IP Library Granted Patent US 11,355,783
Granted Patent B2
US 11,355,783 · App. 15/735,791 · Granted Jun 7, 2022

Method of manufacturing a lithium-ion secondary battery

Inventors: Tomoyuki Ichikawa (Kanagawa, JP); Shinsuke Enomoto (Kanagawa, JP); Naoyuki Iwata (Kanagawa, JP)
Assignee: ENVISION AESC JAPAN LTD.
H01M10/058G01R31/3865H01M4/0447H01M10/0525H01M10/0566H01M10/42G01R31/52H01M2300/0037
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,355,783
App. No.
15/735,791
Granted
Jun 7, 2022
Kind
B2
Abstract

A method of manufacturing a lithium-ion secondary battery of the present invention includes at least four steps as follows: an initial charging step of charging the lithium-ion secondary battery, which has not been subjected to initial charging, under a temperature environment ranging of equal to or higher than −20° C. and equal to or lower than 15° C.; an aging step of leaving the lithium-ion secondary battery under a temperature environment ranging of equal to or higher than 30° C. and equal to or lower than 80° C. after the initial charging step; a short circuit detecting step of detecting the presence or absence of a short circuit of the lithium-ion secondary battery by measuring a voltage drop quantity of the lithium-ion secondary battery and comparing the voltage drop quantity with a reference value; and a sorting step of sorting out a lithium-ion secondary battery in which no short circuit is detected.

Claims (36)

1. A method of determining whether a lithium-ion secondary battery is a quality product or a defective unit, the method comprising:

an initial charging step of charging the lithium-ion secondary battery, which has not been subjected to an initial charging, under a temperature environment ranging of equal to or higher than −20° C. and equal to or lower than 15° C.;

an aging step of leaving the lithium-ion secondary battery subjected to the initial charging step under a temperature environment ranging of equal to or higher than 30° C. and equal to or lower than 80° C. after the initial charging step;

a short circuit detecting step of detecting for a short circuit in the lithium-ion secondary battery subjected to the aging step by measuring a voltage drop quantity of the lithium-ion secondary battery and comparing the measured voltage drop quantity with a predetermined reference value; and

a determining step of determining that the lithium-ion secondary battery subjected to said short circuit detecting step is the quality product when the short circuit in the lithium-ion secondary battery is not detected, and determining that the lithium-ion secondary battery subjected to said short circuit detecting step is the defective unit when the short circuit in the lithium-ion secondary battery is detected, and

wherein a viscosity of an electrolytic solution in the lithium-ion secondary battery in the initial charging step is equal to or higher than 6.0 mPa·s.

2. The method of determining whether a lithium-ion secondary batter is a quality product or a defective unit according to claim 1 ,

wherein (T 2 −T 1 ) is equal to or higher than 30° C. when an ambient temperature in the initial charging step is set to T 1 and an ambient temperature in the aging step is set to T 2 .

3. The method of determining whether a lithium-ion secondary batter is a quality product or a defective unit according to claim 1 ,

wherein the aging step is performed without carrying out charging and discharging even once after the initial charging step.

4. The method of determining whether a lithium-ion secondary batter is a quality product or a defective unit according to claim 1 ,

wherein a voltage of the lithium-ion secondary battery when the aging step starts is equal to or higher than 3.80 V.

5. The method of determining whether a lithium-ion secondary batter is a quality product or a defective unit according to claim 1 ,

wherein in the aging step, the lithium-ion secondary battery is left for equal to or longer than two days.

6. The method of determining whether a lithium-ion secondary batter is a quality product or a defective unit according to claim 1 ,

wherein the lithium-ion secondary battery is subjected to discharging after the aging step, and a voltage of the lithium-ion secondary battery in the short circuit detecting step is set to range of equal to or higher than 2.5 V and equal to or lower than 3.8 V.

7. The method of determining whether a lithium-ion secondary batter is a quality product or a defective unit according to claim 1 ,

wherein a viscosity of an electrolytic solution in the lithium-ion secondary battery in the aging step is equal to or lower than 4.5 mPa·s.

8. A method of determining whether a lithium-ion secondary battery is a quality product or a defective unit, the method comprising:

an initial charging step of charging the lithium-ion secondary battery, which has not been subjected to an initial charging, under a temperature environment ranging of equal to or higher than −20° C. and equal to or lower than 15° C.;

an aging step of leaving the lithium-ion secondary battery subjected to the initial charging step under a temperature environment ranging of equal to or higher than 30° C. and equal to or lower than 80° C. after the initial charging step;

a short circuit detecting step of detecting for a short circuit in the lithium-ion secondary battery subjected to the aging step by measuring a voltage drop quantity of the lithium-ion secondary battery and comparing the measured voltage drop quantity with a predetermined reference value; and

a determining step of determining that the lithium-ion secondary battery subjected to said short circuit detecting step is the quality product when the short circuit in the lithium-ion secondary battery is not detected, and determining that the lithium-ion secondary battery subjected to said short circuit detecting step is the defective unit when the short circuit in the lithium-ion secondary battery is detected, and

wherein a viscosity of an electrolytic solution in the lithium-ion secondary battery in the aging step is equal to or lower than 4.5 mPa·s.

9. The method of determining whether a lithium-ion secondary battery is a quality product or a defective unit according to claim 8 ,

wherein (T 2 −T 1 ) is equal to or higher than 30° C. when an ambient temperature in the initial charging step is set to T 1 and an ambient temperature in the aging step is set to T 2 .

10. The method of determining whether a lithium-ion secondary battery is a quality product or a defective unit according to claim 8 ,

wherein the aging step is performed without carrying out charging and discharging even once after the initial charging step.

11. The method of determining whether a lithium-ion secondary battery is a quality product or a defective unit according to claim 8 ,

wherein a voltage of the lithium-ion secondary battery when the aging step starts is equal to or higher than 3.80 V.

12. The method of determining whether a lithium-ion secondary battery is a quality product or a defective unit according to claim 8 ,

wherein in the aging step, the lithium-ion secondary battery is left for equal to or longer than two days.

13. The method of determining whether a lithium-ion secondary battery is a quality product or a defective unit according to claim 8 ,

wherein the lithium-ion secondary battery is subjected to discharging after the aging step, and a voltage of the lithium-ion secondary battery in the short circuit detecting step is set to range of equal to or higher than 2.5 V and equal to or lower than 3.8 V.

14. The method of determining whether a lithium-ion secondary battery is a quality product or a defective unit according to claim 13 ,

wherein a viscosity of an electrolytic solution in the lithium-ion secondary battery in the initial charging step is equal to or higher than 6.0 mPa·s.

Assignments (3)
CHANGE OF NAME Recorded Mar 24, 2022
From: ENVISION AESC ENERGY DEVICES, LTD.
To: ENVISION AESC JAPAN LTD.
Reel/Frame 059387/0668 →
CHANGE OF NAME Recorded Jul 1, 2019
From: NEC ENERGY DEVICES, LTD.
To: ENVISION AESC ENERGY DEVICES, LTD.
Reel/Frame 049638/0005 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 12, 2017
From: ICHIKAWA, TOMOYUKI; ENOMOTO, SHINSUKE; IWATA, NAOYUKI
To: NEC ENERGY DEVICES, LTD.
Reel/Frame 044370/0035 →
Priority Claims (1)
JP JP2015-132834 · Jul 1, 2015 · national
Continuity (1)
Related Publication 20180183091A1 · Jun 28, 2018