42B01J38/44B01J38/46B01J38/48B01J38/54B01J38/66C07C5/412C07C5/415C07C5/417C10G35/04C10G35/06C10G35/085C10G35/095C07C2523/42C07C2529/068C07C2529/60C07C2529/62C10G2300/4037
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,307,740
App. No.
15/597,184
Granted
Jun 4, 2019
Kind
B2
Abstract

Methods for regenerating a spent catalyst are disclosed. Such methods may employ a step of chlorinating the spent catalyst in the gas phase, followed by decoking the chlorinated spent catalyst, and then fluorinating the de-coked catalyst in a fluorine-containing solution of a fluorine-containing compound.

Claims (56)

1. A method for regenerating a spent catalyst comprising a transition metal and a catalyst support, the method comprising:

(1) contacting the spent catalyst with a chlorine-containing stream comprising a chlorine-containing compound to produce a chlorinated spent catalyst;

(2) contacting the chlorinated spent catalyst with a decoking gas stream comprising oxygen to produce a de-coked catalyst; and

(3) contacting the de-coked catalyst with a fluorine-containing solution comprising a fluorine-containing compound in the liquid phase to produce a fluorinated catalyst; wherein:

the transition metal comprises a Group 8-11 transition metal;

the catalyst support comprises a large pore zeolite having an average pore diameter in a range of from about 7 Å to about 12 Å; and

the spent catalyst further comprises chlorine and/or fluorine.

2. The method of claim 1 , wherein step (1) is conducted at a chlorination temperature in a range from about 30° C. to about 250° C.

3. The method of claim 1 , wherein an amount of the chlorine-containing compound in the chlorine-containing stream provides from about 0.5 to about 7 vol. % of chlorine (Cl) in the chlorine-containing stream.

4. The method of claim 3 , wherein the chlorine-containing stream is substantially free of oxygen-containing compounds.

5. The method of claim 1 , wherein the chlorine-containing compound comprises Cl 2 , carbon tetrachloride, tetrachloroethylene, or any combination thereof.

6. The method of claim 1 , wherein the chlorine-containing stream comprises Cl 2 and nitrogen.

7. The method of claim 1 , further comprising a chlorine purging step prior to step (2), the chlorine purging step comprising contacting the chlorinated spent catalyst with a chlorine purging stream comprising an inert gas.

8. The method of claim 1 , wherein:

step (2) is conducted at a peak decoking temperature in a range from about 300° C. to about 500° C.;

the decoking gas stream comprises an inert gas and oxygen; and

the decoking gas stream is substantially free of halogen-containing compounds.

9. The method of claim 1 , wherein step (3) is conducted at a fluorination temperature in a range from about 20° C. to about 50° C.

10. The method of claim 1 , wherein an amount of the fluorine-containing compound in the fluorine-containing solution provides from about 0.1 to about 10 wt. % of fluorine (F) in the fluorine-containing solution.

11. The method of claim 1 , wherein the fluorine-containing solution comprises water and at least one of ammonium fluoride and tetramethylammonium fluoride.

12. The method of claim 1 , further comprising a drying step, a calcination step, or both a drying step and a calcination step, after step (3).

13. The method of claim 1 , further comprising:

a partial decoking step prior to step (1), the partial decoking step comprising contacting the spent catalyst with a partial decoking gas stream comprising oxygen; and

a pre-drying step prior to step (1), the pre-drying step comprising contacting the spent catalyst with a pre-drying gas stream comprising an inert gas.

14. The method of claim 1 , wherein:

the transition metal comprises platinum; and

the catalyst support comprises a KL-zeolite and a binder comprising alumina, silica, a mixed oxide thereof, or a mixture thereof.

15. The method of claim 1 , further comprising:

a calcining step after step (3), the calcining step comprising calcining the fluorinated catalyst to produce a calcined catalyst; and

a reducing step after step (3), the reducing step comprising contacting the calcined catalyst with a reducing gas stream comprising molecular hydrogen.

16. A method for regenerating a spent catalyst comprising a transition metal and a catalyst support, the method comprising:

(a) contacting the spent catalyst with a pre-drying gas stream comprising an inert gas;

(b) contacting the spent catalyst with a chlorine-containing stream comprising a chlorine-containing compound to produce a chlorinated spent catalyst;

(c) contacting the chlorinated spent catalyst with a decoking gas stream comprising oxygen to produce a de-coked catalyst;

(d) contacting the de-coked catalyst with a fluorine-containing solution comprising a fluorine-containing compound in the liquid phase to produce a fluorinated catalyst; and

(e) drying, calcining, or both drying and calcining the fluorinated catalyst; wherein:

the transition metal comprises a Group 8-11 transition metal;

the catalyst support comprises a large pore zeolite having an average pore diameter in a range of from about 7 Å to about 12 Å; and

the spent catalyst further comprises chlorine and/or fluorine.

17. The method of claim 16 , wherein:

the pre-drying gas stream consists essentially of nitrogen;

the decoking gas stream comprises nitrogen and oxygen; and

the fluorine-containing solution comprises water and at least one of ammonium fluoride and tetramethylammonium fluoride.

18. The method of claim 16 , wherein the chlorine-containing compound comprises Cl 2 , carbon tetrachloride, tetrachloroethylene, or a combination thereof.

19. The method of claim 16 , further comprising a step of contacting the spent catalyst, prior to step (b), with a partial decoking gas stream comprising oxygen at a partial decoking temperature in a range from about 125° C. to about 450° C.

20. A reforming process comprising:

(A) contacting a hydrocarbon feed with an aromatization catalyst comprising a transition metal and a catalyst support under reforming conditions in a reactor system to produce an aromatic product;

(B) performing step (A) for a time period sufficient to form a spent catalyst;

(C) contacting the spent catalyst with a chlorine-containing stream comprising a chlorine-containing compound to produce a chlorinated spent catalyst;

(D) contacting the chlorinated spent catalyst with a decoking gas stream comprising oxygen to produce a de-coked catalyst; and

(E) contacting the de-coked catalyst with a fluorine-containing solution comprising a fluorine-containing compound in the liquid phase to produce a fluorinated catalyst; wherein:

the transition metal comprises a Group 8-11 transition metal;

the catalyst support comprises a large pore zeolite having an average pore diameter in a range of from about 7 Å to about 12 Å; and

the aromatization catalyst further comprises chlorine and/or fluorine.

21. The process of claim 20 , wherein the reforming process is an in situ process.

22. The process of claim 20 , wherein step (E) is performed external to the reactor system.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 21, 2017
From: SNELL, RYAN W.; ALVEZ-MANOLI, GABRIELA D.
To: CHEVRON PHILLIPS CHEMICAL COMPANY LP
Reel/Frame 043060/0343 →
Continuity (1)