IP Library › Granted Patent US 10,301,524
Granted Patent B2
US 10,301,524 · App. 15/724,809 · Granted May 28, 2019

Method of drilling a substerranean geological formation with a drilling fluid composition comprising copper nitrate

Inventors: Salah El-Din Elkatatny (Dhahran, SA); Reyad Awwad Shawabkeh (Dhahran, SA); Mohamed Ahmed Nasr El-Din Mahmoud (Dhahran, SA)
Assignee: King Fahd University of Petroleum and Minerals
C09K8/08E21B21/003E21B41/02C09K2208/20E21B21/062E21B43/26
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,301,524
App. No.
15/724,809
Granted
May 28, 2019
Kind
B2
Abstract

A drilling fluid composition comprising an aqueous base fluid, a viscosifier, and a H 2 S scavenger comprising copper nitrate, wherein the drilling fluid composition has a H 2 S sorption capacity from about 4.0 to about 6.0 gram per one milliliter of the drilling fluid composition; and a method of drilling a subterranean geological formation using thereof are provided. Various embodiments of the drilling fluid composition and the method are also provided.

Claims (21)

1. A method of drilling a subterranean geological formation, comprising:

driving a drill bit to form a wellbore into the subterranean geological formation thereby producing a formation fluid that contains H 2 S; and

injecting a drilling fluid composition into the subterranean geological formation through the wellbore,

wherein the drilling fluid composition comprises

an aqueous base fluid,

a viscosifier, and

a H 2 S scavenger comprising copper nitrate, and

wherein copper nitrate present in the drilling fluid composition reacts with H 2 S present in the formation fluid to form copper sulfide;

recovering the copper sulfide from the drilling fluid composition; and

treating the copper sulfide with nitric acid to regenerate copper nitrate while concurrently forming elemental sulfur.

2. The method of claim 1 , wherein the wellbore is a horizontal or a multilateral wellbore.

3. The method of claim 1 , wherein a temperature of the wellbore ranges from 50 to 200° C.

4. The method of claim 1 ,

wherein the wellbore contains a casing that is made of at least one metal selected from the group consisting of stainless steel, aluminum, and titanium, the casing is exposed to a gaseous mixture containing up to 12 vol % of H 2 S, and

wherein a corrosion rate of the casing is no more than 0.0006 lb/ft 2 after 6 hours of contacting with the drilling fluid composition.

5. The method of claim 4 , wherein the corrosion rate of the casing is no more than 0.00084 lb/ft 2 after 24 hours of contacting with the drilling fluid composition.

6. The method of claim 1 ,

wherein the formation fluid is produced for at least 1 hour but no more than 4 hours, and

wherein a concentration of H 2 S in the formation fluid is no more than 40 ppm.

7. The method of claim 1 , further comprising:

circulating the drilling fluid composition within the wellbore for at least 30 minutes but no more than 3 hours, after the injecting.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Oct 4, 2017
From: SHAWABKEH, REYAD AWWAD; MAHMOUD, MOHAMED AHMED NASR EL-DIN; ELKATATNY, SALAH EL-DIN
To: KING FAHD UNIVERSITY OF PETROLEUM AND MINERALS
Reel/Frame 043781/0948 →
Continuity (1)
Related Publication 20190100684A1 · Apr 4, 2019